会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 3. 发明授权
    • Slide surface construction
    • 滑动面施工
    • US5882804A
    • 1999-03-16
    • US609444
    • 1996-03-01
    • Yusuke ToyodaMasamune TabataKenji DosakaTakahiro Gunji
    • Yusuke ToyodaMasamune TabataKenji DosakaTakahiro Gunji
    • C23C30/00F16C33/12B32B3/12B32B15/01B32B33/00
    • F16C33/12C23C30/00F16C2204/60Y10S384/912Y10S428/935Y10T428/1266Y10T428/12951Y10T428/12993
    • A slide surface construction is formed of an aggregate of metal crystals on a surface of a slide member. The area rate A of pyramid-shaped metal crystals in the slide surface is in the range of A.gtoreq.40%, and the oxygen (O) content and/or the phosphorous (P) content in the aggregate is in a range of 0.gtoreq.0.2% by weight and P.gtoreq.0.04% by weight. The slide surface takes on an intricate aspect due to the presence of the large number of hexagonal pyramid-shaped metal crystals and hence, has a good oil retention. In addition, the wearing of the hexagonal pyramid-shaped metal crystals is inhibited by an increase in hardness caused by the oxygen contained, and therefore, the oil retention is maintained. Thus, the slide surface construction exhibits an excellent seizure resistance. In addition to oxygen (O) and/or phosphorous (P), the elements that may be added to the aggregate include hydrogen (H), carbon (C) and boron (B).
    • 滑动面构造由滑动构件的表面上的金属结晶体形成。 滑石表面金字塔状金属晶体的面积率A在A> 40%的范围内,聚集体中的氧(O)含量和/或磷(P)含量在 0重量%= 0.2重量%,P> = 0.04重量%。 由于存在大量的六角锥形金属晶体,因此滑动表面具有复杂的方面,因此具有良好的保油性。 此外,六角锥形金属晶体的磨损由于所含氧引起的硬度的增加而被抑制,因此保持保油性。 因此,滑动面构造表现出优异的耐咬住性。 除了氧(O)和/或磷(P)之外,可以添加到骨料中的元素包括氢(H),碳(C)和硼(B)。
    • 4. 发明授权
    • High-hardness metal skin film
    • 高硬度金属皮肤膜
    • US5547771A
    • 1996-08-20
    • US424873
    • 1995-04-17
    • Takahiro GunjiMasamune TabataKenji DosakaKenji Hirose
    • Takahiro GunjiMasamune TabataKenji DosakaKenji Hirose
    • C23C30/00F16J1/02B32B15/00
    • C23C30/00F16J1/02Y10S428/935Y10T428/12951Y10T428/12993
    • A high-hardness metal skin film is formed of an aggregate of metal crystals. The area rate A of pyramid-shaped metal crystals in a surface of the skin film is in a range of A.gtoreq.40%. The aggregate contains at least one element selected from boron (B), carbon (C) and hydrogen (H) as an added element, wherein the B content is in a range of B.gtoreq.0.01% by weight, the C content is in a range of C.gtoreq.0.03% by weight, and the H content is in a range of H.gtoreq.0.01% by weight. The skin surface takes on an intricate aspect due to the presence of a large number pyramid-shaped metal crystals and hence, has a good oil retention. In addition, the wear of each pyramid-shaped metal crystal is inhibited by an increase in hardness produced with the containment of boron and/or carbon and/or hydrogen and therefore, the oil retention is maintained.
    • 高硬度金属皮膜由金属结晶体形成。 皮肤膜表面的棱锥状金属结晶的面积率A在A> 40%的范围内。 骨料含有选自硼(B),碳(C)和氢(H)中的至少一种元素作为添加元素,其中B含量在B> / = 0.01重量%的范围内,C含量为 在C> / = 0.03重量%的范围内,H含量在H> / = 0.01重量%的范围内。 由于存在大量的金字塔形金属晶体,所以皮肤表面复杂,因此具有良好的保油性。 此外,通过使含有硼和/或碳和/或氢的容纳物产生的硬度增加,每个金字塔形金属晶体的磨损被抑制,因此保持油保留。
    • 7. 发明授权
    • Functional copper skin film
    • 功能性铜皮膜
    • US5952114A
    • 1999-09-14
    • US622416
    • 1996-03-27
    • Takahiro GunjiMasamune TabataKenji Dosaka
    • Takahiro GunjiMasamune TabataKenji Dosaka
    • F16C33/12B32B15/20B23P9/00
    • F16C33/12Y10T428/12903Y10T428/12993
    • A Cu skin film is formed of an aggregate of Cu crystals. Pyramid-shaped Cu crystals and/or conical Cu crystals exist in the surface of the Cu skin film. The area rate A of the pyramid-shaped Cu crystals, the area rate A of the conical Cu crystals or the sum A of the area rates of these Cu crystals in the skin film surface are set in a range of A.gtoreq.40%. The skin film surface takes on an intricate aspect due to the existence of the infinite number of pyramid-shaped Cu crystals and/or conical Cu crystals. If such a Cu skin film is formed, for example, on a surface opposite from that surface of a backing of a slide bearing which is opposed to a rotary shaft, the Cu skin film exhibits a good oil retention and therefore seizure due to a fretting can be avoided.
    • 铜皮膜由Cu晶体的聚集体形成。 在Cu皮膜的表面存在金字塔形Cu晶体和/或锥形Cu晶体。 锥形Cu晶体的面积率A,锥形Cu晶体的面积率A或皮肤膜表面中这些Cu晶体的面积率的总和A设定在A> 40%的范围内 。 由于存在无数数量的金字塔形Cu晶体和/或锥形Cu晶体,皮膜表面具有复杂的方面。 如果这样的Cu皮膜例如形成在与旋转轴相对的滑动轴承的背衬的表面相对的表面上,则Cu皮膜显示出良好的保油性,因此由于微动而发生癫痫发作 可以避免。
    • 8. 发明授权
    • Slide surface construction and process for producing the same
    • 滑动面施工及其生产工艺
    • US5897968A
    • 1999-04-27
    • US616874
    • 1996-03-15
    • Kenji DosakaYusuke ToyodaMasamune TabataHiroshi Koinuma
    • Kenji DosakaYusuke ToyodaMasamune TabataHiroshi Koinuma
    • F16C9/04F16C33/12F16H55/06B32B15/18
    • F16H55/06F16C33/12F16C33/122F16C9/04F05C2201/021F05C2201/0448F16C2204/60Y10S384/912Y10S428/935Y10T428/12493Y10T428/12951Y10T428/12993
    • A slide surface construction of a slide bearing is formed of an aggregate of two different metal crystals. The sliding condition of a first region of the slide bearing is more severe than that of a second region. The (2hhh) oriented metal crystals having a body-centered cubic structure with their (2hhh) planes (by Miller indices) oriented toward a slide surface exist in the first region. The content S.sub.2hhh of the (2hhh) oriented metal crystals is set in a range of S.sub.2hhh .gtoreq.20%. These crystals have a high hardness and are in the form of fish-like metal crystals in the slide surface and hence, an aggregate of these metal crystals has a good oil retention. The (hhh) oriented metal crystals having a body-centered cubic structure with their (hhh) planes (by Miller indices) oriented toward a slide surface exist in the second region. The content S.sub.hhh of the (hhh) oriented metal crystals is set in a range of S.sub.hhh .gtoreq.40%. These crystals are in the form of hexagonal pyramid-shaped metal crystals and hence, an aggregate of these metal crystals has a good oil retention. Thus, it is possible for the two regions with different sliding conditions to exhibit an excellent sliding characteristic.
    • 滑动轴承的滑动表面结构由两种不同的金属晶体的聚集体形成。 滑动轴承的第一区域的滑动状态比第二区域的滑动状态更严重。 在第一区域中存在具有以体积为中心的立方结构的(2hhh)取向金属晶体及其朝向滑动表面的(2hhh)平面(通过米勒指数)。 (2hhh)取向金属晶体的含量S2hhh设定在S2hhh≥20%的范围内。 这些晶体具有高硬度并且在滑动表面中呈鱼状金属晶体的形式,因此这些金属晶体的聚集体具有良好的保油性。 在第二区域中存在具有以体积为中心的立方结构的(hhh)取向金属晶体及其(hhh)面(通过米勒指数)朝向滑动面。 (hhh)取向金属晶体的含量Shhh设定在Shhh≥40%的范围内。 这些晶体呈六角锥形金属晶体的形式,因此这些金属晶体的聚集体具有良好的保油性。 因此,具有不同滑动条件的两个区域可以表现出优异的滑动特性。
    • 10. 发明授权
    • Plasma reactor
    • 等离子体反应器
    • US07727489B2
    • 2010-06-01
    • US11374120
    • 2006-03-14
    • Atsuo KondouYasumasa FujiokaTakeshi SakumaMasaaki MasudaKenji DosakaKeizo Iwama
    • Atsuo KondouYasumasa FujiokaTakeshi SakumaMasaaki MasudaKenji DosakaKeizo Iwama
    • B01J19/08
    • H01J37/32009
    • A plasma reactor is provided with two or more plasma generating electrodes which are installed in series inside a gas passage in a casing, with each plasma generating electrode being electrically controlled independently. The surface area of the conductor on each unit electrode forming the plasma generating electrode installed on the upstream side of the gas passage is smaller than the surface area of the conductor on the unit electrode forming the plasma generating electrode installed on the downstream side of the gas passage. Plasma can be generated between each of the unit electrodes by supplying each of the plasma generating electrodes with independently controlled electric power. The plasma reactor can efficiently react specific components contained in the gas passing through the gas passage.
    • 等离子体反应器设置有两个或更多个等离子体产生电极,其串联安装在壳体中的气体通道内,每个等离子体产生电极被独立地电控制。 形成设置在气体通道上游侧的等离子体发生电极的各单位电极上的导电体的表面积小于形成设置在气体下游侧的等离子体发生电极的单位电极上的导体的表面积 通道。 可以通过向等离子体产生电极中的每一个提供独立控制的电力而在每个单元电极之间产生等离子体。 等离子体反应器可以有效地反应通过气体通道的气体中包含的特定组分。