    • A process of preparing bisphenol A having low residual contents of oxygen and phenol is described. The process involves: (a) melting mixed crystals of bisphenol A and phenol under a nitrogen atmosphere at a temperature of 100° C. to 120° C.; (b) feeding continuously the melt formed in step (a) into the top of a distillation unit under conditions of 120° C. to 80 mbar to 200 mbar; (c) feeding contemporaneously with step (b) nitrogen into the bottom of the distillation unit; (d) allowing the melted feed material and the nitrogen feed to contact each other within the distillation unit, thereby forming a concentrated melt material having (i) a phenol content reduced to 10 to 25 wt. %, and (ii) a reduced oxygen content (e.g., an oxygen content of
    • 描述了制备具有低残留氧含量和苯酚的双酚A的方法。 该方法包括:(a)在氮气气氛下,在100℃至120℃的温度下,将双酚A和苯酚的混合物熔融。 (b)在120℃至<160℃和压力> 80毫巴至200毫巴的条件下,将步骤(a)中形成的熔体连续进料到蒸馏单元的顶部; (c)与步骤(b)同时进料氮气到蒸馏单元的底部; (d)允许熔融的进料和氮气进料在蒸馏单元内彼此接触,从而形成浓缩的熔融材料,其具有(i)苯酚含量降低至10至25wt。 %,和(ii)氧含量降低(例如,氧含量<1ppm); 和(e)在至少大气压,180℃至220℃和氮分压为1至1.5巴的条件下,任选地使氮气流通过浓缩熔融材料,从而从浓缩的 熔融材料(例如,导致苯酚含量<50ppm)。 具有减少的氧和苯酚含量的熔融材料可以进一步加工成例如粒料。