    • Impact-resistant thermoplastic resin composition containing a grafted
butadiene rubber
    • 含有接枝丁二烯橡胶的耐冲击热塑性树脂组合物
    • US5283286A
    • 1994-02-01
    • US879999
    • 1992-05-08
    • Yosuke TakahashiYasumasa KomatsuHiroshi HagiwaraTakayuki Katto
    • Yosuke TakahashiYasumasa KomatsuHiroshi HagiwaraTakayuki Katto
    • C08F279/02C08L21/00C08L25/16C08L33/04C08L33/12C08L33/18C08L33/20C08L51/00C08L51/04C08L35/06
    • C08L25/16C08L33/12C08L51/04
    • A thermoplastic resin composition is prepared by blending 50-95 wt. % of a copolymer (A) of 10-75 wt. % of .alpha.-methyl styrene, 10-60 wt. % of methyl methacrylate, 5-35 wt. % of acrylonitrile and 0-20 wt. % of a monomer copolymerizable therewith; and 5-50 wt. % of a graft copolymer (B) comprising 50-85 wt. parts of a butadiene-based rubber polymer and 15-50 wt. parts of a vinyl monomer graft-polymerized onto the rubber polymer. The butadiene-based rubber polymer includes 50-98 wt. % of butadiene, 2-50 wt. % of an aromatic polycyclic vinyl monomer represented by a formula (I) below and 0-20 wt. % of a monomer copolymerizable therewith: ##STR1## wherein R denotes an optionally substituted biphenylyl or naphthyl group, and R.sub.1 denotes a hydrogen atom or a methyl group. The thermoplastic resin composition is provided with a good balance among heat-resistance, impact resistance, transparency and processability because the graft copolymer (B) using an aromatic polycyclic vinyl monomer shows a good impact resistance-modifying effect while retaining a relatively high refractive index and the copolymer (A) shows a good heat resistance and a relatively low refractive index.
    • 热塑性树脂组合物通过混合50-95wt。 %的共聚物(A)为10-75wt。 %的(α) - 甲基苯乙烯,10-60wt。 %的甲基丙烯酸甲酯,5-35wt。 丙烯腈的百分比和0-20重量% 可与其共聚的单体的%。 和5-50wt。 %的接枝共聚物(B)包含50-85wt。 部分丁二烯类橡胶聚合物和15-50wt。 部分接枝聚合到橡胶聚合物上的乙烯基单体。 丁二烯类橡胶聚合物包含50-98wt。 丁二烯的%,2-50wt。 %的由下式(I)表示的芳族多环乙烯基单体和0-20重量% 可与其共聚的单体的%:(*化学结构*)(I)其中R表示任选取代的联苯基或萘基,R 1表示氢原子或甲基。 由于使用芳族多环乙烯基单体的接枝共聚物(B)在保持相对高的折射率的同时表现出良好的耐冲击性改性效果,所以热塑性树脂组合物在耐热性,耐冲击性,透明性和加工性方面具有良好的平衡, 共聚物(A)显示良好的耐热性和较低的折射率。
    • 2. 发明授权
    • Thermoplastic resin composition
    • 热塑性树脂组合物
    • US4701495A
    • 1987-10-20
    • US834122
    • 1986-02-26
    • Takayuki KattoYasumasa KomatsuZenya Shiiki
    • Takayuki KattoYasumasa KomatsuZenya Shiiki
    • C08L51/00C08L7/00C08L21/00C08L25/00C08L25/02C08L25/16C08L25/18C08L33/00C08L33/02C08L33/04C08L33/20C08L51/02C08L51/04C08L51/06C08L55/00C08L55/02
    • C08L25/16C08L25/02C08L55/02
    • A thermoplastic resin composition of high heat resistance and high impact resistance is described, comprising: (A) 50 to 90% by weight of a copolymer prepared by copolymerization of 10 to 35% by weight of acrylonitrile, 60 to 85% by weight of a monomer mixture of 2-isopropenylnaphthalene (2-IPN) and .alpha.-methylstyrene (.alpha.-MeSt), the proportion of 2-IPN being 5 to 70% by weight based on the total weight of 2-IPN and .alpha.-MeSt, and 0 to less than 10% by weight of a vinyl monomer copolymerizable with the foregoing monomers; and (B) 10 to 50% by weight of a graft copolymer prepared by polymerizing 15 to 50 parts by weight of at least one monomer selected from the group consisting of aromatic vinyl compounds, vinyl cyanides, methacrylic acid alkyl esters, and acrylic acid alkyl esters in the presence of 50 to 85 parts by weight of a butadiene- or alkyl acrylate-based rubber, the sum of the graft and rubber components being 100 parts by weight.
    • 描述了具有高耐热性和高耐冲击性的热塑性树脂组合物,其包含:(A)通过共聚合10至35重量%的丙烯腈,60至85重量%的丙烯腈制备的共聚物,50至90重量% 2-异丙烯基萘(2-IPN)和α-甲基苯乙烯(α-MeSt)的单体混合物,2-IPN的比例为5至70重量%,基于2-IPN和α-MeSt的总重量,0 至少于10重量%的可与上述单体共聚的乙烯基单体; 和(B)10至50重量%的通过聚合15至50重量份的至少一种选自芳族乙烯基化合物,乙烯基氰化物,甲基丙烯酸烷基酯和丙烯酸烷基酯的单体制备的接枝共聚物 在50至85重量份的基于丙烯酸丁酯或丙烯酸酯的橡胶存在下,所述接枝和橡胶组分的总和为100重量份。
    • 6. 发明授权
    • Thermoplastic resin composition
    • 热塑性树脂组合物
    • US4636553A
    • 1987-01-13
    • US618662
    • 1984-06-08
    • Takayuki KattoYasumasa KomatsuZenya Shiiki
    • Takayuki KattoYasumasa KomatsuZenya Shiiki
    • C08F12/00C08F212/32C08L7/00C08L21/00C08L25/00C08L25/02C08L25/16C08L33/00C08L33/02C08L51/00C08L51/02C08L51/04C08L69/00C08L51/06C08L55/02
    • C08L69/00C08L25/02C08L25/16C08L51/04
    • A thermoplastic resin composition of high heat resistance and high impact resistance is described, comprising: (A) 5 to 85% by weight of a copolymer prepared from 40 to 85% by weight of a monomer mixture of 2-isopropenylnaphthalene (2-IPN) and .alpha.-methylstyrene (.alpha.-MeSt), the proportion of 2-IPN being 5 to 70% by weight based on the total weight of 2-IPN and .alpha.-MeSt, 7.5 to 35% by weight of acrylonitrile, and 0 to 40% by weight of a vinyl monomer copolymerizable with the foregoing monomers; (B) 1 to 40% by weight of a graft copolymer prepared by graft polymerization of 15 to 50 parts by weight of at least one monomer as the graft component selected from the group consisting of methacrylic acid alkyl esters, acrylic acid alkyl esters, aromatic vinyl compounds, and vinyl cyan compounds onto 50 to 85 parts by weight of a butadiene-based rubber or alkyl acrylate-based rubber as the rubber component, provided that the sum of the graft and rubber components is 100 parts by weight; and (C) 10 to 90% by weight of a polycarbonate.
    • 描述了一种具有高耐热性和高耐冲击性的热塑性树脂组合物,其包含:(A)5-85重量%的由40至85重量%的2-异丙烯基萘(2-IPN)单体混合物制备的共聚物, 和α-甲基苯乙烯(α-MeSt),2-IPN的比例为5至70重量%,基于2-IPN和α-MeSt的总重量,7.5至35重量%的丙烯腈和0至40 可与上述单体共聚的乙烯基单体的重量% (B)1〜40重量%的接枝共聚物,其通过接枝聚合15〜50重量份的至少一种单体作为接枝成分,所述接枝成分选自甲基丙烯酸烷基酯,丙烯酸烷基酯,芳香族 乙烯基化合物和乙烯基青色化合物作为橡胶组分的50至85重量份的丁二烯基橡胶或丙烯酸烷基酯橡胶,条件是接枝橡胶组分的总和为100重量份; 和(C)10〜90重量%的聚碳酸酯。