    • CRIMPED FIBER AND NONWOVEN FABRIC
    • GEKRÄUSELTERFASER- UND VLIESSTOFF
    • EP3121314A1
    • 2017-01-25
    • EP15765590.3
    • 2015-03-18
    • Idemitsu Kosan Co. Ltd (IKC)
    • KOORI, YoheiTAKEBE, TomoakiMINAMI, YutakaKANAMARU, Masami
    • D01F8/06D04H3/007D04H3/147
    • D04H3/018B32B5/022B32B5/26B32B2250/20B32B2262/0253B32B2262/12D01D5/32D01D5/34D01F6/46D01F8/06D02G1/14D04H1/4291D04H3/007D04H3/03D10B2321/022
    • Provided is a crimped fiber constituted of the following first component and second component, wherein the first component is a propylene-based resin composition containing a propylene-based polymer (1-A) in which a melting point (Tm-D) obtained under a specified condition exceeds 120°C and a propylene-based polymer (1-B) satisfying the conditions that (a) a weight average molecular weight (Mw) is 10,000 to 200,000, (b) a molecular weight distribution (Mw/Mn) is less than 4.0, and (c) a melting point (Tm-D) obtained under a specified condition is 0 to 120°C; and the second component is a propylene-based polymer (2) in which a melt flow rate (MFR) under the foregoing measurement condition is 1 g/10 min or more and 2,000 g/10 min or less, and a melting point (Tm-D) observed under the foregoing measurement condition by using a differential scanning calorimeter (DSC) exceeds 120°C, or a propylene-based resin composition containing the propylene-based polymer (2).
    • 本发明提供一种由以下第一成分和第二成分构成的卷曲纤维,其中,第一成分为含有丙烯系聚合物(1-A)的丙烯系树脂组合物,其中,在 规定条件超过120℃,满足(a)重均分子量(Mw)为10,000〜200,000,(b)分子量分布(Mw / Mn)的条件的丙烯系聚合物(1-B)为 小于4.0,(c)在规定条件下得到的熔点(Tm-D)为0〜120℃; 第二成分是丙烯类聚合物(2),其中在上述测定条件下的熔体流动速率(MFR)为1g / 10分钟以上且2,000g / 10分钟以下,熔点(Tm -D)通过使用差示扫描量热计(DSC)在上述测量条件下观察超过120℃,或含有丙烯类聚合物(2)的丙烯类树脂组合物。
    • 7. 发明公开
    • POLYPROPYLENE-BASED RESIN COMPOSITION, AND FIBER AND NONWOVEN FABRIC USING SAME
    • EP3660091A1
    • 2020-06-03
    • EP18837516.6
    • 2018-07-23
    • Idemitsu Kosan Co., Ltd
    • YABE, MariSUGIUCHI, TakumiMINAMI, YutakaTAKEBE, Tomoaki
    • C08L23/10C08L23/02D01F1/10D01F6/06D01F8/06D04H3/007D04H3/14D04H3/147
    • The present invention relates to [1] a polypropylene-based resin composition satisfying the following requirements (1) and (2) in a differential molecular weight distribution curve which is obtained from measurement by the gel permeation chromatography using polystyrene as a conversion standard, and in which the abscissa represents a logarithmic value log(M) of a molecular weight M, and the ordinate represents a dw/dlog(M) value obtained by differentiating a concentration fraction w by the logarithmic value log(M) of the molecular weight:
      (1) In the differential molecular weight distribution curve, a value obtained by integrating the dw/dlog(M) values in the range of (5.5 ≤ log(M)) is 25% or less relative to a value obtained by integrating the dw/dlog(M) values over the entire range of log(M); and
      (2) In the differential molecular weight distribution curve, a value obtained by integrating the dw/dlog(M) values in the range of (log(M) ≤ 4.5) is more than 10% relative to a value obtained by integrating the dw/dlog(M) values over the entire range of log(M).
      The present invention also relates to [2] a polypropylene-based resin composition having a melt flow rate (MFR) of 10 to 500 g/10 min and a half-crystallization time of more than 0.05 seconds; and further relates to [3] a polypropylene-based resin composition containing 40 to 99% by mass of a polypropylene-based resin (A) having a melting point (Tm-D) of higher than 120°C, 0.5 to 59.5% by mass of a polypropylene-based resin (B-1) having a melting endotherm (ΔH-D) of 0 to 80 J/g, and 0.5 to 59.5% by mass of a wax (B-2).