会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 91. 发明公开
    • VERFAHREN ZUR TROCKNUNG UND HERSTELLUNG VON MIKROPORÖSEN TEILCHEN SOWIE EINE VORRICHTUNG ZUR TROCKNUNG
    • VERFAHREN ZUR TROCKNUNG UND HERSTELLUNG VONMIKROPORÖSENTEILCHEN SOWIE EINE VORRICHTUNG ZUR TROCKNUNG
    • EP1062181A2
    • 2000-12-27
    • EP99915573.2
    • 1999-03-11
    • BASF AKTIENGESELLSCHAFT
    • TEICH, FriedhelmSCHELLING, HeinerKÖSTER, HerbertKRATZER, HorstREICHERT, WolfgangGALL, MartinZIEGLER, Bernd
    • C01B33/00
    • F26B7/00
    • The invention relates to a method for drying microporous particles containing fluid in which the heat required for increasing the temperature is supplied by means of convection by reducing the interfacial tension of the fluid, preferably to 0 to 1/10, especially to 0 to 1/20, pertaining to the interfacial tension of the fluid at room temperature, by correspondingly increasing the temperature when the pressure of the fluid is at a near-critical to supercritical level. The invention also relates to a method for producing microporous, spatially cross-linked particles in which said drying method is applied. In addition, the invention relates to a device for carrying out the drying method. The device comprises a pressure vessel having an inner vessel and a pressure-carrying outer vessel. Said device also comprises suited measuring and regulating devices as well as pumping and heat exchange devices, whereby the inner vessel is provided for accommodating the particles which are to be dried. A gap is provided between the inner and outer vessels.
    • 本发明涉及一种用于干燥含有流体的微孔颗粒的方法,其中通过减少流体的界面张力借助于对流供应升高温度所需的热量,优选为0至1/10,特别是0至1 / 如图20所示,涉及流体在室温下的界面张力,通过相应地增加流体压力对于超临界水平的压力时的温度。 本发明还涉及一种生产微孔,空间交联颗粒的方法,其中应用了所述干燥方法。 另外,本发明涉及用于执行该干燥方法的装置。 该装置包括具有内部容器和承压外部容器的压力容器。 所述装置还包括合适的测量和调节装置以及泵送和热交换装置,其中内容器被设置用于容纳待干燥的颗粒。 内部和外部容器之间提供间隙。
    • 98. 发明公开
    • Preparation method for zircon powder
    • Verfahren zur Herstellung von Zirkonpulver。
    • EP0384728A2
    • 1990-08-29
    • EP90301857.0
    • 1990-02-21
    • TOSOH CORPORATION
    • Mori, ToshiyukiKubota, YoshitakaMitamura, TakashiKobayashi, Hidehiko
    • C01B33/00
    • C01B33/20C04B35/481
    • A preparation method for zircon powder, which comprises heating a feed powder mixture comprising:

      (1) silica and zirconia obtained by subjecting a liquid having a pH of not higher than 8 and containing silica and zirconia in a SiO₂/ZrO₂ molar ratio of substantially 1/1, to liquid-removing treatment, and
      (2) zircon in an amount of at least 0.1% by weight based on the total amount of said silica and zirconia,
      at a heating rate of not higher than 5°C/min from 1,200°C to a calcination temperature, and maintaining it at a calcination temperature of from 1,300° to 1,700°C for from 1.0 to 24 hours, or from 700° to 1,200°C over a period of at least 16 hours and maintaining it at a temperature of from 1,300° to 1,700°C for at least 10 hours.
      A method of making a mixture containing silica and zirconia which comprises dissolving (1) a silicon alkoxide and (2) a reaction mixture of a zirconium alkoxide with a chelating agent, in an organic solvent and contacting the resulting mixed solution with at least the stoichiometric amount of water required for hydrolysis.
    • 一种锆石粉的制备方法,包括加热原料粉末混合物,其包括:(1)二氧化硅和氧化锆,其通过使具有不高于8的液体并且含有二氧化硅和氧化锆的SiO 2 / ZrO 2摩尔比基本为1 / 1进行除液处理,和(2)相对于二氧化硅和氧化锆的总量,至少0.1重量%的锆石以不高于5℃/分钟的加热速率从1200 DEG至煅烧温度,并将其在1300至1700℃的煅烧温度下保持1.0至24小时,或在700至1200℃的温度下在至少16小时的时间内保持,并保持在 温度为1300〜1700℃,保持10小时以上。 一种制备含有二氧化硅和氧化锆的混合物的方法,其包括将(1)硅醇盐和(2)烷氧基锆的反应混合物与螯合剂溶解在有机溶剂中,并将所得混合溶液与至少化学计量 水解所需的水量。