    • 1. 发明申请
    • METHOD AND FINISHING TRAIN FOR HOT-ROLLING STARTING MATERIAL
    • 方法并准备轧机热轧的输入材料的
    • WO2007051521A3
    • 2008-05-22
    • PCT/EP2006009954
    • 2006-10-16
    • SMS DEMAG AGSEIDEL JUERGENPETERS MATTHIAS
    • SEIDEL JUERGENPETERS MATTHIAS
    • C21D1/42B21B1/46B21B37/74B21B45/00C21D8/02C21D8/04C21D11/00
    • C21D1/42B21B1/24B21B1/463B21B45/004C21D8/0226C21D8/0426C21D11/00Y02P10/253
    • The invention relates to a method and a finishing train for hot-rolling starting material. Starting material is finished in several successive roll stands (110 n) in the finishing train, the material cooling off because of heat loss. The material has to be reheated in order for the temperature of the material not to drop below the predefined lower threshold temperature value at low speeds within and at the discharge end of the finishing train. In order to use as little energy as possible for said reheating process, the reheating process within the finishing train is carried out for the first time only when the temperature of the material risks falling below the lower threshold temperature value for the first time relative to the direction of flow of the material because of heat loss. Furthermore, the temperature of the material during the reheating process is increased only to the point where the temperature of the material will not drop below the lower threshold temperature value (T U ) while the material is conveyed on to a next heating device that is mounted downstream in the direction of flow of the material and until the material is discharged from the mill train.
    • 本发明涉及一种方法和用于输入材料的热轧精轧机。 在精轧机组的输入材料是在多个连续的轧辊架(110 - N)精轧,由此材料冷却由于热损失。 因此,材料的温度不降低内和在低速下低于预定下限温度阈值的值在精轧机组的出口处,该材料必须被再次精轧机组内加热。 为了保持能量对于此再加热越低越好,本发明提出的是,由于在材料流动方向上有可能下降到低于下限温度阈值在第一次的热损失进行再加热的第一次仅精轧机组,它看见的材料的温度范围内有。 还提议以增加材料的温度在再加热刚好足够的,使得在该材料向上的至紧邻的下游加热器的进一步输送和直到离开轧机机组只到较低的温度阈值(涂),而不是在该材料的流动方向观察时的温度 但骨子里,下降。
    • 3. 发明申请
    • METHOD AND DEVICE FOR PRODUCING A METAL STRIP BY CONTINUOUS CASTING
    • 方法和设备用于生产金属带连铸
    • WO2007137739A3
    • 2008-07-31
    • PCT/EP2007004560
    • 2007-05-23
    • SMS DEMAG AGSEIDEL JUERGENSUDAU PETER
    • SEIDEL JUERGENSUDAU PETER
    • B22D11/12
    • B22D11/1206B21B1/463
    • The invention relates to a method for producing a metal strip (1) by continuous casting. According to said method, a slab (3), preferably a thin slab, is initially cast in a casting machine (2), said slab being deviated from a vertical direction (V) into a horizontal direction (H), and in the direction of transport (F) of the slab (3) arranged behind the casting machine (2), the slab (3) is subjected to a milling operation in the milling machine (4), in which at least one surface of the slab (3), preferably two surfaces which are opposite to each other, are milled. In order to obtain a high economic viability and improved machining parameters when the strips are rolled, the slab (3) is milled as a first mechanical machining step after the slab (3) is deviated in the horizontal direction (H). The slab (3) is cast with a thickness (d) of at least 50 mm and the slab (3) is cast with a mass flow, which is the product of the casting speed and the slab thickness (v x d), of at least 350 m/min x mm. The invention also relates to a device for producing a metal strip by continuous casting.
    • 本发明涉及一种用于通过连续铸造生产金属带材(1),其特征在于最初在铸造机(2),一平板(3),优选的薄板坯铸造,由垂直方向(V)(在水平方向ħ )进行偏转,其中,在所述板坯的输送方向(F)(3)的铸造机后面(2),所述平板(3),以在研磨机(4)研磨操作,其中,所述板(3)的至少一个表面上,优选两个 相对表面,进行研磨。 为了实现带材的轧制过程中更高的效率和改善的加工参数,本发明提供的是,板(3)板坯(3)在水平方向的偏转后的第一个机械加工步骤的研磨(H),其中,所述 铸造的至少50毫米,并且其中所述板(3)具有质量流量的至少350米的铸造速度和铸片厚度程序(VxD)的产物的铸造/分钟X毫米发生(3)具有厚度(d)的板坯。 此外,本发明涉及一种用于通过连续铸造生产金属带材。
    • 8. 发明专利
    • METHOD AND DEVICE FOR PRODUCING A METAL STRIP BY CONTINUOUS CASTING
    • CA2653360C
    • 2010-07-20
    • CA2653360
    • 2007-05-23
    • SMS DEMAG AG
    • SEIDEL JUERGENSUDAU PETER
    • B22D11/12
    • The invention relates to a method for producing a metal strip (1) by continuous casting. According to said method, a slab (3), preferably a thin slab, is initially cast in a casting machine (2), said slab being deviated from a vertical direction (V) into a horizontal direction (H), and in the direction of transport (F) of the slab (3) arranged behind the casting machine (2), the slab (3) is subjected to a milling operation in the milling machine (4), in which at least one surface of the slab (3), preferably two surfaces which are opposite to each other, are milled. In order to obtain a high economic viability and improved machining parameters when the strips are rolled, the slab (3) is milled as a first mechanical machining step after the slab (3) is deviated in the horizontal direction (H). The slab (3) is cast with a thickness (d) of at least 50 mm and the slab (3) is cast with a mass flow, which is the product of the casting speed and the slab thickness (v x d), of at least 350 m/min x mm. The invention also relates to a device for producing a metal strip by continuous casting.