    • 10. 发明公开
    • LAMINATE, AND ELEMENT COMPRISING SUBSTRATE MANUFACTURED USING SAME
    • 层压材料,以及使用该材料制造的包含基材的元件
    • EP2985143A1
    • 2016-02-17
    • EP14782948.5
    • 2014-04-08
    • LG Chem, Ltd.
    • JEONG, Hye WonKIM, KyungjunKIM, Kyoung HoonPARK, Chan HyoSHIN, BoRaLEE, Seung YupPARK, HangAhLEE, JinHoIM, MiRa
    • B32B7/04B32B7/06B32B7/12B32B27/06H01L51/56
    • The present invention relates to a laminate and a device fabricated using the laminate. The laminate includes a first polyimide resin layer between a carrier substrate and a second polyimide resin layer, wherein the first polyimide resin layer has a coefficient of thermal expansion(CTE) equal to or lower than the CTE of the second polyimide-based resin layer at a temperature of 100 to 200°C, and the adhesive strength of the first resin layer to the second resin layer decreases when a physical stimulus causing no chemical changes in the first resin layer is applied to the laminate. According to the present invention, the flexible substrate can be easily separated from the carrier substrate without the need for further processing such as laser or light irradiation. Therefore, the use of the laminate facilitates the fabrication of the device having the flexible substrate. The device may be, for example, a flexible display device. In addition, the device can be prevented from deterioration of reliability and occurrence of defects caused by laser or light irradiation. This ensures improved characteristics and high reliability of the device.
    • 本发明涉及层压体和使用该层压体制造的装置。 所述层压体包括在载体基板和第二聚酰亚胺树脂层之间的第一聚酰亚胺树脂层,其中所述第一聚酰亚胺树脂层的热膨胀系数(CTE)等于或低于所述第二聚酰亚胺基树脂层在 温度为100-200℃,并且当在第一树脂层中不引起化学变化的物理刺激施加到叠层时,第一树脂层对第二树脂层的粘合强度降低。 根据本发明,柔性基板可以容易地从载体基板分离而不需要进一步处理,例如激光或光照射。 因此,层压板的使用便于制造具有柔性基板的器件。 该设备可以是例如柔性显示设备。 另外,可以防止装置的可靠性恶化以及由激光或光照引起的缺陷的发生。 这确保了设备的改进特性和高可靠性。