    • 9. 发明专利
    • ES2218450T3
    • 2004-11-16
    • ES01969784
    • 2001-09-27
    • SMS DEMAG AG
    • GOTZINGER KARL REINERLEMKE STEFANREICHEL JOHANNROLLINGER BERNT
    • C21C7/00C21C5/00C21C5/52C21C7/068F27B3/04F27B3/22
    • The invention relates to a method for producing stainless steels, in particular steels containing chromium and chromium-nickel. The method is carried out in a melting device containing a metallurgical vessel, or in a melting device ( 1 ) containing at least two vessels ( 2, 3 ) for supplying a steel-casting installation, an electric arc furnace process ( 1 ) and an air-refining process taking place alternately in the two vessels ( 2, 3 ). To improve the efficiency of a method of this type, the aim of the invention is to carry out a reversible treatment of unreduced converter slag in the electric-arc furnace mode. To achieve this, in the first treatment stage, the slag ( 19 ) with a high chromium content is melted together with the added charge, the slag is then reduced during the melting process with the silicon and carbon under favorable thermodynamic conditions of the arc, once the slag has reached a minimum temperature of 1,490° C. and the slag is subsequently removed. The air-refining process is then carried out, during which the carbon content is reduced to a value of less than 0.9%. The metal slag ( 18 ) is tapped at a tapping temperature of between 1,620 and 1,720° C., the unreduced slag ( 19 ) with a high chromium content from the air-refining process remaining in the treatment vessel.
    • 10. 发明专利
    • DE50101945D1
    • 2004-05-13
    • DE50101945
    • 2001-09-27
    • SMS DEMAG AG
    • GOETZINGER REINERLEMKE STEFANREICHEL JOHANNROLLINGER BERNT
    • C21C7/00C21C5/00C21C5/52C21C7/068F27B3/04F27B3/22
    • The invention relates to a method for producing stainless steels, in particular steels containing chromium and chromium-nickel. The method is carried out in a melting device containing a metallurgical vessel, or in a melting device ( 1 ) containing at least two vessels ( 2, 3 ) for supplying a steel-casting installation, an electric arc furnace process ( 1 ) and an air-refining process taking place alternately in the two vessels ( 2, 3 ). To improve the efficiency of a method of this type, the aim of the invention is to carry out a reversible treatment of unreduced converter slag in the electric-arc furnace mode. To achieve this, in the first treatment stage, the slag ( 19 ) with a high chromium content is melted together with the added charge, the slag is then reduced during the melting process with the silicon and carbon under favorable thermodynamic conditions of the arc, once the slag has reached a minimum temperature of 1,490° C. and the slag is subsequently removed. The air-refining process is then carried out, during which the carbon content is reduced to a value of less than 0.9%. The metal slag ( 18 ) is tapped at a tapping temperature of between 1,620 and 1,720° C., the unreduced slag ( 19 ) with a high chromium content from the air-refining process remaining in the treatment vessel.