    • 55. 发明公开
    • UNIFORM GRAIN SIZE IN HOT WORKED SPINODAL ALLOY
    • ELEER FOLLORGEKORNGRÖSSEIN EINER WARMVERFORMTEN SPINODALEN LEGIERUNG
    • EP2971214A1
    • 2016-01-20
    • EP14769727.0
    • 2014-03-12
    • Materion Corporation
    • LONGENBERGER, Edward
    • C22F1/08C22F1/10C22C9/06
    • C22F1/08C22C9/00C22C9/06
    • Processes for producing a uniform grain hot worked spinodal alloy are disclosed. The processes generate a uniform grain spinodal alloy without cracking and without the need for a homogenization step. The processes include providing an as-cast spinodal alloy, heating the as-cast spinodal alloy between 1200 and 1300° F. for approximately 12 hours and hot working, allowing the spinodal alloy to cool, performing a second hot work on the as-cast spinodal alloy after it has been heated to 1700° F. for a defined time period, exposing the alloy to a third temperature, performing a second hot work reduction, and cooling the alloy again.
    • 公开了用于生产均匀晶粒热加工旋节状合金的方法。 这些方法产生均匀的晶体旋节状合金,而不会产生裂纹,而不需要均化步骤。 这些方法包括提供铸态亚稳态合金,在1200和1300°F之间加热铸造旋节状合金约12小时并进行热加工,允许旋节状合金冷却,对铸态进行第二次热加工 在将其加热至1700°F一段规定时间后,将合金暴露于第三温度,进行第二热作业还原,再次冷却合金。
    • 56. 发明公开
    • ULTRA HIGH STRENGTH COPPER-NICKEL-TIN ALLOYS
    • ULTRAHOCHFESTE KUPFER-NICKEL-ZINN-LEGIERUNGEN
    • EP2971199A1
    • 2016-01-20
    • EP14769653.8
    • 2014-03-11
    • Materion Corporation
    • WETZEL, John F.SKORASZEWSKI, Ted
    • C22C9/00C22F1/08
    • The present disclosure relates to ultra high strength wrought copper—nickel—tin alloys and processes for improving the yield strength of the copper—nickel—tin alloy such that the resulting 0.2% offset yield strength is at least 175 ksi. The alloy includes about 14.5 wt % to about 15.5% nickel, about 7.5 wt % to about 8.5% tin, and the remaining balance is copper. The steps include cold working the copper—nickel—tin alloy wherein the alloy undergoes between 50%-75% plastic deformation. The alloy is heat treated at elevated temperatures between about 740° F. and about 850° F. for a time period of about 3 minutes to 14 minutes.
    • 本公开内容涉及超高强度锻造铜 - 镍锡合金和用于提高铜 - 镍 - 锡合金的屈服强度的方法,使得所得到的0.2%偏移屈服强度至少为175ksi。 该合金包括约14.5重量%至约15.5重量%的镍,约7.5重量%至约8.5重量%的锡,余下的其余为铜。 这些步骤包括对铜 - 镍 - 锡合金进行冷加工,其中合金经历50%-75%的塑性变形。 该合金在约740°F至约850°F的高温下热处理约3分钟至14分钟的时间。