    • 8. 发明公开
    • ACRYLIC RESIN COMPOSITION
    • ACRYLHARZZUSAMMENSETZUNG
    • EP1535963A1
    • 2005-06-01
    • EP03791319.1
    • 2003-08-27
    • KANEKA CORPORATIONKaneka Texas Corporation
    • SUGAYA, TakahikoNISHIMURA, RiichiTAJIMA, Kazuhisa
    • C08L33/12C08L51/06E06B1/26
    • B32B27/30C08L33/08C08L2205/02Y10T428/31855C08L2666/06
    • An acrylic resin composition with excellent impact resistance, weatherability, processability and low gloss is provided. The acrylic resin composition comprises, (A) 10 to 40 parts by weight of a high molecular weight acrylic (co)polymer which is a one-step or multi-step polymer containing 72 to 100 % by weight of methyl methacrylate and 0 to 28 % by weight of a copolymerizable monomer, the (co)polymer having a specific viscosity of at least 0.5 (solvent: toluene, concentration: 0.4 %, temperature: 30°C), wherein a polymer layer obtained in one of the steps contains at least 72 % by weight of methyl methacrylate, has a specific viscosity of at least 0.5 and makes up at least 55 % by weight of the total weight of the high molecular weight acrylic (co)polymer (A); (B) 0 to 80 parts by weight of an acrylic (co)polymer containing 50 to 100 % by weight of methyl methacrylate and 0 to 50 % by weight of a copolymerizable monomer, the acrylic (co)polymer having a specific viscosity of less than 0.5; (C) 10 to 90 parts by weight of an impact modifier with a multilayer structure, wherein the total of (A), (B) and (C) is 100 parts by weight and the composition has a melt flow index of 0.35 g/10 minutes to 1.4 g/ 10 minutes (230°C, 3.8 kg load).
    • 提供了具有优异的耐冲击性,耐候性,加工性和低光泽性的丙烯酸树脂组合物。 丙烯酸树脂组合物包含:(A)10至40重量份的高分子量丙烯酸(共)聚合物,其是含有72至100重量%的甲基丙烯酸甲酯和0至28的一步或多步聚合物 重量%的可共聚单体,比浓度至少为0.5的(共)聚合物(溶剂:甲苯,浓度:0.4%,温度:30℃),其中在其中一个步骤中获得的聚合物层含有 至少72重量%的甲基丙烯酸甲酯,比粘度至少为0.5,占高分子量丙烯酸(共)聚合物(A)总重量的至少55重量%。 (B)0至80重量份的含有50至100重量%的甲基丙烯酸甲酯和0至50重量%的可共聚单体的丙烯酸(共)聚合物,所述丙烯酸(共)聚合物的比粘度较低 比0.5; (C)10〜90重量份具有多层结构的抗冲改性剂,其中(A),(B)和(C)的总和为100重量份,组合物的熔体流动指数为0.35g / 10分钟至1.4g / 10分钟(230℃,3.8kg负荷)。
    • 10. 发明公开
    • VINYL CHLORIDE RESIN COMPOSITION
    • 乙烯基氯化物树脂组合物
    • EP0892015A1
    • 1999-01-20
    • EP97908565.1
    • 1997-03-31
    • KANEKA CORPORATION
    • TAKAKI, AkiraYAUCHI, ShinichiYUI, KojiNISHIMURA, RiichiTAKESADA, Kentaro
    • C08L27/06C08L51/04C08L51/06
    • C08L27/06C08L51/003C08L51/04C08L51/06C08L2666/24C08L2666/02
    • A vinyl chloride resin composition containing a graft copolymer A having an average particle diameter of at least 0.15 µm , prepared by polymerizing 50 to 90 % of a solid matter of a rubber latex having a glass transition temperature of at most 0°C, the rubber latex being prepared by polymerizing 50 to 100 % of butadiene and/or alkyl acrylate, 0 to 40 % of an aromatic vinyl monomer, 0 to 10 % of a vinyl monomer and 0 to 5 % of a polyfunctional monomer, with 10 to 50 % of a mixture comprising 10 to 100 % of an alkyl methacrylate, 0 to 90 % of an aromatic vinyl monomer, 0 to 25 % of a vinyl cyamide monomer and 0 to 20 % of a vinyl monomer; a graft copolymer B having an average particle diameter of 0.05 to 0.13 µm, prepared by polymerizing 50 to 90 % of the solid matter of the rubber latex with 10 to 50 % of the mixture; and a vinyl chloride resin C; wherein the weight ratio of (copolymer A)/(copolymer B) is 50/50 to 90/5, and the weight ratio of (the total amount of copolymer A and copolymer B)/(vinyl chloride resin composition C) is 1/99 to 30/70; the composition being excellent in impact resistance and usable for the production of a pipe, a window frame and the like.
    • 一种氯乙烯树脂组合物,其含有平均粒径为0.15μm以上的接枝共聚物A,该接枝共聚物A是通过使玻璃化转变温度为0℃以下的橡胶胶乳的固体成分50〜90%聚合而得到的橡胶 胶乳是通过聚合50至100%的丁二烯和/或丙烯酸烷基酯,0至40%的芳族乙烯基单体,0至10%的乙烯基单体和0至5%的多官能单体制备的,具有10至50% 的包含10-100%甲基丙烯酸烷基酯,0-90%芳族乙烯基单体,0-25%乙烯基氰胺单体和0-20%乙烯基单体的混合物; 平均粒径为0.05〜0.13μm的接枝共聚物B,其通过将橡胶胶乳的固体成分的50〜90%与10〜50%的混合物聚合而得到; 和氯乙烯树脂C; (共聚物A)/(共聚物B)的重量比为50/50至90/5,并且(共聚物A和共聚物B的总量)/(氯乙烯树脂组合物C)的重量比为1 / 99至30/70; 该组合物耐冲击性优异并可用于制造管道,窗框等。