    • 3. 发明专利
    • Device for repairing pipe joint of existing pipe
    • 用于维修现有管道管道接头的装置
    • JPS6118462A
    • 1986-01-27
    • JP13838384
    • 1984-07-03
    • Hakko Co LtdTokyo Gas Co Ltd
    • HAYASHI MITSUTOSHISAITOU ISAOIKE NOBUKATSUOOSAWA TOSHIHIKO
    • B05C7/08F16L55/16F16L55/18
    • F16L55/18
    • PURPOSE: To perform secure repair without consuming resin uselessly by applying a flexible covering body for enlarging a part of a dragging wire to large diameter to the external periphery of the dragging wire in a specified range in the front side of a pig.
      CONSTITUTION: Pigs 2, 3 inserted into an existing pipe 1 through an inserting pipe are drawn by the operation of the dragging wire 4. In this stage, resin C having low viscosity charged to the front side of the front pig 2 diffuses to the inside of the pipe 1 and into dusts incorporated in the space of a pipe joint 13 to improve the lubricity of the internal periphery of the pipe 1 and makes movement of resin D to be filled in the joint and the movement of a hind pig 3 easier. Furthermore, since a cylindrical body 14 is provided to the external periphery of the dragging wire 4 at the front side of the pig 3 in the stage for drawing the pigs 2, 3, the length in the inside of the pipe 1 occupied by the resin D is increased and the viscous resistance is increased and the resin pressure is also increased. Moreover, the time for filling the resin to the joint part is prolonged. Therefore, the filling time to the joint part is prolonged and the repair is performed securely with less consumption of resin.
      COPYRIGHT: (C)1986,JPO&Japio
    • 目的:通过在猪的正面的特定范围内施加用于将拖曳线的一部分的大直径放大到拖曳线的外围的柔性覆盖体,无需消耗树脂来进行安全的修复。 构成:通过插入管插入现有管1中的猪2,3被牵引线4的操作拉出。在此阶段,向前猪2的前侧充填的具有低粘度的树脂C扩散到内部 并且形成在管接头13的空间中的灰尘,以提高管1的内周的润滑性,并使待填充在接头中的树脂D的移动更容易。 此外,由于在用于抽取猪2,3的阶段中,在猪3的前侧的牵引线4的外周设置圆筒体14,所以管1的内部长度由树脂占据 D增加,粘性阻力增加,树脂压力也增加。 此外,延长了将树脂填充到接合部的时间。 因此,延长接合部的充填时间,并且以更少的树脂消耗可靠地进行修理。
    • 6. 发明专利
    • Butt welder
    • 焊接机
    • JPS59111811A
    • 1984-06-28
    • JP22150682
    • 1982-12-16
    • Osaka Gas Co LtdToho Gas KkTokyo Gas Co Ltd
    • MORIOKA MASAKAZUSAITOU ISAOMATSUZAKI MASAHITO
    • B29C65/00B29C53/00B29C65/18B29C65/20B29C65/34
    • B29C65/34B29C65/20B29C66/1142B29C66/5221B29C66/71B29C66/73921B29C66/91643B29C66/92445B29C66/92921B29C66/944B29K2023/06
    • PURPOSE:To easily perform butt welding with good efficiency all the time by providing a control circuit to operate all the processes smoothly at preset pressing forces and time. CONSTITUTION:The ends of paired thermoplastic resin tubes to be butt-welded are polished, a heater is inserted between both the tubes, and the end faces of both the tubes are pressingly contacted with the heating face of the heater through an operating lever. When the pressing force through a torque wrench reaches a given set pressure, the timer 87 of a controller 85 is started through a start switch 86. At the same time, a pressing and welding process display lamp 51 is lighted through a drive circuit 50, and at the same time solenoids 43 and 44 are demagnetized. Thereby, a moving bar is fixed by a brake plunger, and the pressing forces of both the tubes are held. Under the condition, the pressing and welding process is performed for a given period of time by the timer 87 and the following processes, a heating and holding process, a heater removal process, a welding process, and a cooling process, are continuously performed at set pressing force and time. Better butt welding can thus be performed with good efficiency by an easy operation all the time.
    • 目的:通过提供控制电路,以预设的按压力和时间顺利地运行所有过程,以便以高效率轻松执行对接焊接。 构成:对接成对的热塑性树脂管的端部进行抛光,在两管之间插入加热器,两个管的端面通过操作杆与加热器的加热面紧密接触。 当通过扭矩扳手的按压力达到给定的设定压力时,控制器85的定时器87通过启动开关86启动。同时,按压焊接处理显示灯51通过驱动电路50点亮, 并且同时螺线管43和44被去磁。 因此,通过制动柱塞固定移动杆,并且保持两个管的按压力。 在这种条件下,通过定时器87进行按压和焊接过程一段给定的时间,并且以下过程,加热保持过程,加热器去除过程,焊接过程和冷却过程在 设定按压力和时间。 因此,可以通过简单的操作始终以更好的效率进行更好的对接焊接。