    • 8. 发明授权
    • Asphalt/aggregate composition of enhanced adhesion
    • 沥青/骨料组合增强附着力
    • US07384468B2
    • 2008-06-10
    • US11010612
    • 2004-12-13
    • James R. ButlerWilliam LeePaul Buras
    • James R. ButlerWilliam LeePaul Buras
    • C08L95/00C09D195/00
    • C08L95/00C08L2666/74
    • An asphalt/aggregate composition having enhanced adhesion characteristics and its preparation. An asphalt base material is heated to a molten state in order to permit mixing of the asphalt with added components. A heavy metal soap is incorporated into the asphalt base material to enhance the adhesion of the asphalt base material with an aggregate component which is mixed with the asphalt base material to provide an asphalt/aggregate blend. The asphalt and aggregate can be blended together in a mixing chamber to provide a fluid asphalt/aggregate concrete which is then dispensed on a substrate surface or the asphalt base material and aggregate components can be separately applied to the substrate surface to provide the ultimate asphalt/aggregate concrete. The heavy metal soap is a C14-C18 heavy metal soap such as zinc stearate. Zinc oxide may also be added to the asphalt base material in an amount which is less than the amount of zinc stearate. The asphalt base material may be polymer-modified asphalt and may incorporate a crumb rubber component to provide a rubber-modified asphalt.
    • 具有增强的粘合特性及其制备的沥青/骨料组合物。 将沥青基材料加热至熔融状态,以使沥青与添加的组分混合。 沥青基材中加入重金属皂以增强沥青基材与沥青基料混合的聚集体组分的粘附性,从而提供沥青/骨料混合物。 沥青和骨料可以在混合室中混合在一起,以提供流体沥青/骨料混凝土,然后将其分配到基材表面上,或者将沥青基体材料和骨料组分分别施加到基材表面以提供最终的沥青/ 骨料混凝土 重金属皂是C 14-14 -C 18重金属皂,例如硬脂酸锌。 也可以将氧化锌以少于硬脂酸锌的量添加到沥青基材中。 沥青基材料可以是聚合物改性沥青,并且可以加入碎屑橡胶组分以提供橡胶改性沥青。
    • 9. 发明申请
    • Process for the preparation of crumb rubber/asphalt blends
    • 制备橡胶/沥青混合料的方法
    • US20080015287A1
    • 2008-01-17
    • US10966969
    • 2004-10-15
    • James R. ButlerWilliam Lee
    • James R. ButlerWilliam Lee
    • C08L23/00
    • C08L19/003C08L21/00C08L95/00C08L2207/24C08L2666/02C08L2666/08
    • A method for preparing a homogeneous blend of asphalt and ground tire rubber. An asphalt base material is heated to a temperature sufficient to permit the stirring of the asphalt base material within a mixing vessel. A particulate crumb rubber component having a designated average particle size is added to the asphalt base material. The crumb rubber material can be partially devulcanized or partially depolymerized and may be accompanied by the incorporation of another rubber component, such as a ground styrene butadiene rubber. Zinc oxide is added to the asphalt base material. The mixture incorporating the zinc oxide is stirred for a period sufficient to provide for substantial solubilization of the crumb rubber within the asphalt base material to provide a blend which has a higher homogeneity than a corresponding blend of the same asphalt and particulate rubber components which is heated and stirred under the identical conditions, but without the addition of the zinc oxide.
    • 一种制备沥青和地面轮胎橡胶均匀混合物的方法。 将沥青基材料加热到足以允许在混合容器内搅拌沥青基料的温度。 将具有指定平均粒径的颗粒状碎屑橡胶组分加入到沥青基材中。 碎屑橡胶材料可以部分地脱硫或部分解聚,并且可以伴随着另外的橡胶组分如丁苯橡胶的掺入。 将氧化锌加入到沥青基材中。 将掺入氧化锌的混合物搅拌足够的时间以使碎屑橡胶在沥青基体材料中显着溶解,以提供与相同的沥青和颗粒状橡胶组分的相应混合物具有更高的均匀性的共混物,该共混物被加热 并在相同条件下搅拌,但不加入氧化锌。