    • 1. 发明授权
    • Method of preparing wet process phosphoric acid
    • 湿法磷酸的制备方法
    • US07172742B2
    • 2007-02-06
    • US10362845
    • 2001-05-15
    • Yisheng FengJiutian FengXigang LiuYurui WangTianbao Lu
    • Yisheng FengJiutian FengXigang LiuYurui WangTianbao Lu
    • C01B25/222C01B25/231
    • C01F11/46C01B25/231
    • The present invention relates to a method of preparing wet process phosphoric acid, which comprises: dividing raw materials which contain phosphate rock slurry and sulfuric acid into two parts, and then feeding these two parts into two reactors separately. In the first reactor, feeding 70–90 wt. % of the total amount of the slurry and sulfuric acid, in which the ratio of phosphate rock slurry to sulfuric acid to recycled phosphoric acid is set to be 1:0.6˜0.8:1.0˜2.5. 10˜30% of the reaction solution directly flows into conversion cell, participating in the conversion reaction of dihydrate gypsum. Thus resulted phosphoric acid concentration is 33˜39 wt. %. The recovery efficiency of P2O5 is 99% or more. When putting coke powders in the conversion solution as filter aid, the filtration efficiency can be improved by 10˜30%, and in so produced hemihydrate gypsum, P2O5 is 0.05˜0.2%, water of hydration is 4˜8%. The product can be used for producing sulfuric acid and cement without baking dry.
    • 本发明涉及一种制备湿法磷酸的方法,包括:将含有磷酸盐岩浆和硫酸的原料分成两部分,然后分别将这两部分进料到两个反应器中。 在第一反应器中,加入70-90wt。 磷酸盐岩与硫酸与再生磷酸的比例为1:0.6〜0.8:1.0〜2.5的浆料和硫酸的总量的%。 10〜30%的反应溶液直接流入转化池,参与二水石膏的转化反应。 因此磷酸浓度为33〜39wt。 %。 P 5 <5的回收效率为99%以上。 当将焦炭粉末作为助滤剂放入转化溶液中时,过滤效率可以提高10〜30%,在这样制造的半水石膏中,P 2 O 5 O 5 0.05〜0.2%,水合水质为4〜8%。 该产品可用于生产硫酸和水泥,无需烘干。