会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明公开
    • Water-repellent glass pane and method for producing same
    • Wasserabweisende Glasscheibe und Verfahren zu deren Herstellung
    • EP0825157A2
    • 1998-02-25
    • EP97114294.8
    • 1997-08-19
    • CENTRAL GLASS COMPANY, LIMITED
    • Akamatsu, YoshinoriHamaguchi, ShigeoNishida, YoshihiroYamamoto, Hideki
    • C03C17/30B05D1/18
    • C03C17/30C09K3/18Y10T428/315Y10T428/31525Y10T428/3154Y10T428/31612
    • The invention relates to a water-repellent glass pane having a glass substrate and a water-repellent film formed thereon. This glass pane is prepared by a first or second method. The first method includes sequential steps of (a) mixing together a raw material for producing the water-repellent film, an organic solvent for diluting the raw material, and water for hydrolyzing the raw material, such that the raw material is subjected to hydrolysis and then to dehydration and polycondensation, thereby to turn a mixture of the raw material, the organic solvent and the water into a sol; (b) adjusting water content of the sol, thereby to prepare a coating liquid; and (c) applying the coating liquid to the glass substrate, in an atmosphere having a first temperature and a relative humidity. The second method includes sequential steps of: (a) subjecting a surface of the glass substrate to an abrasive treatment; (b) subjecting the surface of the glass substrate to an acid treatment; and (c) applying a coating liquid to the surface of the glass substrate. The glass pane prepared by the first or second method is superior in abrasion resistance, sunshine resistance, hardness, adhesion to the glass substrate, and water-repellency for a long time.
    • 本发明涉及一种具有形成在其上的玻璃基板和防水膜的防水玻璃板。 该玻璃板通过第一种或第二种方法制备。 第一种方法包括以下顺序步骤:(a)将用于制备防水膜的原料,用于稀释原料的有机溶剂和用于水解原料的水混合在一起,使原料进行水解, 然后进行脱水缩聚,从而将原料,有机溶剂和水的混合物变成溶胶; (b)调节溶胶的含水量,由此制备涂布液; 和(c)在具有第一温度和相对湿度的气氛中将涂布液涂布到玻璃基板上。 第二种方法包括以下顺序的步骤:(a)对玻璃基板的表面进行磨料处理; (b)对玻璃基板的表面进行酸处理; 和(c)将涂布液施加到玻璃基板的表面。 通过第一种或第二种方法制备的玻璃板在耐磨性,耐日光性,硬度,与玻璃基材的粘附性以及长时间的拒水性方面都是优异的。
    • 7. 发明公开
    • Glass plate with water-repellent film and method for producing same
    • ung ung ung ung ung ung ung ung ung ung ung ung ung ung ung ung ung
    • EP0891953A1
    • 1999-01-20
    • EP97112061.3
    • 1997-07-15
    • CENTRAL GLASS COMPANY, LIMITED
    • Akamatsu, YoshinoriYuasa, AkiraYamamoto, Hideki
    • C03C17/30C03C17/42C08J7/04
    • C03C17/42C03C2217/76
    • The invention relates to a water-repellent glass plate having a glass substrate; a first film which is formed on the glass substrate and is made of silica; and a water-repellent second film formed on the first film. This glass plate is prepared by a method including steps of: (1) applying a first coating liquid containing tetraisocyanate silane to the glass substrate, thereby to form thereon a precursory film; and (2) subjecting the precursory film to a drying at room temperature or to a heat treatment, thereby to prepare the first film; and (3) applying a second coating liquid to the first film, thereby to form the second film on the first film. The tetraisocyanate silane of the step (1) is curable at room temperature. The second coating liquid contains an alkoxysilane having at least one fluorocarbon group substituted for at least one hydrogen atom thereof. By the provision of the first film, the water-repellent second film becomes superior in solar resistance, abrasion resistance, chemical resistance, and adhesion to the glass substrate.
    • 本发明涉及一种具有玻璃基板的防水玻璃板; 形成在玻璃基板上并由二氧化硅制成的第一膜; 以及形成在第一膜上的防水第二膜。 该玻璃板通过以下步骤制备:(1)将含有四异氰酸酯硅烷的第一涂布液涂布在玻璃基板上,由此在其上形成前体膜; 和(2)在室温下对前体膜进行干燥或热处理,由此制备第一膜; 和(3)将第二涂布液施加到第一膜上,从而在第一膜上形成第二膜。 步骤(1)的四异氰酸酯硅烷在室温下是可固化的。 第二涂布液含有至少一个氟代烃基取代至少一个氢原子的烷氧基硅烷。 通过设置第一膜,防水性第二膜在耐太阳能,耐磨性,耐化学性和与玻璃基板的粘附性方面变得优异。
    • 8. 发明公开
    • Water-repellent glass pane and method for producing same
    • 防水玻璃板及其制造方法
    • EP0825157A3
    • 1998-08-19
    • EP97114294.8
    • 1997-08-19
    • CENTRAL GLASS COMPANY, LIMITED
    • Akamatsu, YoshinoriHamaguchi, ShigeoNishida, YoshihiroYamamoto, Hideki
    • C03C17/30B05D1/18
    • C03C17/30C09K3/18Y10T428/315Y10T428/31525Y10T428/3154Y10T428/31612
    • The invention relates to a water-repellent glass pane having a glass substrate and a water-repellent film formed thereon. This glass pane is prepared by a first or second method. The first method includes sequential steps of (a) mixing together a raw material for producing the water-repellent film, an organic solvent for diluting the raw material, and water for hydrolyzing the raw material, such that the raw material is subjected to hydrolysis and then to dehydration and polycondensation, thereby to turn a mixture of the raw material, the organic solvent and the water into a sol; (b) adjusting water content of the sol, thereby to prepare a coating liquid; and (c) applying the coating liquid to the glass substrate, in an atmosphere having a first temperature and a relative humidity. The second method includes sequential steps of: (a) subjecting a surface of the glass substrate to an abrasive treatment; (b) subjecting the surface of the glass substrate to an acid treatment; and (c) applying a coating liquid to the surface of the glass substrate. The glass pane prepared by the first or second method is superior in abrasion resistance, sunshine resistance, hardness, adhesion to the glass substrate, and water-repellency for a long time.
    • 本发明涉及一种具有玻璃基板和形成在其上的防水膜的防水玻璃板。 该玻璃板通过第一种或第二种方法制备。 第一种方法包括以下顺序步骤:(a)将用于制造防水膜的原材料,用于稀释原材料的有机溶剂和用于水解原材料的水混合在一起,使得原材料经受水解并且 然后进行脱水和缩聚,从而将原料,有机溶剂和水的混合物转化为溶胶; (b)调节溶胶的含水量,从而制备涂布液; 和(c)在具有第一温度和相对湿度的气氛中将涂布液施涂到玻璃基材上。 第二种方法包括以下顺序步骤:(a)使玻璃基材的表面经受研磨处理; (b)对玻璃基板的表面进行酸处理; 和(c)将涂布液施加到玻璃基材的表面上。 通过第一或第二种方法制备的玻璃板在耐磨性,抗日光性,硬度,对玻璃基材的粘合性和长期的防水性方面优异。