    • METHOD FOR PRODUCING CURED PRODUCT OF EPISULFIDE-BASED RESIN
    • VERFAHREN ZUR HERSTELLUNG EINESGEHÄRTETENPRODUKTS AUS EPISULFIDBASIERTEM HARZ
    • EP3135710A1
    • 2017-03-01
    • EP15782270.1
    • 2015-04-20
    • Mitsubishi Gas Chemical Company, Inc.
    • NAMIKI KousukeFUSE SawakoKOSHIISHI EijiFURUKAWA KikuoHORIKOSHI Hiroshi
    • C08G75/08B29C39/02B29C39/24B29C39/38G02B1/04G02C7/00B29L11/00
    • The present invention can provide a method for producing a cured product of an episulfide-based resin, the method having: (A) a step for obtaining a composition for a resin by mixing compound (a), compound (b) and a polymerization catalyst; (B) a step for pouring the composition for a resin into a mold; and (C) a step in which, by increasing the temperature of a heating medium, the composition for a resin is polymerized in the heating medium that contains a liquid having a thermal conductivity of 0.2 W/m·K or higher, or in a shower of the heating medium. The maximum temperature of the heating medium in step (C) is 55 to 110°C. (a) A compound which has two episulfide groups per molecule and which is represented by formula (1):

      wherein m represents an integer from 0 to 4 and n represents an integer from 0 to 2 (b) A compound having one or more thiol groups per molecule.
    • 本发明可以提供一种制备环硫系树脂固化物的方法,该方法具有以下步骤:(A)通过混合化合物(a),化合物(b)和聚合催化剂得到树脂组合物的步骤 ; (B)将树脂用组合物倒入模具中的工序; 和(C)通过增加加热介质的温度,在含有导热率为0.2W / m·K以上的液体的加热介质中,或者在 淋浴的加热介质。 步骤(C)中加热介质的最高温度为55〜110℃。 (a)每分子具有两个环硫基并由式(1)表示的化合物:其中m表示0至4的整数,n表示0至2的整数(b)具有一个或多个硫醇的化合物 每个分子。
    • 85. 发明公开
    • FORMWERKZEUG MIT VERDREHSICHER WIE AUCH SCHWIMMEND GELAGERTEN WERKZEUGKOMPONENTEN
    • 与扭曲以及浮动工具ELEMENTS模具
    • EP2933084A1
    • 2015-10-21
    • EP15164053.9
    • 2015-04-17
    • Thielke, Joachim
    • Thielke, Joachim
    • B29C39/24B29C33/00
    • B29C39/24B29C33/30B29C33/76B29C45/4005
    • Die Erfindung betrifft ein Formwerkzeug (2) zur Formung von Werkstücken, das wenigstens ein erstes Formungsteil 4 aufweist, welches wiederum eine Kavität (8) für die Formung des Werkstückes aufweist. Ferner dient eine Halteeinrichtung (10) dem Halten von Bauteilen (12) am Formungsteil (4,6). Die Erfindung ist dadurch gekennzeichnet, dass die Halteeinrichtung (10) Lagerungsmittel (14) zur schwimmenden Bauteillagerung aufweist, die derart eingerichtet und ausgebildet sind, dass wenigstens ein Bauteil (12) in Umfangsrichtung (16) zu dessen Bauteilachse (18) verdrehgesichert und radial zu dessen Bauteilachse (18) entlang wenigstens einer ersten Führungsrichtung (20) bewegbar gelagert ist.
    • 本发明涉及一种模制工具(2),用于成形的工件,其具有至少一个第一成形部分4,这反过来又具有用于对工件的成形的腔体(8)。 此外,保持装置(10)是用于保持在成形部分(4.6)的组件(12)的。 本发明的特征在于,所述保持装置(10)的存储装置(14),用于浮动元件存储,其被如此布置和设计成使得在圆周方向(16)与组分轴线(18)的至少一个部件(12)固定以防止转动并沿径向 是沿着至少一个第一引导方向(20)可移动地支撑所述部件轴线(18)。
    • 86. 发明公开
    • METHOD FOR MANUFACTURING POLARIZING PLASTIC LENS
    • VERFAHREN ZUR HERSTELLUNG EINER POLARISIERENDEN KUNSTSTOFFLINSE
    • EP2921274A1
    • 2015-09-23
    • EP13854348.3
    • 2013-11-14
    • EHS Lens Philippines, Inc.
    • IHARA, MasakiSHIMIZU, HiroshiITO, YoshinobuSHIMIZU, ToshihikoTONOUCHI, Kenichi
    • B29C39/10B29C39/24G02B5/30G02C7/12B29L11/00
    • B29D11/00413B29C39/10B29C39/24B29D11/00442B29D11/00644B29K2629/04B29K2995/0034B29L2011/0016
    • An aspect of the present invention relates to a method of manufacturing a polarizing plastic lens, which comprises an upper mold positioning step of positioning an upper mold so that a nonmolding surface faces up and a molding surface faces down, an adhesive column forming step of discharging a thixotropic curable adhesive from a discharge nozzle positioned beneath the molding surface of the upper mold to form adhesive columns on a rim portion of the molding surface of the upper mold, a bonding step of bonding the upper mold and a polarizing film by means of the adhesive columns that have been formed, an adhesive column curing step of subjecting the adhesive columns to a curing treatment after the bonding step, a casting mold assembling step of assembling a casting mold having a cavity within which the polarizing film has been positioned with the upper mold to which the polarizing film has been bonded, a lower mold positioned opposite the upper mold so as to sandwich the polarizing film, and a sealing member maintaining a spacing between the upper mold and lower mold, and a polymerizing and curing step of casting a curable composition into the cavity, and polymerizing and curing the curable composition that has been cast to provide a polarizing plastic lens within which the polarizing film is positioned.
    • 本发明的一个方面涉及一种制造偏振塑料透镜的方法,该方法包括:上模定位步骤,定位上模以使非模制表面朝上并且模制表面朝下;粘合剂柱形成步骤, 来自位于上模具的模制表面下方的排放喷嘴的触变性固化粘合剂,以在上模具的模制表面的边缘部分上形成粘合剂柱,通过粘合步骤将上模和偏振膜粘合 已经形成的粘合剂柱,在接合步骤之后对粘合剂柱进行固化处理的粘合剂柱固化步骤,组装具有偏振膜已定位的空腔的铸模与上部 已经粘合了偏光膜的模具,与上模相对定位的下模,以夹持偏光膜 m,以及保持上模和下模之间的间隔的密封构件,以及将可固化组合物浇铸到空腔中的聚合和固化步骤,以及聚合和固化已浇铸的可固化组合物以提供偏振塑料透镜 其中偏振膜被定位。
    • 88. 发明公开
    • RTM METHOD
    • RTM-VERFAHREN
    • EP2818294A1
    • 2014-12-31
    • EP13751599.5
    • 2013-02-21
    • Toray Industries, Inc.
    • YAMAMOTO KohnosukeTSUJI SeijiWATANABE Kazuya
    • B29C39/24B29C39/42B29C39/44B29K105/08
    • B29C70/48B29C45/02B29C45/14786B29C45/1671B29C45/22B29C70/546B29K2105/0872B29L2009/00
    • An RTM method, which injects and impregnates resin from a plurality of injection ports into a preform placed inside the cavity of a molding die, wherein the plurality of injection ports are disposed in first positions in the central section of the cavity corresponding to positions of the preform located in a product area of an article to be finally molded and second positions located in the periphery of the cavity corresponding to positions outside the product area of the article to be finally molded or corresponding to positions inside the cavity but outside the preform area, and the timings for closing the injection ports after resin injection are made to be different from each other between the injection ports of the first positions and of the second positions. In an RTM method that injects resin from a plurality of injection ports, the invention is able to achieve both high-velocity resin impregnation and improvement of the quality of a molded article.
    • 一种RTM方法,其将树脂从多个注入口注入并浸渍到放置在模具模具的腔体内的预制件中,其中所述多个注射口设置在所述腔的中心部分的第一位置, 位于待最终模制的制品的产品区域中的预成型件和位于所述空腔的周边中的第二位置,所述第二位置对应于待最终模制的制品的产品区域外的位置,或对应于所述空腔内部但在所述预制件区域外部的位置, 在第一位置和第二位置的喷射口之间使树脂注入后关闭喷射口的定时彼此不同。 在从多个注入口注入树脂的RTM方法中,本发明能够实现高速树脂浸渍和提高成型制品的质量。
    • 89. 发明公开
    • Device and method for the production of a cosmetic product for make-up
    • Vorrichtung und Verfahren zur Herstellung eines kosmetischen Produktsfür化妆品
    • EP2781168A1
    • 2014-09-24
    • EP14158164.5
    • 2014-03-06
    • CHROMAVIS S.p.A.
    • Larceri, NicolaMoroni, Fabio
    • A45D40/16A61Q1/12A61K8/02B29C39/24
    • B29C33/44A45D33/006A45D33/18A45D40/16A45D40/24A61K8/0237B29C43/18B29C43/20B29C43/203B29C43/34B29C2043/181
    • A device for accurately dosing cosmetic pastes in multicolour form on a base for the production of a cosmetic product for make-up, comprising a base element adapted to house a base, a mould which moves at least between an opening position and a closing position, said mould having at least one partition which divides a surface thereof facing the base element into at least two compartments, a peripheral element provided with walls which define an opening with shape similar to the perimeter shape of the mould and in which the mould is at least partially housed when it is in said closed position, said peripheral element being provided with at least two channels which run into said opening and protrude into it at least partially, the device providing means adapted to prevent the gluing of said cosmetic paste at least to the wall of the mould facing the base element.
    • 一种用于在用于化妆的化妆品的生产用基础上以多色形式准确地配量化妆品糊剂的装置,包括适于容纳基底的基底元件,至少在打开位置和关闭位置之间移动的模具, 所述模具具有至少一个将面向所述基座元件的表面划分成至少两个隔室的隔板,设置有壁的外围元件,所述外围元件限定具有类似于所述模具的周边形状的形状的开口,并且其中所述模具至少 当所述外围元件处于所述关闭位置时被部分地容纳,所述外围元件设置有至少两个通道,所述至少两个通道至少部分地进入所述开口并突出到所述开口中,所述装置提供装置适于防止所述化妆品糊料至少胶粘到 模具的壁面向基座元件。