    • 1. 发明公开
    • Decorative mold for forming concrete surface with uneven pattern and process for its manufacture
    • 通过与不平坦图案,使这种形式的方法的混凝土表面的变形形成用于生产的装饰效果
    • EP0703049A3
    • 1996-06-12
    • EP95114199.3
    • 1995-09-11
    • JSP CORPORATION
    • Mitsumoto, MasanoriKuwabara, HidekiOmori, KazuhikoShioya, SatoruWataru Kikuchi
    • B28B7/34
    • B28B7/0073B28B7/007B28B7/346B28B7/348
    • The present invention relates to a decorative mold (1) having an uneven pattern for forming a concrete surface with an uneven pattern by transfer. The present decorative mold (1) is made of a molded product of polypropylene type foamed particles having a density of 0.02 to 0.06 g/cm³ and is formed with an uneven pattern (2) on one surface for forming a pattern on a concrete surface by transfer, and in the surface having the uneven pattern (2) for transfer, the total area, in terms of projected plane, of gap sections (4) present in all the projected plane of the decorative mold (1) accounts for less than 0.5% of all the area, in terms of projected plane, of the decorative mold (1). The maximum bending strength of the decorative mold (1) determined by pressing from the undersurface opposite to the side having the uneven pattern (2) is preferably 8.0 kgf/cm² or more, and the average particle diameter of the polypropylene type resin foamed particles (3) that are a raw material constituting the decorative mold is preferably 1 to 4 mm. The side walls are preferably spread out from the undersurface side of the decorative mold (1) toward the side of the surface (2) having the uneven pattern. Further the molded product of polypropylene type resin foamed particles that constitutes the decorative mold has preferably such a crystalline structure that the DSC curve obtained by subjecting the molded product to differential scanning calorimetry has a high-temperature peak the amount of heat of which is 13 to 30 J/g. The present decorative mold is obtained by loading a raw material, i.e., polypropylene type resin foamed particles (3) from a loader (15) into the cavity (12) of a mold (7), then introducing heating steam through the steam supply pipes (16) and (17) to heat the foamed particles and molding them.
    • 本发明涉及一种装饰模具(1)上具有用于通过转印在凹凸图案与形成在混凝土表面的凹凸图案。 本装饰模具(1)由聚丙烯类发泡颗粒的具有0.02至0.06的密度的模制产品的克/厘米<3>和在一个表面上形成有与上图案(2)凹凸形成在图案 通过转移,平坦的混凝土表面上,并在表面上具有凹凸图案(2),用于传送,总面积中的投影而言,间隙部(4)存在于所述装饰模具的所有投影平面(1)占 装饰模具的所有面积的小于0.5%,在投影方面的规划,(1)。 装饰模具(1)通过从底面按压相反具有凹凸图案的侧确定性开采的最大弯曲强度(2)优选为8.0千克力/厘米<2>以上,聚丙烯类树脂的平均颗粒直径 发泡颗粒(3)做是构成装饰模具的原料优选为1至4mm。 的侧壁优选从装饰模具(1)向具有凹凸图案的表面(2)的侧部的下侧展开。 进一步发泡颗粒确实聚丙烯类树脂的成型品构成的装饰用金属模优选寻求的晶体结构并通过将模制产品差示扫描量热法获得的DSC曲线具有高温峰是13至的所有热量 为30J / g。 本装饰模具由通过蒸汽供给管从一个装载机(15)加载的原料,即,聚丙烯类树脂发泡粒子(3)到模具(7),然后导入加热蒸汽的所述腔体(12)中得到 (16)和(17)来加热发泡颗粒和模塑它们。
    • 3. 发明公开
    • Decorative mold for forming concrete surface with uneven pattern and process for its manufacture
    • 通过与不平坦图案,使这种形式的方法的混凝土表面的变形形成用于生产的装饰效果
    • EP0703049A2
    • 1996-03-27
    • EP95114199.3
    • 1995-09-11
    • JSP CORPORATION
    • Mitsumoto, MasanoriKuwabara, HidekiOmori, KazuhikoShioya, SatoruWataru Kikuchi
    • B28B7/34
    • B28B7/0073B28B7/007B28B7/346B28B7/348
    • The present invention relates to a decorative mold (1) having an uneven pattern for forming a concrete surface with an uneven pattern by transfer. The present decorative mold (1) is made of a molded product of polypropylene type foamed particles having a density of 0.02 to 0.06 g/cm³ and is formed with an uneven pattern (2) on one surface for forming a pattern on a concrete surface by transfer, and in the surface having the uneven pattern (2) for transfer, the total area, in terms of projected plane, of gap sections (4) present in all the projected plane of the decorative mold (1) accounts for less than 0.5% of all the area, in terms of projected plane, of the decorative mold (1). The maximum bending strength of the decorative mold (1) determined by pressing from the undersurface opposite to the side having the uneven pattern (2) is preferably 8.0 kgf/cm² or more, and the average particle diameter of the polypropylene type resin foamed particles (3) that are a raw material constituting the decorative mold is preferably 1 to 4 mm. The side walls are preferably spread out from the undersurface side of the decorative mold (1) toward the side of the surface (2) having the uneven pattern. Further the molded product of polypropylene type resin foamed particles that constitutes the decorative mold has preferably such a crystalline structure that the DSC curve obtained by subjecting the molded product to differential scanning calorimetry has a high-temperature peak the amount of heat of which is 13 to 30 J/g. The present decorative mold is obtained by loading a raw material, i.e., polypropylene type resin foamed particles (3) from a loader (15) into the cavity (12) of a mold (7), then introducing heating steam through the steam supply pipes (16) and (17) to heat the foamed particles and molding them.