    • 7. 发明申请
    • GLASS COMPOSITION FOR SUBSTRATES AND PROCESS FOR ITS PRODUCTION
    • 基材玻璃组合物及其生产工艺
    • US20100137122A1
    • 2010-06-03
    • US12699944
    • 2010-02-04
    • Kensuke NagaiTetsuya NakashimaKei Maeda
    • Kensuke NagaiTetsuya NakashimaKei Maeda
    • C03C3/087C03B18/02
    • H01J5/04C03C3/087H01J2217/49264
    • A glass composition for substrates excellent in productivity is provided by lowering the high temperature viscosity while securing characteristics and quality required for FPD substrates, particularly for PDP substrates. A glass composition for substrates, which is characterized by comprising, as represented by mass% based on oxides, from 55 to 75% of SiO2, from 5 to 15% of Al2O3, from 4 to 18% of MgO, from 3 to 12% of CaO, from 4 to 18% of SrO, from 0 to 20% of BaO, from 6 to 20% of Na2O+K2O, from 0.5 to 6% of ZrO2 and from 18 to 25% of MgO+CaO+SrO+BaO, as a glass matrix composition, and containing from 0.001 to 0.6% of SO3, and which is further characterized in that when the viscosity is represented by q, the temperature satisfying logη=2 is at most 1,545° C. and the devitrification temperature is at most the temperature satisfying logη=4, the thermal expansion coefficient is from 75×10−7 to 90×10−7/° C., the specific gravity is at most 2.8, and the glass transition point is at least 600° C.
    • 通过在确保FPD基板,特别是对于PDP基板所需的特性和质量的同时降低高温粘度来提供生产率优异的基板用玻璃组合物。 一种基材用玻璃组合物,其特征在于,以质量%为基准,以氧化物计,55〜75%的SiO 2,5〜15%的Al 2 O 3,4〜18%的MgO,3〜12% 的CaO,4〜18%的SrO,0〜20%的BaO,6〜20%的Na 2 O + K 2 O,0.5〜6%的ZrO 2和18〜25%的MgO + CaO + SrO + BaO 作为玻璃基质组合物,含有0.001〜0.6%的SO 3,其特征还在于当粘度由q表示时,满足log&eggr = 2的温度为至多1,545℃,失透温度 至多满足log&eegr = 4,热膨胀系数为75×10-7〜90×10-7 /℃,比重为2.8以下,玻璃化转变点为600以上 C。
    • 8. 发明授权
    • Glass composition for substrates and process for its production
    • 用于基材的玻璃组合物及其生产方法
    • US08377834B2
    • 2013-02-19
    • US12699944
    • 2010-02-04
    • Kensuke NagaiTetsuya NakashimaKei Maeda
    • Kensuke NagaiTetsuya NakashimaKei Maeda
    • C03C3/087
    • H01J5/04C03C3/087H01J2217/49264
    • A glass composition for substrates excellent in productivity is provided by lowering the high temperature viscosity while securing characteristics and quality required for FPD substrates, particularly for PDP substrates. A glass composition for substrates, which is characterized by comprising, as represented by mass% based on oxides, from 55 to 75% of SiO2, from 5 to 15% of Al2O3, from 4 to 18% of MgO, from 3 to 12% of CaO, from 4 to 18% of SrO, from 0 to 20% of BaO, from 6 to 20% of Na2O+K2O, from 0.5 to 6% of ZrO2 and from 18 to 25% of MgO+CaO+SrO+BaO, as a glass matrix composition, and containing from 0.001 to 0.6% of SO3, and which is further characterized in that when the viscosity is represented by η, the temperature satisfying logη=2 is at most 1,545° C. and the devitrification temperature is at most the temperature satisfying logη=4, the thermal expansion coefficient is from 75×10−7 to 90×10−7/° C., the specific gravity is at most 2.8, and the glass transition point is at least 600° C.
    • 通过在确保FPD基板,特别是对于PDP基板所需的特性和质量的同时降低高温粘度来提供生产率优异的基板用玻璃组合物。 一种基材用玻璃组合物,其特征在于,以质量%为基准,以氧化物计,55〜75%的SiO 2,5〜15%的Al 2 O 3,4〜18%的MgO,3〜12% 的CaO,4〜18%的SrO,0〜20%的BaO,6〜20%的Na 2 O + K 2 O,0.5〜6%的ZrO 2和18〜25%的MgO + CaO + SrO + BaO ,作为玻璃基质组合物,含有0.001〜0.6%的SO 3,其特征还在于当粘度由&eegr表示时,满足log&eegr = 2的温度为至多1545℃,失透 温度至多满足log&eggr = 4,热膨胀系数为75×10-7〜90×10-7 /℃,比重为2.8以下,玻璃化转变点为至少 600℃