会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明公开
    • A monocentric autostereoscopic viewing apparatus using resonant fiber-optic image generation
    • Eine monozentrische,autostereoscopische Anzeigevorrichtung mit einer resonancenanten faseroptischen Bilderzeugung
    • EP1351092A1
    • 2003-10-08
    • EP03075664.7
    • 2003-03-07
    • EASTMAN KODAK COMPANY
    • Agostinelli, John A., c/o Eastman Kodak CompanyCobb, Joshua M., c/o Eastman Kodak Company
    • G02B27/22H04N13/00
    • G02B27/225G02B6/3502G02B6/3566G02B26/101G02B2006/0098
    • A substantially monocentric arrangement of optical components provides stereoscopic display of a real image, electronically scanned by resonant actuation of a resonant fiber scanner (137) using a flexible optical waveguide and projected toward a curved retro-reflective surface (124). To form each left and right intermediate image component, separate left and right image generation systems (70) each comprise a resonant fiber scanner (137) that itself comprises a resonant cantilever portion (139) of optical fiber (138) that directs a modulated beam in a curved pattern for projection, such as by a ball lens assembly (30). A monocentric arrangement of optical components images the left and right ball lens pupil at the corresponding left and right viewing pupil (14) of the observer (12) and essentially provides a single center of curvature for projection components. Use of such a monocentric arrangement provides an exceptionally wide field of view with large viewing pupils (14).
    • 光学部件的基本上单中心布置提供了通过谐振光纤扫描器(137)的谐振致动而使用柔性光波导电子扫描的真实图像的立体显示,并向弯曲的反射表面(124)投影。 为了形成每个左和右中间图像分量,单独的左和右图像生成系统(70)各自包括谐振光纤扫描器(137),其自身包括光纤(138)的共振悬臂部分(139),其引导调制束 用于投影的弯曲图案,例如通过球透镜组件(30)。 光学部件的单中心布置将观察者(12)的相应左和右视瞳(14)上的左右球透镜光瞳图像化,并且基本上为投影部件提供单个曲率中心。 使用这种单中心布置提供了与大观察瞳孔(14)非常宽的视场。
    • 5. 发明公开
    • Improved superconductive layer on monocrystalline substrate and process for its preparation
    • 单晶衬底上提高超导层,以及它们的制备方法。
    • EP0531236A2
    • 1993-03-10
    • EP92420287.2
    • 1992-08-31
    • EASTMAN KODAK COMPANY
    • Hung, Liang-Sun, c/o Eastman Kodak CompanyAgostinelli, John A., c/o Eastman Kodak CompanyPaz-pujalt, Gustavo R., c/o Eastman Kodak Company
    • H01L39/24
    • H01L39/2425H01L39/126H01L39/2458
    • A superconductive article is disclosed comprised of a substrate having a monocrystalline oxide surface supporting a superconductive crystalline oxide layer satisfying the formula:

              P₂Sr₂Ca n Cu n+1 O 6+2n-z


      where
         P represents Bi 1-z Pb z ;
         n is zero, 1 or 2; and
         z is 0 to 0.30.
      At least half of the crystal unit cells of the superconductive crystalline oxide layer are oriented with their c-axes normal to the substrate surface and with their minor axes relatively angularly aligned within a deviation range of less than 5°. The superconductive crystalline oxide layer is formed by (a) applying to the substrate surface a coating solution comprised of a volatilizable film forming solvent and metal-ligand compounds of each of P, Sr, Ca and Cu containing at least one thermally volatilizable organic ligand, with at least one fluoro-substituted organic compound providing a F:Sr atomic ratio of at least 3:1, (b) removing the volatile components of the coating by heating and (c) forming the residual components of the coating into the superconductive crystalline oxide layer by firing to a temperature in the range of from 800 to 860°C.
    • 超导制品是游离缺失盘具有单晶氧化物表面支撑超导结晶氧化物层满足下式的基片包括:P2Sr2CanCun + 1o6 + 2N-Z其中P darstellt的Bi 1-zPbz; n是零,1或2; 且z是0至12:30。 超导结晶氧化物层的晶体晶胞中的至少一半的取向为它们的c轴垂直于基片表面并与他们的短轴相对小于5℃的偏差范围内成角度地对准。 超导结晶氧化物层由形成(a)施加于基板表面包括可挥发的成膜每个P的的溶剂和金属 - 配体的化合物,Sr,Ca和含Cu的至少一种可热挥发的有机配体的涂覆溶液, 与提供A F至少一个氟substituiertem有机化合物:至少3锶原子比:1,(b)在形成涂层的剩余组分引入到超导结晶加热和(c)除去所述涂层的挥发性组分 通过在800至860℃的的范围内烧成的温度下的氧化层
    • 9. 发明公开
    • Improved superconductive layer on monocrystalline substrate and process for its preparation
    • 改善单晶基板上的超导层及其制备工艺
    • EP0531236A3
    • 1993-05-12
    • EP92420287.2
    • 1992-08-31
    • EASTMAN KODAK COMPANY
    • Hung, Liang-Sun, c/o Eastman Kodak CompanyAgostinelli, John A., c/o Eastman Kodak CompanyPaz-pujalt, Gustavo R., c/o Eastman Kodak Company
    • H01L39/24
    • H01L39/2425H01L39/126H01L39/2458
    • A superconductive article is disclosed comprised of a substrate having a monocrystalline oxide surface supporting a superconductive crystalline oxide layer satisfying the formula:
              P₂Sr₂Ca n Cu n+1 O 6+2n-z
      where
         P represents Bi 1-z Pb z ;
         n is zero, 1 or 2; and
         z is 0 to 0.30.
      At least half of the crystal unit cells of the superconductive crystalline oxide layer are oriented with their c-axes normal to the substrate surface and with their minor axes relatively angularly aligned within a deviation range of less than 5°. The superconductive crystalline oxide layer is formed by (a) applying to the substrate surface a coating solution comprised of a volatilizable film forming solvent and metal-ligand compounds of each of P, Sr, Ca and Cu containing at least one thermally volatilizable organic ligand, with at least one fluoro-substituted organic compound providing a F:Sr atomic ratio of at least 3:1, (b) removing the volatile components of the coating by heating and (c) forming the residual components of the coating into the superconductive crystalline oxide layer by firing to a temperature in the range of from 800 to 860°C.
    • 公开了一种超导制品,其包括具有支撑超导结晶氧化物层的单晶氧化物表面的衬底,其满足以下式:P2Sr2CanCun + 1O6 + 2n-z,其中P表示Bi1-zPbz; n为零,1或2; z为0〜0.30。 超导结晶氧化物层的至少一半的晶体单元电池的c轴垂直于衬底表面并且其短轴在小于5°的偏差范围内相对角度地对准。 超导结晶氧化物层通过以下步骤形成:(a)将由可挥发成膜溶剂构成的涂布溶液和含有至少一种可热挥发的有机配体的P,Sr,Ca和Cu各自的金属 - 配体化合物施加到基材表面, 与至少一种提供至少3:1的F:Sr原子比的氟取代的有机化合物,(b)通过加热除去涂层的挥发性组分,和(c)将涂层的残留组分形成为超导结晶 氧化物层的烧成温度为800〜860℃的范围