    • Polypropylene resin composition
    • 聚丙烯树脂组合物
    • US5308908A
    • 1994-05-03
    • US936389
    • 1992-08-28
    • Osamu FukuiKouhei UenoYoshifumi NakanoIkunori SakaiTakao NomuraTakeyoshi NishioHisayuki Iwai
    • Osamu FukuiKouhei UenoYoshifumi NakanoIkunori SakaiTakao NomuraTakeyoshi NishioHisayuki Iwai
    • C08K3/34C08L23/08C08L23/16C08L53/00C08L23/04
    • C08K3/34C08L53/00C08L2205/02C08L23/0815C08L23/16
    • A polypropylene resin composition comprising:(A) 45 to 70% by weight of an ethylene-propylene block copolymer synthesized under the process comprising the steps of;(a) polymerizing propylene with a Ziegler-Natta catalyst to obtain a highly crystalline polypropylene that contain not less than 97% by weight of a fraction insoluble in boiling n-heptane, and(b) copolymerizing ethylene with the polypropylene (a), and which(a) contains 0.5 to 10% by weight of ethylene,(b) contains 5 to 20% by weight of a fraction being soluble in p-xylene at room temperature and having an intrinsic viscosity value of not less than 2 (measured in decalin at 135.degree. C.),(c) has a melt-flow index value of 30 to 100 g/10 min., and,(d) has a value of flexural modulus of not less than 18,000 kg/cm.sup.2,(B) 10 to 20% by weight of an amorphous ethylene-propylene copolymer having(a) an ethylene content of 70 to 90% by weight,(b) a Mooney viscosity value (ML.sub.1+4 at 100.degree. C.) of 5 to 70,(C) 5 to 15% by weight of an ethylene-.alpha.-olefin copolymer having(a) an .alpha.-olefin content of 5 to 15% by mole,(b) a value of gravity of not more than 0.91, and(c) a melt-flow index value of 2.2 to 50 g/10 min. at 230.degree. C.,(D) 1 to 10% by weight of an amorphous ethylene-butene copolymer having(a) a butene content of 10 to 25% by weight, and(b) a Mooney viscosity value (ML.sub.1+4, at 100.degree. C.) of 5 to 20,(E) not more than 15% by weight of a talc that(a) has an average diameter D50 of from 1.0 to 3.0 .mu.m, and(b) does not contain a particle having a diameter of 10 .mu.m or more,wherein the component (B) is rubber reinforced by lamellae of components (C) and (D).
    • 一种聚丙烯树脂组合物,其包含:(A)45至70重量%的在包括以下步骤的方法中合成的乙烯 - 丙烯嵌段共聚物: (a)用齐格勒 - 纳塔催化剂聚合丙烯以获得含有不少于97重量%不溶于沸腾正庚烷的馏分的高度结晶的聚丙烯,和(b)使乙烯与聚丙烯(a)共聚,和 (a)含有0.5〜10重量%的乙烯,(b)在室温下含有5〜20重量%的可溶于对二甲苯的馏分,其特性粘度值不小于2(以 十氢萘在135℃),(c)的熔体流动指数值为30〜100g / 10分钟,(d)弯曲弹性模量值不小于18,000kg / cm 2,(B )10〜20重量%的(a)乙烯含量为70〜90重量%,(b)门尼粘度值(100℃时ML1 + 4)为5〜70的无定形乙烯 - 丙烯共聚物 ,(C)5〜15重量%的(a)α-烯烃含量为5〜15摩尔%的乙烯-α-烯烃共聚物,(b)重力值不大于0.91,( c)熔体流动inde x值为2.2〜50g / 10min。 (D)1〜10重量%的(a)丁烯含量为10〜25重量%的无定形乙烯 - 丁烯共聚物,(b)门尼粘度值(ML1 + 4, 在100℃下为5〜20,(E)不超过15重量%的滑石,(a)平均直径D50为1.0〜3.0μm,(b)不含有颗粒 其直径为10μm以上,其中,成分(B)由成分(C)和(D)的薄片橡胶增强。
    • 3. 发明授权
    • Crystalline propylene block-copolymer composition for use in automobile
parts
    • 用于汽车零件的结晶丙烯嵌段共聚物组合物
    • US6121363A
    • 2000-09-19
    • US251331
    • 1999-02-17
    • Ikunori SakaiMikio HashimotoTakayuki NagaiTakao NomuraMasatoshi MatsudaOsamu KitoHisayuki Iwai
    • Ikunori SakaiMikio HashimotoTakayuki NagaiTakao NomuraMasatoshi MatsudaOsamu KitoHisayuki Iwai
    • B29C45/00B29K23/00C08K3/34C08L53/00C08L53/02C08K3/22C08L23/10
    • C08L53/00
    • A crystalline propyleiie block-copolymer composition exhibiting superior flowability upon molding for use in automobile parts, which composition comprises 41 to 71% by weight of a crystalline propylene block-copolymer composed of a propylene homopolymer portion (Fp) and an ethylene/propylene random copolymer portion (Fc) and having an ethylene content of 1 to 10% by weight and a melt flow rate (MFR) of 20 to 100 g/10 min.; 12 to 22% by weight of a first hydrogenated product of a block-copolymer having a relatively smaller stylene content; 2 to 12% by weight of a second hydrogenated product of a block-copolymer having a relatively greater stylene content; and 15 to 25% by weight of talc, wherein the propylene homopolymer portion (Fp) contains 20 to 50% by weight of a low molecular weight propylene homopolymer having an MFR of 400 to 1,000 g/10 min., the average MFR being 100 to 350 g/10 min. and the isotactic pentad fraction being at least 98%, and wherein the said (Fc) has an intrinsic viscosity of 7 dl/g or higher.
    • 一种结晶丙烯嵌段共聚物组合物,其成型用于汽车部件时具有优异的流动性,该组合物包含41至71重量%的由丙烯均聚物部分(Fp)和乙烯/丙烯无规共聚物组成的结晶丙烯嵌段共聚物 (Fc),乙烯含量为1〜10重量%,熔体流动速率(MFR)为20〜100g / 10分钟。 12至22重量%的具有相对较小的苯乙烯含量的嵌段共聚物的第一氢化产物; 2至12重量%的具有相对较大的苯乙烯含量的嵌段共聚物的第二个氢化产物; 和15〜25重量%的滑石,其中丙烯均聚物部分(Fp)含有20〜50重量%的MFR为400〜1000g / 10分钟的低分子量丙烯均聚物,平均MFR为100 至350g / 10min。 和全同立构五单元组分数为98%以上,其中所述(Fc)的特性粘度为7dl / g以上。
    • 10. 发明授权
    • Polypropylene-base resin composition and products of injection molding thereof
    • 聚丙烯基树脂组合物及其注射成型品
    • US06441081B1
    • 2002-08-27
    • US09555826
    • 2000-07-11
    • Hajime SadatoshiKenichi OhkawaSusumu KanzakiHisayuki IwaiTakao NomuraShoichi Ichikawa
    • Hajime SadatoshiKenichi OhkawaSusumu KanzakiHisayuki IwaiTakao NomuraShoichi Ichikawa
    • C08K334
    • C08L23/12C08F297/083C08L23/0815C08L23/10C08L23/16C08L53/00C08L2666/04C08L2666/24C08L2666/02
    • A polypropylene resin composition which comprises: (1) 55 to 75% by weight of (A) a polypropylene resin consisting of a mixture of the following polymers (i) and (ii): (i) a propylene-ethylene block copolymer having a propylene homopolymer part which is the first segment and having a propylene-ethylene random copolymer part which is the second segment and (ii) a propylene homopolymer having an intrinsic viscosity [&eegr;]P of 0.8 to 1.8 dl/g as measured in tetralin at 135° C., (2) 21 to 30% by weight of (B) an ethylene-1-octene copolymer rubber having a melt flow rate (JIS-K-6758 at 190° C.) of 2 to 10 g/10 min and having a 1-octene component content of 20 to 25% by weight, and (3) 5 to 20% by weight of (C) talc having an average particle diameter of not more than 3 &mgr;m, wherein when the amount of the second segment contained in the propylene-ethylene block copolymer of the polypropylene resin (A) is designated as (A)′ and the ethylene-1-octene copolymer rubber content is designated as (B)′, the following expression is satisfied: 0.10≦{(A)′/[(A)′+(B)′]}≦0.30, and when the above composition is subjected to a tensile test according to ASTM D638, it exhibits, an ultimate elongation of at least 400%, and the melt flow rate (JIS-K-6758 at 230° C.) of the composition is at least 30 g/10 min, and an injection-molded article obtained by injection molding the above polypropylene resin composition.
    • 一种聚丙烯树脂组合物,其包含:(1)55至75重量%的(A)由以下聚合物(i)和(ii)的混合物组成的聚丙烯树脂:(i)丙烯 - 乙烯嵌段共聚物,其具有 丙烯均聚物部分,其是第一链段并且具有作为第二链段的丙烯 - 乙烯无规共聚物部分和(ii)在135℃下在四氢化萘中测得的特性粘度ηP为0.8至1.8dl / g的丙烯均聚物 (2)熔体流动速率(JIS-K-6758,190℃)的(B)乙烯-1-辛烯共聚物橡胶的21〜30重量%为2〜10g / 10分钟 并且具有20至25重量%的1-辛烯组分含量,和(3)5至20重量%的(C)平均粒径不大于3μm的滑石,其中当第二 包含在聚丙烯树脂(A)的丙烯 - 乙烯嵌段共聚物中的链段被称为(A)',乙烯-1-辛烯共聚物橡胶含量指定为(B)', 满足以下表达式:当根据ASTM D638对上述组合物进行拉伸试验时,其表现出至少400%的极限伸长率和熔体流动速率(JIS-K-6758在230℃) )为30g / 10分钟以上,注射成型上述聚丙烯树脂组合物得到的注射成型体。