    • 5. 发明申请
    • Cordierite Porous Ceramic Honeycomb Articles
    • 堇青石多孔陶瓷蜂窝制品
    • US20110293883A1
    • 2011-12-01
    • US12789833
    • 2010-05-28
    • Weiguo MiaoJianguo Wang
    • Weiguo MiaoJianguo Wang
    • C04B35/195B32B3/12
    • C04B38/0006B01D46/2425B01D46/2444B01D2046/2433B01D2046/2437B01D2046/2496B01J35/04C04B35/195C04B2111/00793C04B2111/0081F01N3/0222F01N2260/10Y10T428/24149C04B38/0074
    • Porous ceramic honeycomb articles for use as particulate filters and processes for making the same are described herein. The porous ceramic honeycomb articles include a fired cordierite body. The fired cordierite body has a microcrack parameter (Nb3) of about 0.05 to about 0.25 prior to exposure to a microcracking condition. After exposure to the microcracking condition, the fired cordierite body has a microcrack parameter (Nb3) at least 20% greater than the microcrack parameter prior to exposure to the microcracking condition. The fired cordierite body has a coefficient of thermal expansion (CTE) of about 7.0×10−7/° C. to about 15.0×10−7/° C. over from about 25° C. to about 800° C. prior to exposure to the microcracking condition and a coefficient of thermal expansion of about 1.0×10−7/° C. to about 10.0×10−7/° C. over from about 25° C. to about 800° C. after exposure to the microcracking condition. The microcrack parameter may include a thermal cycle or a chemical treatment.
    • 用作微粒过滤器的多孔陶瓷蜂窝体制品及其制造方法在此描述。 多孔陶瓷蜂窝体制品包括烧制的堇青石体。 烧制的堇青石体在暴露于微裂纹状态之前具有约0.05至约0.25的微裂纹参数(Nb 3)。 在暴露于微裂纹状态之后,烧结的堇青石体在暴露于微裂纹状态之前具有比微裂纹参数大至少20%的微裂纹参数(Nb 3)。 煅烧的堇青石体在约25℃至约800℃之前的热膨胀系数(CTE)为约7.0×10 -7 /℃至约15.0×10 -7 /℃, 暴露于微裂纹条件和热膨胀系数约为1.0×10-7 /℃至约10.0×10-7 /℃,超过约25℃至约800℃。 微裂纹状况。 微裂纹参数可以包括热循环或化学处理。