    • Powder coating composition containing vinylidene fluoride copolymer and methyl methacrylate copolymer
    • 含有偏二氟乙烯共聚物和甲基丙烯酸甲酯共​​聚物的粉末涂料组合物
    • US06551708B2
    • 2003-04-22
    • US09091267
    • 1998-06-17
    • Nobuhiko TsudaRyuzi Iwakiri
    • Nobuhiko TsudaRyuzi Iwakiri
    • C09D0503
    • C09D127/16C08F259/06C08L27/16C08L33/12C09D133/12Y10S525/934Y10T428/2982Y10T428/2998C08F220/14C08L2666/04
    • To provide a powder coating composition being capable of forming a coating film which has good pigment dispersibility, is excellent in weather resistance, film forming ability, appearance and stain-proofing property and, when used for PCM, is difficult to cause cracks because of its particularly excellent bending resistance at the time of bending of a metal plate. The powder coating composition comprises a powder which contains 100 parts by weight of a vinylidene fluoride copolymer having a melting point of not higher than 150° C., a crystallinity of not higher than 35% and a weight average molecular weight (Mw) of 1×104 to 5×105 and 10 to 400 parts by weight of a methyl methacrylate copolymer having a glass transition temperature of not higher than 110° C. and a weight average molecular weight of 1×104 to 5×105; an average particle size of particles constituting the powder being from 1 to 100 &mgr;m and an apparent density of the powder being from 0.2 to 1 g/ml.
    • 为了提供能够形成具有良好颜料分散性的涂膜的粉末涂料组合物,具有优异的耐候性,成膜性,外观和防污性,并且当用于PCM时,难以引起裂纹,因为它 在金属板弯曲时特别优异的抗弯曲性。 粉末涂料组合物包含粉末,其含有100重量份的熔点不高于150℃,结晶度不高于35%,重均分子量(Mw)为1×10 4的偏二氟乙烯共聚物 至5×10 5和10至400份重量的玻璃化转变温度不高于110℃,重均分子量为1×10 4至5×10 5的甲基丙烯酸甲酯共​​聚物; 构成粉末的颗粒的平均粒径为1-100μm,粉末的表观密度为0.2-1g / ml。