    • AROMATIC POLYCARBONATE RESIN COMPOSITION AND MOLDED OBJECT MADE FROM THE SAME
    • 芳香族聚碳酸酯树脂组合物及其成型对象
    • US20090061220A1
    • 2009-03-05
    • US11817364
    • 2006-03-28
    • Akio NoderaYusuke Hayata
    • Akio NoderaYusuke Hayata
    • B32B27/00C08K5/053
    • C08L69/00C08L27/18C08L51/085C08L63/00Y10T428/269C08L2666/02
    • There is provided an aromatic polycarbonate resin composition having excellent flame retardancy, mechanical properties and fluidity and affording a thin-walled molded article.The aromatic polycarbonate resin composition includes a resin component containing (A) 90 to 99.5% by mass of an aromatic polycarbonate resin and (B) 10 to 0.5% by mass of a polyorganosiloxane-containing graft copolymer, and, compounded in 100 parts by mass of the resin component, (C) 0.1 to 5 parts by mass of a bisphenol type epoxy compound and (D) 0.05 to 2 parts by mass of polytetrafluoroethylene capable of forming fibrils, wherein the polyorganosiloxane-containing graft copolymer in the resin composition has a dispersion average particle diameter of 0.1 to 1.0 μm. The molded article has a section with a thickness of 1 mm or less and is obtainable by molding the aromatic polycarbonate resin composition.
    • 提供了具有优异的阻燃性,机械性能和流动性的芳族聚碳酸酯树脂组合物,并提供了薄壁成型制品。 芳香族聚碳酸酯树脂组合物包含含有(A)(A)90〜99.5质量%的芳香族聚碳酸酯树脂和(B)10〜0.5质量%的含聚有机硅氧烷的接枝共聚物的树脂成分,并且配合成100质量份 的树脂成分,(C)0.1〜5质量份双酚型环氧化合物和(D)0.05〜2质量份能够形成原纤维的聚四氟乙烯,其中,所述树脂组合物中的含聚有机硅氧烷的接枝共聚物具有 分散体平均粒径为0.1〜1.0μm。 模制品具有厚度为1mm以下的截面,可以通过模塑芳族聚碳酸酯树脂组合物而获得。
    • 5. 发明授权
    • Aromatic polycarbonate resin composition and molded object made from the same
    • 芳香族聚碳酸酯树脂组合物和由其制成的成型体
    • US07829617B2
    • 2010-11-09
    • US11817364
    • 2006-03-28
    • Akio NoderaYusuke Hayata
    • Akio NoderaYusuke Hayata
    • C08L69/00
    • C08L69/00C08L27/18C08L51/085C08L63/00Y10T428/269C08L2666/02
    • There is provided an aromatic polycarbonate resin composition having excellent flame retardancy, mechanical properties and fluidity and affording a thin-walled molded article.The aromatic polycarbonate resin composition includes a resin component containing (A) 90 to 99.5% by mass of an aromatic polycarbonate resin and (B) 10 to 0.5% by mass of a polyorganosiloxane-containing graft copolymer, and, compounded in 100 parts by mass of the resin component, (C) 0.1 to 5 parts by mass of a bisphenol type epoxy compound and (D) 0.05 to 2 parts by mass of polytetrafluoroethylene capable of forming fibrils, wherein the polyorganosiloxane-containing graft copolymer in the resin composition has a dispersion average particle diameter of 0.1 to 1.0 μm. The molded article has a section with a thickness of 1 mm or less and is obtainable by molding the aromatic polycarbonate resin composition.
    • 提供了具有优异的阻燃性,机械性能和流动性的芳族聚碳酸酯树脂组合物,并提供了薄壁成型制品。 芳香族聚碳酸酯树脂组合物包含含有(A)(A)90〜99.5质量%的芳香族聚碳酸酯树脂和(B)10〜0.5质量%的含聚有机硅氧烷的接枝共聚物的树脂成分,并且配合成100质量份 的树脂成分,(C)0.1〜5质量份双酚型环氧化合物和(D)0.05〜2质量份能够形成原纤维的聚四氟乙烯,其中,所述树脂组合物中的含聚有机硅氧烷的接枝共聚物具有 分散平均粒径为0.1〜1.0μm。 模制品具有厚度为1mm以下的截面,可以通过模塑芳族聚碳酸酯树脂组合物而获得。
    • 7. 发明授权
    • Thermoplastic resin composition and molded product
    • 热塑性树脂组合物和模塑制品
    • US08410214B2
    • 2013-04-02
    • US11814034
    • 2005-12-27
    • Yusuke HayataAkio Nodera
    • Yusuke HayataAkio Nodera
    • C08L69/00C08L67/04C08L51/04
    • C08L67/04C08L51/04C08L55/02C08L69/00C08L83/10C08L2666/02
    • The present invention provides a thermoplastic resin composition comprising 100 mass parts of a polycarbonate resin composition comprising 50 to 95 mass % of (A) a polycarbonate resin and 50 to 5 mass % of (B) a polylactic acid based resin and 5 to 65 mass parts of (C) a vinyl based graft copolymer. The above thermoplastic resin composition comprising the polycarbonate resin and the lactic acid based resin and endowed with a mechanical characteristic of polycarbonate and an excellent fluidity of polylactic acid in combination is improved in a hydrolysis resistance and provides a molded article further improved in an impact resistance and a thin-walled falling weight impact strength. A rise in the above characteristics makes it possible to use the plastic molded articles over a long period of time, and not only the thin-walled molding property and the portability are improved, but also the thermoplastic resin composition of the present invention can industrially advantageously be used as well for large-sized molded articles. In the thermoplastic resin composition of the present invention, use of the polycarbonate-polyorganosiloxane copolymer as the polycarbonate resin component makes it possible to improve as well the flame retardancy and advantageously use the thermoplastic resin composition of the present invention for office automation equipments, information and communication equipments, car parts, building components, home electric appliances and the like.
    • 本发明提供一种热塑性树脂组合物,其包含100质量份的聚碳酸酯树脂组合物,其包含50〜95质量%的(A)聚碳酸酯树脂和50〜5质量%的(B)聚乳酸类树脂,5〜65质量% 部分(C)乙烯基接枝共聚物。 包含聚碳酸酯树脂和乳酸基树脂并且具有聚碳酸酯的机械特性和聚乳酸的优异流动性的上述热塑性树脂组合物的耐水解性提高,并且提供了进一步提高耐冲击性的成型体, 薄壁落锤冲击强度。 上述特征的上升使得可以长时间使用塑料模塑制品,不仅提高了薄壁成型性和便携性,而且本发明的热塑性树脂组合物在工业上可以有利地 也可用于大型成型制品。 在本发明的热塑性树脂组合物中,通过使用聚碳酸酯 - 聚有机硅氧烷共聚物作为聚碳酸酯树脂成分,能够提高阻燃性,有利地将本发明的热塑性树脂组合物用于办公自动化设备,信息和 通信设备,汽车零件,建筑构件,家用电器等。