    • 10. 发明申请
    • Method for Producing a Hardened Profile Part
    • 生产硬化型材零件的方法
    • US20070271978A1
    • 2007-11-29
    • US10566069
    • 2004-06-09
    • Werner BrandstatterHerbert EibensteinerMartin FleischanderlJosef FaderlGerald LandlAnna RaabSiegfried Kolnberger
    • Werner BrandstatterHerbert EibensteinerMartin FleischanderlJosef FaderlGerald LandlAnna RaabSiegfried Kolnberger
    • C23C2/02C21D1/02
    • C21D1/673C21D9/46C21D2221/00C21D2251/02C25D5/36C25D5/48Y10T29/49982Y10T29/49995Y10T428/12799Y10T428/31678
    • The invention relates to a method for producing a hardened profiled structural part from a hardenable steel alloy with cathodic corrosion protection, wherein: a) a coating is applied to a sheet made of a hardenable steel alloy, wherein b) the coating substantially consists of zinc, and c) in addition the coating contains one or several elements with affinity to oxygen in a total amount of 0.1 weight-% to 15 weight-% in relation to the total coating, and d) subsequently the coated sheet steel is roller-profiled in a profiling device, so that the sheet tape is formed into a roller-formed profiled strand, and e) thereafter the coated sheet steel is brought, at least in parts and with the admission of atmospheric oxygen, to a temperature required for hardening and is heated to a structural change required for hardening, wherein f) a skin made of an oxide of the element(s) with affinity to oxygen is formed on the surface of the coating, and g) after sufficient heating the sheet is cooled, wherein the rate of cooling is set in such a way that hardening of the sheet alloy is achieved, as well as to a corrosion-protection layer of the method and a profiled structural element made thereof.
    • 本发明涉及一种由具有阴极腐蚀保护性的可硬化钢合金制造硬化型材结构件的方法,其中:a)将涂层施加到由可硬化钢合金制成的片材上,其中b)涂层基本上由锌 ,以及c)此外,涂层含有相对于总涂层为0.1重量%至15重量%的总量为0.1摩尔%的亲氧性的一种或多种元素,以及d)随后将涂覆的钢板进行辊压成型 在成型装置中,使得片材带形成为辊状成形的股线,以及e)此后,至少部分地并且承受大气中的氧气使得涂覆的钢板达到硬化所需的温度, 被加热到硬化所需的结构变化,其中f)在涂层的表面上形成具有对氧的亲和性的元素的氧化物制成的皮肤,并且g)在充分加热之后,将片冷却,w 这里的冷却速度设定为使得实现了片状合金的硬化,以及该方法的腐蚀保护层和由其制成的异型结构元件。