    • METHOD FOR MANUFACTURING ALUMINUM ALLOY MEMBER AND ALUMINUM ALLOY MEMBER USING SAME
    • VERFAHREN ZUR HERSTELLUNG EINS ALUMINIUMIUM GIERUNGSELEMENTS UND ALUMINIUMLEGIERUNGSELEMENT DAMIT
    • EP3135790A4
    • 2017-06-07
    • EP15799459
    • 2015-05-29
    • MITSUBISHI HEAVY IND LTD
    • INOUE AKIKOTAKAHASHI TAKAYUKI
    • C22F1/053C22C21/10
    • C22F1/053B21C23/002C22C21/10
    • The present invention provides: a method for manufacturing an aluminum alloy member, the method making it possible to manufacture an aluminum alloy member having high strength, high resistance, and exceptional shape accuracy; and the aluminum alloy member. This method for manufacturing an aluminum alloy member includes: a molding step (ST2) for heating, to a temperature of 400°C to 500°C, and performing molding on an aluminum (Al) alloy comprising 1.6-2.6 mass% of magnesium (Mg), 6.0-7.0 mass% of zinc (Zn), 0.5 mass% or less of copper (Cu) or silver (Ag) with the total amount of copper (Cu) and silver (Ag) being 0.5 mass% or less, and 0.01-0.05 mass% of titanium (Ti), the balance being aluminum (Al) and unavoidable impurities; and a cooling step (ST3) for cooling the molded aluminum alloy at a cooling speed of 2-30°C/sec and preferably 2-10°C/sec, and obtaining an aluminum alloy member.
    • 本发明提供一种铝合金构件的制造方法,该方法能够制造具有高强度,高电阻和异常形状精度的铝合金构件; 和铝合金构件。 该铝合金构件的制造方法包括:将含有1.6〜2.6质量%的镁(Al)合金的铝(Al)合金进行加热至400〜500℃的成形工序(ST2) Mg),铜(Cu)和银(Ag)的合计量为0.5质量%以下的情况下,锌(Zn)为6.0〜7.0质量%,铜(Cu)或银(Ag) 和钛(Ti)0.01〜0.05质量%,余量由铝(Al)和不可避免的杂质构成。 和冷却步骤(ST3),用于以2-30℃/秒,优选2-10℃/秒的冷却速度冷却模制铝合金,并获得铝合金构件。