    • 1. 发明申请
    • SEQUENTIAL CASTING METHOD FOR THE PRODUCTION OF A HIGH-PURITY CAST METAL BILLET
    • SEQUENZGIESSVERFAHREN用于生产铸造金属STRAND高纯度
    • WO2005053877A3
    • 2005-11-10
    • PCT/EP2004012711
    • 2004-11-10
    • VOEST ALPINE IND ANLAGENHOHENBICHLER GERALDECKERSTORFER GERALDBRUMMAYER MARKUS
    • HOHENBICHLER GERALDECKERSTORFER GERALDBRUMMAYER MARKUS
    • B22D11/103B22D11/118B22D11/18
    • B22D11/118B22D11/103B22D11/183
    • The invention relates to a sequential casting method for the production of a high-purity cast metal billet (13) from a metal melt, wherein the metal melt is supplied from a melt container (5) in a controlled manner to a distributor vessel (8) and is then supplied from said distributor vessel (8) in a controlled manner into a continuous casting ingot mold (4) without any interruption. According to the invention, in order to cast a qualitatively high-value metal billet even when the melt vessel is changed and to ensure that the restart phase is kept as short as possible, the flow rate into the distributor vessel is greater than the outflow rate from the distributor vessel during a period of time ranging from the resumption of the supply of the metal melt to the distributor vessel until a quasi-stationary operating bath level height is obtained in the distributor vessel (8), wherein during 70 % - 100 % of said time period, the inflow rate into the distributor vessel (8) is less than or equal to twice the outflow rate from the distributor vessel.
    • 本发明是一种Sequenzgiessverfahren用于从金属熔体中制造高纯度的铸造金属带材(13),所述金属熔体调节由熔融槽(5)控制供给到中间包容器(8)并从该分配容器(8)到一个连铸结晶器(4) 被排出,且其中继续进行所述熔融金属的供给到铸模(4)而不中断。 为了能够在熔化用容器改变,其中重启相位可以保持尽可能短期间模制在这个过程中的高品质的金属带材,所以建议在从恢复金属的供给的时间段熔入中间包容器中,直至一个准 -stationaryBetriebsbadspiegelhöhe在分配容器(8),流入速率进中间包容器比在此期间流入速度成分配容器(8)小于或等于从中间包容器中流出速率的两倍的70%至100%的流出速率从浇口盘容器,其中的和更大的 ,
    • 3. 发明申请
    • METHOD FOR THE CONTINUOUS CASTING OF A THIN STRIP AND DEVICE FOR CARRYING OUT SAID METHOD
    • 方法一细条和用于实施该方法连铸装置
    • WO9948635A9
    • 2002-03-28
    • PCT/EP9901249
    • 1999-02-26
    • VOEST ALPINE IND ANLAGENACCIAI SPECIALI TERNI SPAHOHENBICHLER GERALDECKERSTORFER GERALD
    • HOHENBICHLER GERALDECKERSTORFER GERALD
    • B22D11/06B22D11/16
    • B22D11/0622B22D11/0697
    • The invention relates to a method for the continuous casting of a thin strip (1) using the two-roll method. According to said method molten metal (7) is cast into a casting slit (3), which is formed by two casting rolls (2) and corresponds to the thickness of the strip (1) to be cast, resulting in the formation of a molten bath (6). The surfaces (11) of the casting rolls (2) located above the molten bath (6) are rinsed with an inert gas or an inert gas mixture in accordance with the state of the surfaces (11) of the casting rolls (2). To avoid local thermal deformations, the surfaces (11) of the casting rolls (2) are observed along their entire length so as to detect local variations in their state. When local variations in state are detected, the gas rinsing of the surfaces (11) of the casting rolls (2) is carried out such that it differs locally in accordance with local variations observed along the entire length of the casting rolls (2).
    • 在用于薄带(1)的双辊方法的熔融金属的连续铸造的方法(7)倒入两条铸造辊中的一个(2)在待铸造带材(1)的形成(3)在形成的熔融浴的铸造间隙的厚度(6)和 铸辊(2)熔融浴(6)用惰性气体或惰性气体混合物中的依赖于表面(11)的上述状态的表面(11)被清除铸辊(2)。 避免局部热变形,在铸辊(2)的表面(11)观察到的在其纵向范围相对于局部不同的条件和它是气体中的依赖于局部不同的状态的出现铸辊(2)的表面(11)的扫 铸辊的纵向延伸(2)局部地不同的状态进行局部不同。