    • 9. 发明授权
    • Martensitic stainless steel pipe
    • 马氏体不锈钢管
    • US08168008B2
    • 2012-05-01
    • US10587807
    • 2004-12-01
    • Yukio MiyataMitsuo KimuraNoritsugu ItakuraKatsumi Masamura
    • Yukio MiyataMitsuo KimuraNoritsugu ItakuraKatsumi Masamura
    • C22C38/40
    • C22C38/44C21D1/25C21D6/004C21D9/14C22C38/002C22C38/004C22C38/02C22C38/04C22C38/06C22C38/40C22C38/46C22C38/48C22C38/50Y10T428/13
    • A martensitic stainless steel pipe having a heat-affected zone with high resistance to intergranular stress corrosion cracking is provided. In particular, the martensitic stainless steel pipe contains less than 0.0100% of C; less than 0.0100% of N; 10% to 14% of Cr; and 3% to 8% of Ni on a mass basis. Alternatively, the martensitic stainless steel pipe may further contain Si, Mn, P, S, and Al within an appropriate content range. The martensitic stainless steel pipe may further contain one or more selected from the group consisting of 4% or less of Cu, 4% or less of Co, 4% or less of Mo, and 4% or less of W and one or more selected from the group consisting of 0.15% or less of Ti, 0.10% or less of Nb, 0.10% or less of V, 0.10% or less of Zr, 0.20% or less of Hf, and 0.20% or less of Ta on a mass basis. The content Csol defined by the following equation is equal to less than 0.0050%: Csol=C−⅓×Cpre, wherein Cpre=12.0 {Ti/47.9+½(Nb/92.9+Zr/91.2)+⅓(V/50.9+Hf/178.5+Ta/180.9)−N/14.0} or Cpre=0 when Cpre
    • 提供具有耐晶间应力腐蚀开裂性高的热影响区的马氏体不锈钢管。 特别地,马氏体不锈钢管含有小于0.0100%的C; 小于0.0100%的N; 10%〜14%的Cr; 和3%〜8%的Ni。 或者,马氏体不锈钢管可以在适当的含量范围内进一步含有Si,Mn,P,S和Al。 马氏体系不锈钢管可以进一步含有选自Cu,4%以下的Co,4%以下的Mo,4%以下的W和1种以上的选自Cu,4%以下的1种以上 由Ti的0.15%以下,Nb:0.10%以下,V:0.10%以下,Zr:0.10%以下,Hf:0.20%以下,Ta:0.20%以下 基础。 Csol = C-1/3×Cpre,其中Cpre = 12.0 {Ti / 47.9 + 1 /(Nb / 92.9 + Zr / 91.2)+ 1/3(V / 50.9 + 当Cpre <0时,Hf / 178.5 + Ta / 180.9)-N / 14.0}或Cpre = 0。