    • 1. 发明专利
    • Composition for forming semi-rigid polyurethane foam
    • 用于形成半刚性聚氨酯泡沫的组合物
    • JP2011021073A
    • 2011-02-03
    • JP2009165534
    • 2009-07-14
    • Sanyo Chem Ind LtdToyota Motor Corpトヨタ自動車株式会社三洋化成工業株式会社
    • WATANABE TOSHIOURAYAMA YUJITOKUHARA WATARUISHIDA TAKAHIRO
    • C08L71/02C08G18/48C08L51/08
    • PROBLEM TO BE SOLVED: To provide a means for producing a semi-rigid polyurethane foam suitable for producing interior materials for an automotive vehicle maintaining high performance on the strength even under high-temperature and high-humidity conditions. SOLUTION: The composition for forming a semi-rigid polyurethane foam includes: a polyol composition (A) for producing a semi-rigid polyurethane foam containing polyether polyol (a1) comprising polytrimethylene ether glycol which is a polymer of 1,3-propanediol; a foaming agent (D) containing water; a catalyst (E); and a polyisocyanate (C). The method for producing the semi-rigid polyurethane foam includes a step of foaming and curing the composition for forming a semi-rigid polyurethane foam. COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:提供一种用于生产半刚性聚氨酯泡沫的方法,该半硬质聚氨酯泡沫适用于生产用于车辆的内部材料,即使在高温和高湿度条件下也能保持强度高的性能。 解决方案:用于形成半硬质聚氨酯泡沫的组合物包括:用于制备包含聚三亚甲基醚二醇的聚碳酸酯多元醇(a1)的半硬质聚氨酯泡沫的多元醇组合物(A) 丙二醇; 含有水的发泡剂(D) 催化剂(E); 和多异氰酸酯(C)。 半硬质聚氨酯泡沫的制造方法包括使用于形成半硬质聚氨酯泡沫的组合物发泡和固化的步骤。 版权所有(C)2011,JPO&INPIT
    • 5. 发明专利
    • Propylene resin composition and injection-molded product thereof
    • 丙烯树脂组合物和注射成型产品
    • JP2013224423A
    • 2013-10-31
    • JP2013059652
    • 2013-03-22
    • Sumitomo Chemical Co Ltd住友化学株式会社Toyota Motor Corpトヨタ自動車株式会社
    • NAKAJIMA HIROYOSHIWATANABE TOSHIONAKAGAWA SHUJI
    • C08L23/12C08K3/00C08K5/20C08L23/08C08L23/16
    • C08L23/12C08L23/0815C08L23/16C08L2308/00
    • PROBLEM TO BE SOLVED: To provide a propylene resin composition capable of producing a molding excellent in scratch resistance, low in glossiness, and hardly causing flow marks on the injection-molded body; and an injection-molded product thereof.SOLUTION: A propylene resin composition includes a specific propylene resin (A), a specific copolymer (B) of ethylene and ≥4C α-olefin, an inorganic filler (C), a fatty acid amide (D) and carbon black (E). Assuming that the total weight of (A) to (C) is 100 wt.%, the content of the specific propylene resin (A) is 52-72 wt.%, the content of the specific copolymer (B) of ethylene and ≥4C α-olefin is 10-20 wt.%, and the content of the inorganic filler (C) is 18-28 wt.%; and 0.2-0.7 pt.wt. of the fatty acid amide (D) and 0.8-2.2 pts.wt. of the carbon black (E) are contained to 100 pts.wt. of total weight of (A) to (C). An injection-molded product thereof is also disclosed.
    • 要解决的问题:提供一种丙烯树脂组合物,该丙烯树脂组合物能够产生耐刮擦性,低光泽度和在注射成型体上几乎不引起流痕的成型性; 丙烯树脂组合物包括特定丙烯树脂(A),乙烯和≥4Cα-烯烃的特定共聚物(B),无机填料(C),脂肪酸酰胺( D)和炭黑(E)。 假设(A)〜(C)的总重量为100重量%,特定丙烯类树脂(A)的含量为52〜72重量%,乙烯的特定共聚物(B)的含量≥ 4C的α-烯烃为10〜20重量%,无机填充剂(C)的含量为18〜28重量%。 和0.2-0.7重量份 的脂肪酸酰胺(D)和0.8-2.2重量份 的碳黑(E)含量为100重量份 (A)至(C)的总重量。 还公开了其注射成型产品。
    • 7. 发明专利
    • Polypropylene-based resin composition for exterior member of automobile and exterior member of automobile
    • 汽车外部成员和汽车外部成员的基于聚丙烯的树脂组合物
    • JP2013159709A
    • 2013-08-19
    • JP2012022785
    • 2012-02-06
    • Japan Polypropylene Corp日本ポリプロ株式会社Toyota Motor Corpトヨタ自動車株式会社
    • ADACHI MINORUKITAURA KAITOTAKAHASHI AKIHIRONAGAI TAKAYUKIWATANABE TOSHIO
    • C08L23/10B60J5/10B60R13/02B60R13/04B60R19/04B62D25/16C08K3/34C08L23/08C08L53/00
    • PROBLEM TO BE SOLVED: To provide a polypropylene-based resin composition for an exterior member of automobiles excellent in moldability (high flowability), dimensional stability (low thermal expansion coefficient), physical property balance (high rigidity, high impact resistance), and providing molding excellent in quality of appearance, and to provide the exterior member of automobiles.SOLUTION: There are provided a polypropylene-based resin composition for an exterior member of automobiles characterized by comprising following components (1)-(3) in such ratios that component (1) is 35-50 wt.%, component (2) is 15-25 wt.%, component (3) is 35-40 wt.%, based on the total amount of the components (1)-(3), and exterior members of automobiles. Wherein the component (1) is a polypropylene based resin polymerized by using a Ziegler catalyst and having a 100-110 g/10 min of a melt flow rate and 160-165°C of melting peak temperature, the component (2) is an ethylene-α-olefin copolymer having a 2-30 g/10 min of a melt flow rate, and the component (3) is talc having 15-17 of aspect ratio and 6-8 μm of an average particle size.
    • 要解决的问题:提供一种成型性(高流动性),尺寸稳定性(低热膨胀系数),物理性能平衡(高刚性,高耐冲击性),提供优异的成型性的汽车用外用构件的聚丙烯系树脂组合物 成型性优异,并且提供汽车外部构件。解决方案:提供一种用于汽车外部构件的聚丙烯基树脂组合物,其特征在于包括以下组分(1) - (3),其组分 (1)为35-50重量%,组分(2)为15-25重量%,组分(3)为35-40重量%,基于组分(1) - (3)的总量, ,以及汽车的外部成员。 其中组分(1)是通过使用齐格勒催化剂聚合并具有100-110g / 10min的熔体流动速率和160-165℃的熔融峰温度的聚丙烯基树脂,组分(2)是 乙烯-α-烯烃共聚物具有2-30g / 10min的熔体流动速率,组分(3)是具有15-17的纵横比和6-8μm的平均粒度的滑石。
    • 10. 发明专利
    • Repairing method of window member
    • WINDOW会员的修复方法
    • JP2008132446A
    • 2008-06-12
    • JP2006321210
    • 2006-11-29
    • Toyota Motor Corpトヨタ自動車株式会社
    • WATANABE TOSHIOTANAKA TORU
    • B05D3/06B05D5/06B32B27/18B32B27/36B60J1/00B60J7/02B60S5/00
    • PROBLEM TO BE SOLVED: To provide a repairing method of a window member which can be applied to a window member equipped with a hard coat layer on a resin base-material layer, and also in the case where it is applied, does not give a bad influence to the property of the base material and the adhesion property between the base material layer and the hard coat layer.
      SOLUTION: The repairing method of the window member has the first process of processing a defect 3 generated on the hard coat layer 1 until it reaches the base material layer 2, the second process of packing a defect repairing agent 4, mainly composed of a thermoplastic resin, into the defect 3a after processing, the third process of arranging a shape retention sheet 5 permeating the infrared ray on the hard coat layer 1, and the fourth process of irradiating the infrared-ray laser 7 at the part containing the defect 3a after processing from above the shape retention sheet 5.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:为了提供可以应用于在树脂基材层上配置有硬涂层的窗构件的窗构件的修理方法,并且在施加的情况下, 不会对基材的性质和基材层与硬涂层之间的粘合性产生不良影响。 解决方案:窗构件的修复方法具有处理在硬涂层1上产生的缺陷3直到其到达基材层2的第一处理,第二次包装缺陷修复剂4的过程,主要组成 的热塑性树脂,在加工后的缺陷3a中,将形成保持片5布置在硬涂层1上的红外线的第三工序,以及在包含红外线的部分照射红外线激光器7的第四工序 缺陷3a在形状保持片5的上方加工后。版权所有(C)2008,JPO&INPIT