    • 3. 发明授权
    • Process for the preparation of polycarbonate
    • 制备聚碳酸酯的方法
    • US5468836A
    • 1995-11-21
    • US119065
    • 1993-09-13
    • Yoshimichi OkanoTatsuya KannoTsutomu YamatoYasuhiro OshinoMichiyo TanigawaTakaaki KuwanaYutaka Fukuda
    • Yoshimichi OkanoTatsuya KannoTsutomu YamatoYasuhiro OshinoMichiyo TanigawaTakaaki KuwanaYutaka Fukuda
    • C08G64/14C08G64/30C08G64/00
    • C08G64/14C08G64/30C08G64/307
    • A polycarbonate which is not discolored and is substantially free from chlorine ions causative of discoloration, has a branching parameter G of 0.1 to 1.0 and, terminal hydroxyl groups of 20 mole % or below based on all the terminal groups of the polycarbonate, and/or, a chlorine ion concentration in the polycarbonate of 10 ppm or below, and/or, a total of an alkali metal ion concentration and an alkaline earth metal ion concentration in the polycarbonate of 1 ppm or below. A process for preparing the above polycarbonate by the melt transesterification process which comprises using a nitrogenous basic compound (a), and/or, a compound (b) containing an element selected from the group consisting of Groups IIb, IVb and Vb of the periodic table; or, a nitrogenous basic compound (a), and, a compound (c) containing an element selected from the group consisting of alkali metals and alkaline earth metals, as a transesterification catalyst.
    • PCT No.PCT / JP93 / 00104 Sec。 371日期1993年9月13日 102(e)1993年9月13日PCT 1993年1月28日PCT PCT。 公开号WO93 / 15129 日期为1993年8月5日。不变色并且基本上不含有由于变色引起的氯离子的聚碳酸酯,具有0.1至1.0的支化参数G和基于所有末端基团的20摩尔%或更低的末端羟基 的聚碳酸酯和/或聚碳酸酯中的氯离子浓度为10ppm以下,和/或聚碳酸酯中的碱金属离子浓度和碱土金属离子浓度的总和为1ppm以下。 一种通过熔融酯交换方法制备上述聚碳酸酯的方法,其包括使用含氮碱性化合物(a)和/或含有选自周期表中第IIb,IVb和Vb族的元素的化合物(b) 表; 或含氮碱性化合物(a)和含有选自碱金属和碱土金属的元素的化合物(c)作为酯交换催化剂。