热词
    • 5. 发明申请
    • PROCESS FOR MANUFACTURING FLUOROPOLYMER COMPOSITES
    • 制备氟聚合物复合材料的方法
    • WO2014195225A1
    • 2014-12-11
    • PCT/EP2014/061204
    • 2014-05-29
    • SOLVAY SPECIALTY POLYMERS ITALY S.P.A.
    • IEVA, ElianaLIU, RuiSARTIRANA, Elisabetta
    • C08J5/04B29B15/12C08L27/16
    • C03C25/305B29B15/125C03C2217/78C03C2218/111C03C2218/32C08J5/043C08J2327/16
    • The present invention pertains to a process for manufacturing a fluoropolymer composite, said process comprising the following sequential steps: (i) providing an aqueous latex comprising from 10% to 40% by weight, preferably from 15% to 35% by weight of at least one fluoropolymer comprising recurring units derived from vinylidene fluoride (VDF) [polymer (VDF)]; (ii) up-concentrating the aqueous latex provided in step (i) thereby providing an up-concentrated aqueous latex comprising from 45% to 60% by weight, preferably from 45% to 55% by weight of at least one polymer (VDF); (iii) contacting one continuous fibre or a bunch of continuous fibres with the up-concentrated aqueous latex provided in step (ii); (iv) squeezing the impregnated fibrous material provided in step (iii); (v) drying the squeezed fibrous material provided in step (iv), typically at a temperature comprised between 100°C and 120°C; (vi) baking the dried fibrous material provided in step (v) at a temperature comprised between 190°C and 240°C; (vii) cooling the coated fibrous material provided in step (vi), preferably to a temperature of about 20°C; (viii) optionally, contacting the coated fibrous material provided in step (vii) with the up-concentrated aqueous latex provided in step (ii) and submitting the impregnated fibrous material so provided to sequential steps (iv) to (vii); and (ix) optionally, repeating step (viii) one or more times. The present invention also pertains to the fluoropolymer composite thereby provided and to uses of said fluoropolymer composite in various applications.
    • 本发明涉及一种制备含氟聚合物复合材料的方法,所述方法包括以下顺序步骤:(i)提供包含10重量%至40重量%,优选15重量%至35重量%的至少 一种含氟聚合物,其包含衍生自偏氟乙烯(VDF)[聚合物(VDF)]的重复单元; (ii)向上浓缩步骤(i)中提供的水性胶乳,从而提供含有45重量%至60重量%,优选45重量%至55重量%的至少一种聚合物(VDF)的上层浓缩水性胶乳, ; (iii)使一个连续纤维或一束连续纤维与步骤(ii)中提供的上升浓缩水性胶乳接触; (iv)挤压步骤(iii)中提供的浸渍的纤维材料; (v)干燥步骤(iv)中提供的挤压纤维材料,通常在100℃和120℃之间的温度下; (vi)在190℃和240℃之间的温度下烘烤步骤(v)中提供的干燥的纤维材料; (vii)将步骤(vi)中提供的涂覆的纤维材料冷却至约20℃的温度; (viii)任选地,将步骤(vii)中提供的涂覆的纤维材料与步骤(ii)中提供的上层浓缩水性胶乳接触,并将浸渍的纤维材料提供给顺序步骤(iv)至(vii); 和(ix)任选地,重复步骤(viii)一次或多次。 本发明还涉及由此提供的含氟聚合物复合物以及所述含氟聚合物复合材料在各种应用中的用途。