    • 1. 发明公开
    • Corrosion and wear resistant coating for magnetic steel
    • Korrosions- und wetterfeste BeschichtungfürMagnetstahl
    • EP2014792A1
    • 2009-01-14
    • EP08157982.3
    • 2008-06-10
    • Honeywell International Inc.
    • Mittendorf, Don L.Aizaz, Amer
    • C23C18/32
    • C23C18/32
    • A method is provided for manufacturing a magnetic steel component. An electroless nickel plating (14) is formed on a substrate (10) that includes magnetic steel. A thermal cycle is thereafter performed at a temperature that is sufficiently high to sinter the electroless nickel plating (14) and thereby form a densified plating (16) on the substrate (10) . According to one embodiment, the thermal cycle includes a solid state diffusion sintering process wherein the substrate (10) and the densified plating (16) are heated to a temperature of at least about 1300 °F (about 704 °C) but below the melting temperature of the electroless nickel plating (14). According to another embodiment, the thermal cycle includes a transient liquid phase sintering process wherein the substrate (10) and the densified plating (16) are heated at least to the melting temperature of the electroless nickel plating (14).
    • 提供了制造磁钢部件的方法。 在包括磁钢的基板(10)上形成化学镀镍(14)。 此后,在足够高的温度下进行热循环以烧结无电镀镍(14),从而在基板(10)上形成致密的镀层(16)。 根据一个实施例,热循环包括固态扩散烧结工艺,其中将基底(10)和致密化的镀层(16)加热至至少约1300°F(约704℃)但低于熔化温度 化学镀镍(14)的温度。 根据另一个实施例,热循环包括瞬态液相烧结工艺,其中将基底(10)和致密化的镀层(16)至少加热至化学镀镍(14)的熔化温度。
    • 3. 发明公开
    • Noise attenuators and methods of manufacturing noise attenuators and bleed valve assemblies
    • 减噪器和制造阻尼器的方法,和排出阀组件
    • EP2062688A2
    • 2009-05-27
    • EP08169297.2
    • 2008-11-17
    • Honeywell International Inc.
    • Appleby, AndrewAizaz, AmerHitzler, Dan
    • B24C1/04F01D25/30
    • B24C1/045F01D17/105F02K3/075F05D2230/10F05D2260/96Y10T29/496
    • Methods (700) of manufacturing a noise attenuator (206) are provided. In an embodiment, by way of example only, the method (700) includes shaping (702) a plate (902) to have a three-dimensional contour, and forming a plurality of openings (218, 918) through the shaped plate (902) with an abrasive fluid jet to thereby form the bleed valve noise attenuator (206). In another embodiment, a bleed valve assembly is provided. By way of example only, the assembly includes a plate (902) having a three-dimensional contour including a rim section (402, 920) surrounding a dome section (404, 922) and a plurality of openings (218, 918) formed in at least one of the rim section (402, 920) and the dome section (404, 922), the plate (902) comprising a material having no recast material thereon.
    • 提供一种制造噪声衰减器(206)的方法(700)。 ,实施例中通过实施例的方式,所述方法(700)包括成形(702)的板(902)具有三维轮廓,并且形成开口(218,918)通过成形板的多个(902 )与(磨料流体射流,从而形成排气阀噪声衰减器206)。 在另一个中,提供了一个实施方案排放阀组件。 仅通过示例的方式,该组件包括在形成的板(902)具有三维轮廓,其包括轮缘部(402,920)周围的圆顶部分(404,922)和开口(218,918)的多元 至少轮缘部(402,920)和所述圆顶部分的一个(404,922),包括其上具有无重铸材料的材料的板(902)。