会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 2. 发明申请
    • A METHOD OF REDUCING THE FORMATION OF PRIMARY PLATLET-SHAPED BETA-PHASE IN IRON CONTAINING AlSi-ALLOYS, IN PARTICULAR IN Al-Si-Mn-Fe ALLOYS
    • 在Al-Si-Mn-Fe合金中,特别是减少含有AlSi合金的铁中初级平板形成BETA相的形成的方法
    • WO1997013882A1
    • 1997-04-17
    • PCT/SE1996001254
    • 1996-10-09
    • OPTICAST ABBÄCKERUD, LennartARNBERG, LarsCHAI, Guocai
    • OPTICAST AB
    • C22C01/02
    • C22C21/02C22C21/04
    • Iron is a detrimental impurity in aluminium alloys since it causes hard and brittle iron-rich intermetallic phases to precipitate during solidification. The most detrimental phase in the microstructure is the beta-phase of the Al5FeSi-type because it is platelet-shaped. The present invention provides a method of producing iron-containing Al-alloys free from platelet-shaped beta-phase by controlling and regulating the precipitation path during solidification such that the precipitation of Fe containing intermetallic phases starts with the precipitation of the hexagonal phase of the Al8Fe2Si-type. The presence of the Al8Fe2Si-type phase result in that beta-phase will not develop the common platlet-morphology but nucleate on and cover the Al8Fe2Si-type phase which in turn has a less harmful morphology. Furthermore, the invention defines the use of thermal analysis as a means for controlling the morphology of the precipitates.
    • 铁是铝合金中的有害杂质,因为它在固化过程中会导致富铁脆性金属相析出。 微结构中最有害的相是Al5FeSi型的β相,因为它是血小板形的。 本发明提供了一种通过控制和调节凝固过程中的沉淀路径来生产不含血小板形β相的含铁Al合金的方法,使得含Fe金属间相的析出开始于六方相析出 Al8Fe2Si型。 Al8Fe2Si型相的存在导致β相不会形成共同的板状形态,而是在Al8Fe2Si型相上成核并覆盖Al8Fe2Si型相,而Al8Fe2Si型相又具有较小的有害形态。 此外,本发明定义了使用热分析作为控制沉淀物形态的手段。