    • 7. 发明专利
    • Molded ferrite sheet, sintered ferrite substrate and antenna module
    • 铸造铁素体板,烧结铁基板和天线模块
    • JP2008252089A
    • 2008-10-16
    • JP2008058602
    • 2008-03-07
    • Toda Kogyo Corp戸田工業株式会社
    • KIMURA TETSUYATSUCHIDE TOMOHIROYAMAMOTO KAZUMIDOI TAKANORI
    • H01F3/02H01F1/34H01Q7/06
    • PROBLEM TO BE SOLVED: To provide a clean and thin sintered ferrite substrate which is not firmly fixed to a mold even if it is not subjected to mold release treatment by zirconia powder, alumina powder or the like, and a sintered ferrite substrate which is free from contamination due to scattering of mold release powder or the like even if it is mounted on an electronic apparatus.
      SOLUTION: In a 30 to 430 μm thick molded ferrite sheet, at least one surface a center line average roughness is in a range of 170 nm to 800 nm, a maximum height is in a range of 3 μm to 10 μm, and an area occupancy rate of cross section cut in a horizontal direction at a depth of 50% of the maximum height in an area of a square with sides of 100 μm is in a range of 10 to 80%. The molded ferrite sheet is baked and a clean thin layer sintered ferrite substrate is obtained by performing laminate baking for the molded ferrite sheet which does not require mold release treatment.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:为了提供一种清洁和薄的烧结铁氧体衬底,即使没有经过氧化锆粉末,氧化铝粉末等的脱模处理,也没有牢固地固定在模具上,并且烧结的铁氧体衬底 其即使安装在电子设备上也不会由于脱模粉末等的散射而受到污染。 解决方案:在30至430μm厚的模制铁氧体片中,中心线平均粗糙度的至少一个表面在170nm至800nm的范围内,最大高度在3μm至10μm的范围内, 并且在100微米的边的正方形区域的最大高度的50%的深度处,在水平方向上切割的横截面的面积占有率在10至80%的范围内。 通过对不需要脱模处理的模制铁素体片进行层压烘烤,烘焙成型的铁素体片材,并获得干净的薄层烧结铁氧体衬底。 版权所有(C)2009,JPO&INPIT
    • 8. 发明专利
    • Magnetic antenna
    • 磁性天线
    • JP2007019891A
    • 2007-01-25
    • JP2005199451
    • 2005-07-07
    • Toda Kogyo Corp戸田工業株式会社
    • KIMURA TETSUYASATO YOSHIO
    • H01Q7/08
    • PROBLEM TO BE SOLVED: To obtain a magnetic antenna which operates stably even if attached to a metallic surface, and has high mass productivity.
      SOLUTION: The magnetic antenna can be obtained whose magnitude of a resonant frequency change is small even if attached to the metallic surface by forming, via an insulating layer, a structure formed with a conductive layer in a magnetic layer for forming a coil, and operative quality is stable and homogenous by not contacting directly with the metallic surface when attached thereto.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:为了获得即使附着在金属表面上也能稳定地工作并具有高质量生产率的磁性天线。 解决方案:即使通过绝缘层在形成线圈的磁性层中形成由导电层形成的结构,也可以获得谐振频率变化幅度小的附加金属表面的磁性天线 ,并且通过在附着时不与金属表面直接接触,操作质量稳定且均匀。 版权所有(C)2007,JPO&INPIT