    • Naoki Kushida
    • C08L9/06
    • C08K5/372B60C1/0016C08K3/04C08K3/36C08K5/548C08L9/06Y02T10/862C08L2666/08
    • A rubber composition for a tire is blended with diene-based rubber containing 50 wt % or more of SBR, and 0.2 to 5 parts by weight of cyclic polysulfide represented by the below formula (I), 1 to 30 parts by weight of aromatic denatured terpene resin, 20 to 80 parts by weight of silica, and 40 to 100 parts by weight of carbon black relative to 100 parts by weight of the diene-based rubber. Further, a total blending amount of the silica and the carbon black is 70 to 130 parts by weight. In the formula, R represents a substituted or unsubstituted alkylene group having 2 to 18 carbon atoms, a substituted or unsubstituted oxyalkylene group having 2 to 18 carbon atoms, or an alkylene group including an aromatic ring, x represents an average number of 2 to 6, and n represents an integer of 1 to 15.
    • 将轮胎用橡胶组合物与含有50重量%以上的SBR的二烯系橡胶和0.2〜5重量份的由下式(I)表示的环状多硫化物,1〜30重量份的芳族化合物 萜烯树脂,20〜80重量份二氧化硅,40〜100重量份炭黑相对于二烯系橡胶为100重量份。 此外,二氧化硅和炭黑的总混合量为70〜130重量份。 式中,R表示取代或未取代的碳原子数2〜18的亚烷基,取代或未取代的碳原子数2〜18的氧化烯基或芳香族环的亚烷基,x表示平均2〜6个 ,n表示1〜15的整数。
    • 9. 发明授权
    • Method and apparatus for carrying out transference recording of an ink
image
    • 用于进行油墨图像的转印记录的方法和装置
    • US4882593A
    • 1989-11-21
    • US942810
    • 1986-12-22
    • Kouichi ToumaTetsuo HasegawaNaoki KushidaHisao YaegashiYasuyuki TamuraShuzo Kaneko
    • Kouichi ToumaTetsuo HasegawaNaoki KushidaHisao YaegashiYasuyuki TamuraShuzo Kaneko
    • B41M5/26
    • B41M5/26
    • Image recording is indirectly achieved on a recording sheet via an intermediate transferring medium. First, the circumferential surface of a rotatable transferring medium having heat-transferable ink contained therein is fused or softened in response to image information by means of a recording electrode which is disposed at the position opposite to the transferring medium while the intermediate transferring medium is interposed therebetween. After completion of the first transferring step the ink image which has been transferred onto the intermediate transferring medium is transported to the position where a second transferring step is achieved while the ink image is kept in the fused or softened state. The second transferring step is achieved in such a manner that the ink image is transferred onto the recording sheet under the effect of pressure which is imparted by a pressure roller. The intermediate transferring medium may be made of electric conductive material. Intermediate treatment such as removal of the ink image, partial correction of the same, addition of another ink image can be carried out between the first transferring step and second transferring step.
    • 通过中间转印介质在记录纸上间接实现图像记录。 首先,通过设置在与转印介质相对的位置处的记录电极,响应于图像信息,容纳在其中的具有可热转印墨水的可旋转转印介质的圆周表面被熔融或软化,同时中间转印介质被插入 之间。 在完成第一转印步骤之后,转印到中间转印介质上的油墨图像被输送到在油墨图像保持熔融或软化状态的同时实现第二转印步骤的位置。 第二转印步骤以这样一种方式实现:油墨图像在由压力辊赋予的压力的作用下转印到记录纸上。 中间转印介质可以由导电材料制成。 可以在第一转印步骤和第二转印步骤之间进行中间处理,例如去除油墨图像,部分校正,另外的油墨图像的添加。
    • 10. 发明授权
    • Rubber composition for use in tire treads
    • 用于轮胎胎面的橡胶组合物
    • US09309389B2
    • 2016-04-12
    • US14383898
    • 2012-03-08
    • Yoichi TakizawaNaoki Kushida
    • Yoichi TakizawaNaoki Kushida
    • C08L9/06C08K3/00C08K3/04B60C1/00
    • C08L9/06B60C1/0016C08K3/04C08K5/372C08K2201/006C08L81/04C08L91/00C08L93/00C08L2205/025C08K5/45
    • A rubber composition in which from 80 to 150 parts by weight of carbon black having a nitrogen adsorption specific surface area of from 200 to 400 m2/g is compounded per 100 parts by weight of styrene-butadiene rubber including from 60% to 100% by weight of solution-polymerized styrene-butadiene rubber S-SBR1 and from 40% to 0% by weight of solution-polymerized styrene-butadiene rubber S-SBR2 to result in a total of 100% by weight, the styrene quantity of the S-SBR1 being from 30% to 38% by weight, the vinyl quantity of the S-SBR1 being from 60% to 80% by weight, the glass transition temperature of the S-SBR1 being from −20° C. to −5° C., the weight-average molecular weight of the S-SBR1 being from 1,000,000 to 1,800,000, the glass transition temperature of the S-SBR2 being not less than −30° C. and less than −20° C., and the weight-average molecular weight of the S-SBR2 being from 1,000,000 to 1,800,000.
    • 一种橡胶组合物,其中80至150重量份的氮吸附比表面积为200-400m2 / g的炭黑,相对于100重量份的包含60%至100%的苯乙烯 - 丁二烯橡胶 溶液聚合的苯乙烯 - 丁二烯橡胶S-SBR1和40重量%至0重量%的溶液聚合的丁苯橡胶S-SBR2的重量,总共达到100重量%,S- SBR1为30〜38重量%,S-SBR1的乙烯基量为60〜80重量%,S-SBR1的玻璃化转变温度为-20℃〜-5℃ ,S-SBR1的重均分子量为1,000,000至1,800,000,S-SBR2的玻璃化转变温度不低于-30℃且小于-20℃, S-SBR2的平均分子量为1,000,000至1,800,000。