    • Rubber-reinforcing polyester fiber and process for preparation thereof
    • 橡胶增强聚酯纤维及其制备方法
    • US5242645A
    • 1993-09-07
    • US721545
    • 1991-09-13
    • Tai SasamotoTakehiko MiyoshiTakuji Sato
    • Tai SasamotoTakehiko MiyoshiTakuji Sato
    • C08G63/86D01F6/62
    • D01F6/62C08G63/86D02G3/48D10B2331/04
    • A rubber-reinforcing polyester fiber composed of a polyester prepared by using 30 to 150 ppm as antimony of an antimony compound and 5 to 60 ppm as germanium of a germanium compound as the polymerization catalyst. The fiber is characterized in that the terminal carboxyl group content is not larger than 25 eq/ton, diethylene glycol content (DEG) is not larger than 1.3% by weight, the intrinsic viscosity (IV) is at least 0.85, the sum (S) of the intermediate elongation and the dry heat shrinkage is lower than 8%, the product between strength and elongation (T.sqroot.E) is at least (2S+5), and the terminal modulus (TM) is not higher than 40 g/d. The polyester fiber is used as a rubber reinforcement.
    • PCT No.PCT / JP90 / 01491 Sec。 371日期1991年9月13日 102(e)1991年9月13日PCT PCT 1990年11月15日PCT公布。 出版物WO91 / 07529 日期:1991年5月30日。一种橡胶增强聚酯纤维,其由通过使用30至150ppm作为锑化合物的锑制备的聚酯和5至60ppm作为锗化合物的锗作为聚合催化剂制备。 纤维的特征在于末端羧基含量不大于25当量/吨,二甘醇含量(DEG)不大于1.3重量%,特性粘度(IV)至少为0.85,总和(S )的中间伸长率和干热收缩率低于8%,强度和伸长率之间的乘积(T 2ROOT E)至少为(2S + 5),并且末端模量(TM)不高于40g / d。 聚酯纤维用作橡胶增强剂。