热词
    • 62. 发明公开
    • HEAT-SHRINKABLE POLYESTER-BASED FILM ROLL
    • EP3689948A1
    • 2020-08-05
    • EP18861059.6
    • 2018-09-03
    • Toyobo Co., Ltd.
    • HARUTA, MasayukiTABOTA, Norimi
    • C08J5/18
    • To provide a heat-shrinkable polyester-based film roll having a favorable winding property, which is particularly favorable with respect to sag. A heat-shrinkable polyester-based film roll, which is obtained by winding a heat-shrinkable polyester-based film that has a shrinkage ratio of 30% or more in a film main shrinkage direction in hot water at 90°C for 10 seconds, the heat-shrinkable polyester film and the film roll satisfying following requirements (1) to (5) : (1) a winding length of the film roll is 2000 m or more and 25000 m or less; (2) a width of the film roll is 400 mm or more and 2500 mm or less; (3) a thickness of the film is 5 µm or more and 40 µm or less; (4) in thickness unevenness in a width direction of the film on a surface layer of the film roll, there are positions having concave thickness patterns, and in a concave portion that has a maximum thickness difference (maximum concave portion), thickness unevenness in the maximum concave portion, which is obtained from the maximum thickness difference in the maximum concave portion and an average thickness of the film is 10% or less; and (5) winding hardness of the surface layer of the film roll is 400 or more and 800 or less.
    • 66. 发明公开
    • HEAT-SHRINKABLE POLYESTER-BASED FILM AND PACKAGING BODY
    • 可热收缩的聚酯基薄膜和包装体
    • EP3275627A1
    • 2018-01-31
    • EP16768788.8
    • 2016-03-23
    • Toyobo Co., Ltd.
    • HARUTA, MasayukiTABOTA, Norimi
    • B29C61/06B29C55/02C08J5/18
    • The present invention is to provide a heat-shrinkable polyester film in which the differences in physical properties in the width direction are reduced even if the film has a small thickness. The heat-shrinkable polyester film has a main shrinkage direction in a width direction of the film and satisfies following requirements (1) to (5):
      (1) the film has a thickness of 6 µm or more and 27 µm or less;
      (2) a maximum value of the molecular orientation angle is 5 degrees or less;
      (3) a hot-water shrinkage at 90°C in the width direction of the film determined for each of the samples is 40% or more and 85% or less;
      (4) a difference between a maximum value and a minimum value of the hot-water shrinkage at 90°C in the width direction of the film is 2% or less;
      (5) a difference between a maximum value and a minimum value of the maximum shrinkage stress at 90°C in the width direction of the film is less than 0.3 MPa.
    • 本发明提供一种热收缩性聚酯薄膜,即使薄膜厚度薄,其宽度方向的物性差异也会减小。 热收缩性聚酯薄膜在薄膜的宽度方向上具有主收缩方向,并且满足以下要求(1)至(5):(1)薄膜具有6μm以上且27μm以下的厚度; (2)分子取向角的最大值为5度以下, (3)对于每个样品确定的膜在宽度方向上在90℃下的热水收缩率为40%以上且85%以下; (4)膜的宽度方向的90℃时的热水收缩率的最大值与最小值的差为2%以下, (5)膜的宽度方向的90℃时的最大收缩应力的最大值与最小值的差小于0.3MPa。