    • 2. 发明专利
    • Bearing steel excellent in acoustic property and quietness
    • 轴承钢在声学性质和安静性方面优秀
    • JPH11279710A
    • 1999-10-12
    • JP10003198
    • 1998-03-27
    • Kobe Steel LtdNippon Koshuha Steel Co Ltd日本高周波鋼業株式会社株式会社神戸製鋼所
    • MIZUNO YUKITAKAFURUSAWA SADAYOSHIKANATSUKI KOJI
    • F16C33/58C22C38/00C22C38/38C22C38/58
    • PROBLEM TO BE SOLVED: To obtain a steel excellent in an acoustic property and quietness by making an acid insoluble impurity less than a specified pieces per unit steel when dissolving, in a mixed acid aqueous solution heated to a specified temp, the steel which contains a specified content in each of C, Si, Mn, Cr, Al and the balance Fe with inevitable impurities, and restricts Ti, O in the impurities to a specified content.
      SOLUTION: A content, by weight, is 0.6-1.2% C, 0.1-2.0% Si, 0.1-2.0% Mn, 10.0-14.0% Cr, ≤0.04% Al. Ti, O in the impurities, by weight, ≤0.0015% T, ≤0.0012% O. A mixed acid aqueous solution is prepared by mixing, by mass, 60% nitric acid, 96% sulfuric acid, pure water in the volume ratio of 25:1:55 and heating to 90-95°C. An acid insuluble impurity includes Al
      2 O
      3 of 50%, and its size is ≥15 μm major diameter and is less than 19 pieces in 10 g of the steel. In the case corrosion resistance is not required, a Cr content is 0.8-2.0%, and in the case of needing that of medium degree, it is 2.0-10.0%.
      COPYRIGHT: (C)1999,JPO
    • 要解决的问题:为了通过在溶解时将每单位钢中的特定片数的酸不溶性杂质在加热到规定温度的混合酸水溶液中,使其具有优异的声学性质和安静性的钢, 在C,Si,Mn,Cr,Al中的每一种中指定含量,余量为Fe与不可避免的杂质,并将杂质中的Ti,O限制在规定的含量。 解决方案:重量含量为0.6-1.2%C,0.1-2.0%Si,0.1-2.0%Mn,10.0-14.0%Cr,<= 0.04%Al。 杂质中的Ti,O,<= 0.0015%T,<= 0.0012%O.混合酸水溶液通过以质量计混合60%硝酸,96%硫酸,体积中的纯水 比例为25:1:55,加热至90-95℃。 酸不纯的杂质包括50%的Al 2 O 3,其尺寸>15μm的大直径,并且在10g钢中小于19个。 在不需要耐腐蚀性的情况下,Cr含量为0.8〜2.0%,在中等程度的情况下为2.0〜10.0%。
    • 6. 发明专利
    • MANUFACTURE OF STEPPED ANNULAR MEMBER, AND INNER AND OUTER RING MEMBER
    • JPH11197780A
    • 1999-07-27
    • JP1638498
    • 1998-01-12
    • NIPPON KOSHUHA STEEL CO LTD
    • IMAI KATSUYAKAWADA YOKOFURUSAWA SADAYOSHINAKADA MITSUAKIOKAMOTO SATORUIRISAWA KATSUFUMI
    • B21J5/06B21K1/04B21K21/08
    • PROBLEM TO BE SOLVED: To provide a manufacturing method in which the concentricity of each inside diameter and outside diameter of a large diameter cylindrical part and a small diameter cylindrical part of a forged stepped annular member can be machined with high accuracy, the cutting of the inside and outside diameter sides can be dispensed with, and the grinding can be directly performed. SOLUTION: In a forging method in which a disk-like stock 34' is forged or extruded to form a stepped annular member 43 where a large diameter cylindrical part 35 is concentrically connected to a small diameter cylindrical part 38 through a connection part 42, a recessed part 35A of the diameter slightly smaller than the inside diameter of a large diameter part of a product is formed on one surface side of the disk-like stock, and a cup-like stock 37 having a projecting part 36 is formed on the other surface side, a small diameter cylindrical part side of a stepped annular member is formed by the forward extrusion so that a die and a punch are not relatively moved to each other in the projecting part, an inner surface of the recessed part is ironed or extruded by the forward extrusion method to form the inside diameter of the recessed part to be the same as that of a large diameter part of the product, and a bottom plate part 38 on the inside diameter side of the small diameter cylindrical part is punched to communicate the recessed ports of the large diameter cylindrical part 35 and the small diameter cylindrical part. communicate the recessed part of the large diameter cylindrical part 35 with that of the small diameter cylindrical part 38.