    • ATTRITION RESISTANT, SHAPED, CRYSTALLINE Mg-Al-Si-CONTAINING CLAY-CONTAINING BODIES
    • 耐磨,成形,结晶含Mg-Al-Si的含粘土物体
    • EP1204474B1
    • 2005-03-16
    • EP00956420.4
    • 2000-08-11
    • Akzo Nobel N.V.
    • STAMIRES, DennisO'CONNER, PaulJONES, William
    • B01J21/16B01J37/00C04B33/00
    • B01J37/0009B01J21/16B01J23/007C01B33/40
    • The present invention is directed to a process for the preparation of crystalline Mg-Al-Si-containing clay-containing bodies from sources comprising an aluminium source, a magnesium source, and a silicon source, comprising the steps of: a) preparing a precursor mixture; b) shaping the precursor mixture to obtain shaped bodies; c) optionally thermally treating the shaped bodies; and d) aging to obtain crystalline Mg-Al-Si-containing clay-containing bodies. The quintessence of the present invention is that the bodies are shaped prior to the forming of the crystalline clay in said bodies. This results in very attrition resistant bodies, without the need to add a binder material. The crystalline clay is formed from an aluminium source, a magnesium source, and, a silicon source. If only an aluminium source and a magnesium source are present, hydrotalcite is formed. If an aluminium source, a magnesium source, and a silicon source are present, saponite or montmorillonite is formed.
    • 本发明涉及一种从包含铝源,镁源和硅源的来源制备含结晶Mg-Al-Si的含粘土体的方法,包括以下步骤:a)制备前体 混合物; b)使前体混合物成形以获得成形体; c)任选地热处理成形体; 和d)老化以获得含结晶Mg-Al-Si的含粘土体。 本发明的精髓在于,在所述物体中形成结晶粘土之前,所述物体被成形。 这导致非常耐磨的物体,而不需要添加粘合剂材料。 结晶粘土由铝源,镁源和硅源形成。 如果仅存在铝源和镁源,则形成水滑石。 如果存在铝源,镁源和硅源,则形成皂石或蒙脱石。