    • 5. 发明公开
    • LOW-YIELD-RATIO ULTRA-HIGH-STRENGTH HOT-ROLLED Q&P STEEL AND PRODUCTION METHOD THEREFOR
    • 低屈服比超高强度热轧Q&P钢及其生产方法
    • EP3235920A1
    • 2017-10-25
    • EP15869172.5
    • 2015-11-24
    • Baoshan Iron & Steel Co., Ltd.
    • WANG, HuanrongYANG, AnaWANG, Wei
    • C22C38/14C22C38/12C21D8/02
    • Disclosed is a low yield ratio and superhigh-strength hot-rolled Q&P steel and a method for manufacturing the same, having the following chemical composition in weight percentage: C: 0.2-0.3%, Si: 1.0-2.0%, Mn: 1.5-2.5%, P: ≤ 0.015%, S: ≤ 0.005%, Al: 0.5-1.0%, N: ≤ 0.006%, Nb: 0.02-0.06%, Ti: ≤ 0.03%, O: ≤ 0.003%, and the balance being Fe and inevitable impurities. The manufacture method comprises stepped cooling process to finally obtain a three-phase structure containing a certain volume fraction of proeutectoid ferrite + a certain volume fraction of martensite + a certain volume fraction of residual austenite. By controlling the relative contents of the three different phases, a low yield ratio and superhigh-strength hot-rolled Q&P steel having an excellent comprehensive performance which has a yield strength of ≥ 600 MPa and a tensile strength of ≥ 1300 Mpa as well as a good elongation and a low yield ratio, shows an excellent match of high plasticity and can be applied in the field of steels requiring easy deformabilities and wear-resistances, is obtained.
    • 本发明公开了一种低屈服比和超高强度热轧Q&P钢及其制造方法,其具有以下重量百分比的化学组成:C:0.2-0.3%,Si:1.0-2.0%,Mn:1.5- 2.5%,P:≤0.015%,S:≤0.005%,Al:0.5-1.0%,N:≤0.006%,Nb:0.02-0.06%,Ti:≤0.03%,O:≤0.003%,余量 是铁和不可避免的杂质。 该制造方法包括阶梯式冷却工艺,最终得到含有一定体积分数的先共析铁素体+一定体积分数的马氏体+一定体积分数的残余奥氏体的三相组织。 通过控制三种不同相的相对含量,具有屈服强度≥600MPa,拉伸强度≥1300MPa的综合性能优异的低屈服比和超高强度热轧Q&P钢以及 良好的伸长率和低的屈服比,表现出高塑性的极佳匹配,并且可以应用于需要易变形性和耐磨损性的钢领域。