    • 5. 发明专利
    • PRODUCTION OF METALLIC MEMBER
    • JPS6396203A
    • 1988-04-27
    • JP24137986
    • 1986-10-13
    • TOSHIBA CORP
    • SEKIGUCHI SHIGEAKIOKUTOMI ISAO
    • C21D1/00B22F3/10B22F3/26C22F1/00
    • PURPOSE:To easily obtain a good metallic member with good workability by inserting a fibrous ceramic between a heat treatment jig and the metallic member at the time of housing the metallic member into the heat treatment jig and subjecting the member to a heat treatment. CONSTITUTION:A woven and knitted member consisting of fibrous ceramics is interposed between the heat treatment jig and the metallic member at the time of housing the metallic member into the heat treatment jig and subjecting the member to the heat treatment such as sintering or infiltration. The heat treatment jig has a boat- or plate shape and contains carbon. The metallic member is a member contg. at least one kind among Fe, Mo, W, V, Nb, Ta, Ti, Zr, Ni and Co and having carbide formability. The fibrous ceramics is preferably composed essentially of Al2O3 and/or SiO2. The reaction and wetting of the metallic member with the heat treatment jig at the time of the heat treatment are thereby prevented and the good metallic member is obtd.
    • 7. 发明专利
    • ELECTRODE MATERIAL FOR ELECTRIC DISCHARGE MACHINING AND ITS PRODUCTION
    • JPS62127449A
    • 1987-06-09
    • JP26389385
    • 1985-11-26
    • TOSHIBA CORP
    • SEKIGUCHI SHIGEAKIMATSUURA IKUO
    • B23H1/06C22C1/04C22C27/04
    • PURPOSE:To manufacture an electrode material for electric discharge machining excellent in workability and having superior consumption characteristics, by mixing powdered W and powdered Ca, by subjecting the resulting powder mixture to compacting and sintering, and by infiltrating Cu or Ag into the obtained sintered compact so as to form a specific composition. CONSTITUTION:The powdered W and the powdered Ca are mixed in a prescribed ratio, and the powder mixture is compacted and sintered with proper addition of a binder. It is preferable that the average grain size of above- mentioned powdered W is 2-10mum and that sintering is carried out at about 1,000-1,200 deg.C in a nonoxidizing atmosphere. Then Cu and/or Ag is infiltrated into a skeleton consisting of W and Ca obtained by the above-mentioned sintering at about 1,100-1,300 deg.C, so that electrode material for electric discharge machining having a composition consisting of 0.3-3.0wt% Ca, 20-40wt% of Cu and/or Ag, and the balance W can be obtained. The above electrode material is reduced in bores, excellent in workability such as grindability, polishability, etc., and further reduced in electrode consumption in the working of super hard materials, so that long-lived electrodes can be obtained.
    • 8. 发明专利
    • Production of contact point material
    • 生产接触点材料
    • JPS5935643A
    • 1984-02-27
    • JP14384482
    • 1982-08-19
    • Toshiba Corp
    • OKUTOMI ISAOSUZUKI HIDEOSEKIGUCHI SHIGEAKIMATSUURA IKUO
    • B22F1/00C22C1/04C22C1/05C22C1/10H01H11/04
    • PURPOSE: To produce a sintered type contact point material having a uniform contact point characteristic by mixing a part of the main componet material powder of roughly the same amt. as the amt. of auxiliary component material powder with the auxiliary powder then mixing the remaining main component material powder therewith.
      CONSTITUTION: A main component material is constituted of about 15W65% highly conductive components consisting of at least 1 kind of Cu and Ag, and the balance an arc resistant component of at least 1 kind among W, Mo, Cr, Ti, WC, MoC, Cr
      3 C
      2 , TiC. An auxiliary component material is constituted of a component for preventing melt sticking consisting at least 1 kind among Bi, Te, Sb, and a component for improving sintering property consisting of at least 1 kind among Ni, Fe, Co, B. The content of the auxiliary component material in the product, i.e., contact point material, is set at ≤3wt%, and part of the main component material of roughly the same amt. as the amt. of the auxiliary component material is first mixed with the auxiliary component material to prepare a primary powder mixture; further, the remaining main component material is mixed therewith. Such powder mixture is molded under about 1W10 tons/ cm
      2 pressure and is sintered at about 1,000W1,300°C in a non-oxidative atmosphere, whereby the contact point material is obtd.
      COPYRIGHT: (C)1984,JPO&Japio
    • 目的:通过混合大致相同的主要成分材料粉末的一部分,制造具有均匀接触点特性的烧结型接触点材料。 作为amt。 辅助成分材料粉末与辅助粉末混合,然后将剩余的主要成分材料粉末与其混合。 构成:主要成分材料由至少1种Cu和Ag组成的约15-65%的高导电性组分构成,余量为W,Mo,Cr,Ti,WC中至少1种的电弧组分 ,MoC,Cr3C2,TiC。 辅助成分材料由用于防止在Bi,Te,Sb中至少1种的熔融粘附的组分和用于改善由Ni,Fe,Co,B中的至少1种组成的烧结性的组分构成。 产品中的辅助成分材料即接触点材料设定为<= 3wt%,主要成分材料的一部分大致相同。 作为amt。 的辅助成分材料首先与辅助成分材料混合以制备初级粉末混合物; 此外,剩余的主要成分材料与其混合。 将这种粉末混合物在约1-10吨/ cm 2的压力下成型,并在非氧化性气氛中在约1,000-1300℃下烧结,由此可以接触接触材料。