热词
    • 1. 发明公开
    • LAMINATED PLATE, AND METHOD OF PRODUCING LAMINATED PLATE
    • LERINITE PLATTE UND VERFAHREN ZUR FERTIGUNG EINER LAMINIERTEN PLATTE
    • EP3138689A1
    • 2017-03-08
    • EP16185665.3
    • 2016-08-25
    • Asahi Glass Company, Limited
    • NOTSU, KeijiSADAKANE, ShunsukeNARITA, MakotoNISHIHAMA, Jirou
    • B32B17/10
    • B32B17/10036B32B17/10137B32B17/1055B32B17/10889B32B2250/40B32B2605/006
    • A laminated plate includes a first plate; a second plate; and an intermediate film for bonding the first plate and the second plate, wherein the first plate includes a first main surface arranged at a side opposite to the intermediate film, and a second main surface that contacts the intermediate film, wherein the second plate has a third main surface that contacts the intermediate film, and a fourth main surface arranged at a side opposite to the intermediate film, wherein, upon the bonding by the intermediate film being released, a radius of curvature of the second main surface is smaller than that of the third main surface both in a transverse section and in a longitudinal section, and wherein a maximum value of bending compressive stress at an outer peripheral portion of the fourth main surface is less than or equal to 100 MPa.
    • 层压板包括第一板; 第二盘 以及用于接合所述第一板和所述第二板的中间膜,其中所述第一板包括布置在与所述中间膜相对的一侧的第一主表面和与所述中间膜接触的第二主表面,其中所述第二板具有 与中间膜接触的第三主表面和布置在与中间膜相对的一侧的第四主表面,其中当中间膜被粘合时,第二主表面的曲率半径小于 第三主表面在横截面和纵向截面中,并且其中第四主表面的外周部分处的弯曲压缩应力的最大值小于或等于100MPa。
    • 3. 发明公开
    • LAMINATED PLATE
    • 层压板
    • EP3189965A1
    • 2017-07-12
    • EP16204319.4
    • 2016-12-15
    • ASAHI GLASS COMPANY, LIMITED
    • NOTSU, KeijiNAKANO, Atsushi
    • B32B17/10
    • B32B17/10155B32B3/263B32B17/10036B32B17/10137B32B17/10293B32B17/10889B32B2307/412B32B2605/006B32B2605/08
    • A laminated plate includes first and second plates bonded to each other via an intermediate film. The laminated plate further includes a first main surface of the first plate and a fourth main surface of the second plate arranged on sides opposite to the intermediate film, respectively; and a second main surface of the first plate and a third main surface of the second plate being in contact with the intermediate film, respectively. A thickness of the first plate is thicker than a thickness of the second plate. In at least a part of an outer periphery of the laminated plate, on a cross-sectional surface orthogonal to the outer periphery, the first plate has a first linear chamfered part which extends diagonally to the second main surface, and the second plate is located on an inner surface side of an extended line of the first linear chamfered part.
    • 层压板包括通过中间膜彼此结合的第一和第二板。 层叠板还包括分别布置在与中间膜相对的侧上的第一板的第一主表面和第二板的第四主表面; 并且第一板的第二主表面和第二板的第三主表面分别与中间膜接触。 第一板的厚度比第二板的厚度厚。 在所述层叠板的外周的至少一部分的与所述外周正交的截面上,所述第一板具有相对于所述第二主面倾斜地延伸的第一直线状的倒角部,所述第二板位于 在第一直线倒角部的延长线的内表面侧。