    • 2. 发明授权
    • Ceramic composition of matter and its use
    • 陶瓷组合物及其用途
    • US5145540A
    • 1992-09-08
    • US601861
    • 1990-10-23
    • Paul FoleyRainer Buckpesch
    • Paul FoleyRainer Buckpesch
    • C04B37/04C03C10/08C03C14/00C04B35/18H01B3/08H01B3/12H01L21/48H01L23/15H05K1/03H05K3/46
    • C03C14/004H01B3/085H01B3/12H01L21/4807H01L23/15H05K1/0306C03C2214/04H01L2924/0002H01L2924/09701Y10S428/901Y10T428/24917Y10T428/24926
    • A ceramic composition of matter which is sinterable at low temperatures is composed ofa) 40 to 90% by weight of a finely disperse, high-melting oxidic material andb) 10 to 60% by weight of a finely disperse glass having a softening point of 500.degree. to 850.degree. C., a coefficient of thermal expansion (=CTE) of 2 to 5.times.10.sup.-6 K.sup.-1 (measured in the interval from 0.degree. to 400.degree. C.) and a dielectric constant of less than 5 (measured at 10.sup.6 Hz and 20.degree. C.). The finely disperse oxidic material is composed of a mixture of MgO, Al.sub.2 O.sub.3 and SiO.sub.2 in an Al.sub.2 O.sub.3 /MgO weight ratio of 1.8-4 with an SiO.sub.2 weight fraction of 42-65% by weight or an equivalent quantity of corresponding oxide precursors which, on heating, decompose to give these oxides. The MgO or the MgO precursor has a mean grain size of 0.05 to 3 .mu.m and the SiO.sub.2 or the SiO.sub.2 precursor has a mean grain size of 2 to 20 .mu.m. The composition sinters at 900.degree.-1100.degree. C. and is suitable for producing substrates or metallized housings.
    • 在低温下可烧结的物质的陶瓷组合物由以下组成:a)40-90%重量的细分散高熔点氧化物,和b)10-60%重量的具有软化点的细分散玻璃 在500〜850℃下,热膨胀系数(= CTE)为2〜5×10 -6 K -1(在0〜400℃的间隔内测定),介电常数小于5( 在106Hz和20℃测量​​)。 精细分散的氧化物材料由MgO,Al 2 O 3和SiO 2的混合物组成,Al 2 O 3 / MgO重量比为1.8-4,SiO 2重量分数为42-65%重量或相当量的相应氧化物前体, 加热分解,得到这些氧化物。 MgO或MgO前体的平均粒径为0.05〜3μm,SiO 2或SiO 2前体的平均粒径为2〜20μm。 组合物在900°-1100℃烧结,适用于生产基材或金属化外壳。