    • 6. 发明授权
    • Method of manufacture for graphene fluoropolymer dispersion
    • 石墨烯氟聚合物分散体的制造方法
    • US09394421B2
    • 2016-07-19
    • US14044190
    • 2013-10-02
    • Xerox Corporation
    • Qi ZhangYu QiSandra J. GardnerNan-Xing Hu
    • B05D3/02C08K3/04C08K5/54C08J3/215
    • C08K3/04C08J3/215C08K5/5406C09D127/12C09D127/18C08L69/00C08K9/06C08K3/042C08L33/16
    • A method for forming a dispersion includes mixing graphene particles, a fluorosilane coupling agent and a first solvent to produce a first dispersion wherein the graphene particles are from about 0.1 to about 0.8 weight percent of the first dispersion. The method includes concentrating the first dispersion by removing the first solvent to produce a second dispersion wherein the graphene particles are from about 2.0 to about 10.0 weight percent of the concentrated dispersion. The concentrated dispersion is mixed with a fluoropolymer dispersion including a second solvent, a surfactant, and fluoropolymer particles wherein the fluoropolymer dispersion has a solids content of about 30 weight percent to about 50 weight percent to form a second dispersion. A polymer binder in a third solvent is mixed with the second dispersion to form the coating dispersion.
    • 形成分散体的方法包括混合石墨烯颗粒,氟硅烷偶联剂和第一溶剂以产生第一分散体,其中石墨烯颗粒为第一分散体的约0.1至约0.8重量%。 该方法包括通过除去第一溶剂来浓缩第一分散体以产生第二分散体,其中石墨烯颗粒为浓缩分散体的约2.0至约10.0重量%。 将浓缩的分散体与包含第二溶剂,表面活性剂和含氟聚合物颗粒的含氟聚合物分散体混合,其中氟聚合物分散体具有约30重量%至约50重量%的固体含量以形成第二分散体。 将第三溶剂中的聚合物粘合剂与第二分散体混合以形成涂料分散体。
    • 8. 发明申请
    • METHOD OF MANUFACTURE FOR GRAPHENE FLUOROPOLYMER DISPERSION
    • 石墨氟聚合物分散体的制备方法
    • US20150093511A1
    • 2015-04-02
    • US14044190
    • 2013-10-02
    • Xerox Corporation
    • Qi ZhangYu QiSandra J. GardnerNan-Xing Hu
    • C09D127/12C08K3/04C08K5/54
    • C08K3/04C08J3/215C08K5/5406C09D127/12C09D127/18C08L69/00C08K9/06C08K3/042C08L33/16
    • A method for forming a dispersion includes mixing graphene particles, a fluorosilane coupling agent and a first solvent to produce a first dispersion wherein the graphene particles are from about 0.1 to about 0.8 weight percent of the first dispersion. The method includes concentrating the first dispersion by removing the first solvent to produce a second dispersion wherein the graphene particles are from about 2.0 to about 10.0 weight percent of the concentrated dispersion. The concentrated dispersion is mixed with a fluoropolymer dispersion including a second solvent, a surfactant, and fluoropolymer particles wherein the fluoropolymer dispersion has a solids content of about 30 weight percent to about 50 weight percent to form a second dispersion. A polymer binder in a third solvent is mixed with the second dispersion to form the coating dispersion.
    • 形成分散体的方法包括混合石墨烯颗粒,氟硅烷偶联剂和第一溶剂以产生第一分散体,其中石墨烯颗粒为第一分散体的约0.1至约0.8重量%。 该方法包括通过除去第一溶剂来浓缩第一分散体以产生第二分散体,其中石墨烯颗粒为浓缩分散体的约2.0至约10.0重量%。 将浓缩的分散体与包含第二溶剂,表面活性剂和含氟聚合物颗粒的含氟聚合物分散体混合,其中氟聚合物分散体具有约30重量%至约50重量%的固体含量以形成第二分散体。 将第三溶剂中的聚合物粘合剂与第二分散体混合以形成涂料分散体。