    • 10. 发明公开
    • FLAME-RETARDANT RESIN COMPOSITION, METHOD FOR PRODUCING SAME, MOLDED BODY OF SAME, AND ELECTRIC WIRE
    • 阻燃树脂组合物,用于生产,成型体和电线在线
    • EP2805994A4
    • 2015-08-26
    • EP13738820
    • 2013-01-21
    • MITSUI CHEMICALS INC
    • NODA KIMINORIYAMAGUCHI MASAYOSHIKOMIYA KANUEHARA HIROSHI
    • C08L23/08B29C47/02C08K3/22C08K3/38C08L23/10C08L23/14C08L83/04H01B3/44H01B7/295
    • C08L23/0853B29B7/48B29C47/40B29C47/92B29C2947/92704C08K3/22C08K3/38C08K2003/2224C08K2003/387C08L23/12C08L23/14C08L83/04C08L2201/02C08L2203/202C08L2205/03H01B3/44H01B3/441H01B3/448H01B7/295
    • Disclosed is a flame-retardant resin composition comprising, as a polymer component: 50 to 95% by mass of copolymer (A) of ethylene and a vinyl ester, 5 to 50% by mass of propylene copolymer (B) wherein the content of an ±-olefin except for propylene is 10 to 60% by mole, and 0 to 40% by mass of polypropylene (C) wherein the content of an ±-olefin except for propylene is less than 10% by mole; wherein the total of components (A), (B), and (C) is 100% by mass; and further comprising, with respect to 100 parts by mass of the total of components (A), (B), and (C): 50 to 350 parts by mass of metal hydroxide (D), 0.1 to 50 parts by mass of zinc borate (E), and 0.1 to 50 parts by mass of powdered silicone (F); wherein the mass ratio [D/(E+F)] of component (D) with respect to the total amount of components (E) and (F) is 15 or less, and is preferably the above-mentioned flame-retardant resin composition comprising 15% by mass or more of component (B), or comprising 10% by mass or more of component (B) and 1% by mass or more of polypropylene (C); further satisfying following conditions (i) and (2): (1) the Shore D hardness measured according to ASTM D2240 is 40 to 65; and (ii) the tensile breaking elongation of a press sheet with a thickness of 2 mm measured according to JIS K7113-2 is 100 % or more.
    • 本发明公开了一种阻燃性树脂组合物,包括,作为聚合物成分:worin的含量为50〜95%的乙烯的共聚物(A)和乙烯基酯,5至50%的丙烯共聚物(B)的质量的质量 丙烯以外的烯烃±为10〜60摩尔%,和0至40%的聚丙烯(C)的质量worin丙烯以外的所述的烯烃±的含量为小于10%(摩尔); worin的总组分的(A),(B)和(C)是100质量%; 并且还包括,由所述总组分的(A),(B)的相对于100质量份和(C):50〜350质量份的金属氢氧化物的质量(D)0.1至50份锌质量 硼酸盐(e)和0.1至50份的粉末状聚硅氧烷的质量(F); worin的质量比[D /(E + F)]相对于组分的总量(E)和(F)成分(D)的是15或更小,且优选为上述的阻燃性树脂组合物 质量以上的组分(B),或包含10%质量或更多的组分(B)和1%的由聚丙烯的质量以上(C),其包含15%; 进一步满足下述条件(i)和(2):(1)肖氏D硬度测得gemäß到ASTM D2240为40〜65; 和(ii)的拉伸断裂的压片的伸长率与测量gemäß到JIS K7113-2的厚度为2毫米的100%或更多。