    • 2. 发明申请
    • Alpha + beta or beta TITANIUM ALLOY AND METHOD FOR PRODUCTION THEREOF
    • α+β或β钛合金及其生产方法
    • US20140044584A1
    • 2014-02-13
    • US14113823
    • 2012-04-27
    • Osamu KanouSatoshi SugawaraHideo Takatori
    • Osamu KanouSatoshi SugawaraHideo Takatori
    • C22C1/04C22C14/00
    • C22C1/0458B22F3/14B22F3/20B22F9/023C22C14/00
    • A titanium alloy containing copper, which cannot be realized by a conventional method, is provided, having a composition in which copper is contained in titanium with no segregation, and having improved strength and hardness. In addition a method is also provided, in which the titanium alloy is produced at lower cost than in a conventional method. The α+β or β titanium alloy contains copper at 1 to 10 mass %, has a crystal phase of β and α phase or of β phase, is formed of crystal particles not more than 100 μm, and has a copper concentration per an arbitrary specified 1 mm3 portion of the crystal phase at within ±40% compared to another arbitrary specified portion. The α+β or β titanium alloy is produced by mixing 1 to 10 mass % of copper powder and the remainder of titanium alloy powder and then pressing and forming while being heated. The method for production of the α+β or β titanium alloy has a step of mixing 1 to 10 mass % of copper powder and the remainder of titanium alloy powder and a step of pressing and forming the mixture while being heated.
    • 提供了含有铜的钛合金,其通过常规方法不能实现,其具有在钛中含有铜而没有偏析并且具有改善的强度和硬度的组成。 此外,还提供了一种方法,其中以比常规方法更低的成本生产钛合金。 α+β或β钛合金含有1〜10质量%的铜,具有β相和α相或β相的结晶相,由不超过100μm的晶体粒子形成,并且具有任意的铜浓度 相对于另一个任意的指定部分,指定晶体相的1mm 3部分在±40%以内。 通过混合1〜10质量%的铜粉末和剩余的钛合金粉末,然后在加热的状态下进行加压成型,生成α+β或β钛合金。 制造α+β或β钛合金的方法具有将1〜10质量%的铜粉和剩余的钛合金粉末混合的步骤,以及在加热时压制和形成混合物的步骤。