    • 7. 发明授权
    • Process for producing customized thermoplastic resins
    • 生产定制热塑性树脂的方法
    • US5846607A
    • 1998-12-08
    • US884943
    • 1997-06-30
    • James M. HurleyBernd B. Brian
    • James M. HurleyBernd B. Brian
    • B05D1/18B05D3/02B05D7/02C08J3/20C08J3/22
    • C08J3/226B05D1/18B05D3/0218B05D7/02C08J3/203C08J2423/00C08J2491/00
    • Disclosed is a method for customizing a thermoplastic resin in which a thermoplastic resin body, a thermoplastic polymeric component, and an additive component are provided in a container with means for mixing. The thermoplastic resin body is at a first temperature that is above the onset temperature of the melt processing range of the polymeric component. A coating that is a mixture of the additive component and the polymeric component is formed on at least a portion of the thermoplastic resin body. After the coating is applied, the resin body is cooled to solidify the coating composition. The customized thermoplastic resins produced according to the invention may be heated to above the onset temperature of the melt processing range of the resin body, mixed to form a substantially uniform mixture and formed into an article.
    • 公开了一种定制热塑性树脂的方法,其中将热塑性树脂体,热塑性聚合物组分和添加剂组分设置在具有混合装置的容器中。 热塑性树脂体处于高于聚合物组分的熔融加工范围的起始温度的第一温度。 在热塑性树脂体的至少一部分上形成作为添加成分和聚合物成分的混合物的涂层。 涂布后,将树脂体冷却,固化涂料组合物。 根据本发明制备的定制热塑性树脂可以被加热到高于树脂体的熔融加工范围的起始温度,混合以形成基本均匀的混合物并形成制品。
    • 8. 发明授权
    • Rigid thermoplastic article having soft covering
    • 具有柔软覆盖层的刚性热塑性制品
    • US5932353A
    • 1999-08-03
    • US994785
    • 1997-12-19
    • Roger Jyh-Chiarng R. HuarngJames M. Hurley
    • Roger Jyh-Chiarng R. HuarngJames M. Hurley
    • B32B27/08B32B27/34B32B27/40
    • B32B27/08Y10T428/31551Y10T428/31562
    • The present invention provides a process for making articles of manufacture, as well as the articles themselves, comprising thermoplastic nylon materials and thermoplastic polyurethane blends capable of adhering to the thermoplastic nylon materials, wherein the thermoplastic polyurethane blends comprise:a) 3 to 200 parts of a terpolymer of styrene/.alpha.-methylstyrene/acrylonitrile/C.sub.1 -C.sub.6 alkyl acrylate with a glass transition temperature (Tg) below 0.degree. C.;b) 100 parts of a thermoplastic polyurethane produced from a diisocyanate, a C.sub.2 -C.sub.10 diol, and a polyether and/or polyester-based polyol; andc) 0 to 50 parts of various additives including lubricants, pigments, stabilizers, etc. The articles of manufacture may be configured as power tool housings, luggage handles, gear shifts, automotive pedals, etc.
    • 本发明提供了一种制造制品的方法,以及制品本身,其包括热塑性尼龙材料和能够粘附到热塑性尼龙材料上的热塑性聚氨酯共混物,其中热塑性聚氨酯共混物包括:a)3至200份 苯乙烯/α-甲基苯乙烯/丙烯腈/丙烯酸C1-C6烷基酯的三元共聚物,玻璃化转变温度(Tg)低于0℃。 b)100份由二异氰酸酯,C2-C10二醇和聚醚和/或聚酯类多元醇制得的热塑性聚氨酯; 和c)0至50份各种添加剂,包括润滑剂,颜料,稳定剂等。制品可以被配置为电动工具壳体,行李把手,换挡,汽车踏板等。
    • 9. 发明授权
    • Process for producing customized thermoplastic resins
    • 生产定制热塑性树脂的方法
    • US5919530A
    • 1999-07-06
    • US884803
    • 1997-06-30
    • James M. HurleyBernd B. BrianMary E. TuttleBill Popovski
    • James M. HurleyBernd B. BrianMary E. TuttleBill Popovski
    • C08J3/22B05D3/06
    • C08J3/226C08J2491/00Y10T156/10
    • Disclosed is a method for customizing a thermoplastic resin in which a thermoplastic resin body is at least partially coated with a thermoplastic coating composition comprising an additive component and a polymeric component. The thermoplastic resin body is at a temperature that is above the onset temperature of the melt processing range of the coating composition. After the coating is applied, the resin body is cooled to solidify the coating composition. Customized thermoplastic resins may be produced more efficiently using the present method than by conventional methods. The customized thermoplastic resins produced according to the invention may be heated to above the onset temperature of the melt processing range of the resin body, mixed to form a substantially uniform mixture and formed into an article.
    • 公开了一种定制热塑性树脂的方法,其中热塑性树脂体至少部分地涂覆有包含添加剂组分和聚合物组分的热塑性涂料组合物。 热塑性树脂体的温度高于涂料组合物的熔融加工范围的起始温度。 涂布后,将树脂体冷却,固化涂料组合物。 使用本方法可以比常规方法更有效地制备定制的热塑性树脂。 根据本发明制备的定制热塑性树脂可以被加热到高于树脂体的熔融加工范围的起始温度,混合以形成基本均匀的混合物并形成制品。