    • 7. 发明授权
    • Sintering process for producing thin films of calcium phosphate entities
    • 用于生产磷酸钙实体薄膜的烧结工艺
    • US5766669A
    • 1998-06-16
    • US960702
    • 1997-10-30
    • Sydney M. PughTimothy J. N. Smith
    • Sydney M. PughTimothy J. N. Smith
    • A61L27/00A61F2/00A61L27/32C01B25/32C03C17/25C04B35/447C04B41/50B05D3/02B05D5/00
    • A61L27/32C03C17/25C04B41/5048A61F2310/00796C03C2217/23C03C2218/113C03C2218/32
    • An improved process for producing a thin film of calcium phosphate entities to support bone cell activity thereon. The material to be sintered is prepared by combining a solution of ammonium phosphate with a solution of calcium nitrate to form a sol-gel containing hydroxyapatite. A film of the sol gel is applied to at least one side of the substrate and the film coated on the substrate is sintered to form a solid film of calcium phosphate entities. The improvement in the process comprising sintering the film at temperatures selected from a range of temperatures which optimize a composition of calcium phosphate entities in the film. The sintering step converts hydroxyapatite to .alpha.-tricalcium phosphate where extent of such conversion is temperature dependent. The optimized composition comprises a ratio of hydroxyapatite to .alpha.-tricalcium phosphate in the range of 50:50 to 20:80. A sintering temperature is selected to provide these ratios. The sintering temperature is selected from a range of 920.degree. C. up to 1100.degree. C. where the higher the select temperature, the greater the amount of .alpha.-tricalcium phosphate in the ratio.
    • 一种用于生产磷酸钙实体薄膜以支持骨细胞活性的改进方法。 待烧结的材料通过将磷酸铵溶液与硝酸钙溶液组合以形成含羟基磷灰石的溶胶 - 凝胶来制备。 将溶胶凝胶膜施加到基材的至少一侧,并将涂覆在基材上的膜烧结以形成磷酸钙实体的固体膜。 该方法的改进包括在选自优化膜中磷酸钙实体的组成的温度范围内的温度下烧结膜。 烧结步骤将羟基磷灰石转化为α-磷酸三钙,其中这种转化的程度是温度依赖性的。 优化的组合物包含羟基磷灰石与α-磷酸三钙的比例为50:50至20:80。 选择烧结温度以提供这些比例。 烧结温度选择在920℃至1100℃的范围内,其中选择温度越高,α磷酸三钙的量越大。