    • 7. 发明申请
    • Method for Producing Low Anisotropy Pressure-Sensitive Adhesives
    • 生产低各向异性压敏粘合剂的方法
    • US20080226905A1
    • 2008-09-18
    • US12090896
    • 2006-11-01
    • Thilo DollaseBernd DietzKlaus Keite-Telgenbuscher
    • Thilo DollaseBernd DietzKlaus Keite-Telgenbuscher
    • B05D5/10B32B7/12
    • C09J133/04C09J7/10C09J7/20C09J9/00C09J2433/00Y10T428/28
    • The invention relates to a method for producing pressure-sensitive adhesives that have low or no anisotropy, the process elements including an adhesive supply system, an application unit and a placement element. A melt strip of the pressure-sensitive adhesive is produced between the outlet of the application unit and the point of placement on the placement element and is stretched. The invention is characterized by controlling the stretching of the pressure-sensitive adhesive in the free melt strip by adjusting an effective ration G which is defined as the ratio of the effective time Δt of the stretching to the stretching rate R, and which is adjust to a value of not more that 0.008 s2. The effective time Δt is defined by the formula 2 Lr/[vstrip (1+r)] wherein L is the length of the melt strip, r is the stretching ratio and vstrip is the speed of the melt strip and the stretching rate R is defined as a temporal derivative of the stretching ratio r.
    • 本发明涉及一种具有低或无各向异性的压敏粘合剂的制造方法,所述工艺元件包括粘合剂供应系统,涂布单元和放置元件。 在施加单元的出口和放置元件上的位置之间产生压敏粘合剂的熔融条,并且被拉伸。 本发明的特征在于通过调节定义为拉伸的有效时间Deltat与拉伸速度R的比值的有效比例G来控制自由熔融条中的压敏粘合剂的拉伸,并将其调整为 不大于0.008s <2的值。 有效时间Deltat由公式2 Lr / [v> strip(1 + r)]定义,其中L是熔体条的长度,r是拉伸比,v带 / SUB>是熔条的速度,拉伸速度R被定义为拉伸比r的时间导数。
    • 8. 发明申请
    • Method for Producing High Anisotropy Pressure-Sensitive Adhesives
    • 生产高各向异性压敏粘合剂的方法
    • US20100221532A1
    • 2010-09-02
    • US12090923
    • 2006-11-01
    • Thilo DollaseBernd DietzKlaus Keite-Telgenbuscher
    • Thilo DollaseBernd DietzKlaus Keite-Telgenbuscher
    • C09J7/02B05D5/10B05D3/06
    • C09J133/04C09J7/10C09J2407/00C09J2421/00C09J2423/00C09J2431/00C09J2433/00Y10T428/28
    • The invention relates to a method for producing pressure-sensitive adhesives that have low or no anisotropy, the process elements including an adhesive supply system, an application unit and a placement element. A melt strip of the pressure-sensitive adhesive is produced between the outlet of the application unit and the point of placement on the placement element and is stretched. The invention is characterized by controlling the stretching of the pressure-sensitive adhesive in the free melt strip by adjusting an effective ratio G which is defined as the ratio of the effective time Δt of the stretching to the stretching rate R, and which is adjusted to a value of at least 0.006 s2 or to a value of not more that 0.004 s2. The effective time Δt is defined by the formula 2Lr/[vstrip(1+r)] wherein L is the length of the melt strip, r is the stretching ratio and vstrip is the speed of the melt strip and the stretching rate R is defined as a temporal derivative of the stretching ratio r.
    • 本发明涉及一种具有低或无各向异性的压敏粘合剂的制造方法,所述工艺元件包括粘合剂供应系统,涂布单元和放置元件。 在施加单元的出口和放置元件上的位置之间产生压敏粘合剂的熔融条,并且被拉伸。 本发明的特征在于通过调节有效比G来控制自由熔体条中的压敏粘合剂的拉伸,该有效比G定义为拉伸的有效时间&Dgr; t与拉伸速度R的比值, 调整为至少0.006s2的值或不大于0.004s2的值。 有效时间&Dgr t由公式2Lr / [vstrip(1 + r)]定义,其中L是熔体条的长度,r是拉伸比,vstrip是熔条的速度,拉伸速率R 被定义为拉伸比r的时间导数。
    • 10. 发明授权
    • Process for producing a rubber-based double-sided pressure-sensitive adhesive tape
    • 橡胶系双面粘合带的制造方法
    • US06527899B1
    • 2003-03-04
    • US09063745
    • 1998-04-21
    • Bernd DietzWerner Kluge-PalettaWerner KarmannBodo SzonnFrank Henke
    • Bernd DietzWerner Kluge-PalettaWerner KarmannBodo SzonnFrank Henke
    • B29C4706
    • B32B25/08B29C47/0021B29C47/065B29C47/145B32B37/153B32B2038/0076B32B2310/0887B32B2405/00
    • Process for producing a pressure-sensitive double-sided adhesive tape, in which a) a ready-made rubber-based backing material is introduced into a screw extruder, where 1. the backing material is heated by means of heating elements present on the screw extruder, 2. in a degassing zone, the backing material is freed from volatile constituents by means of the application of reduced pressure, 3. the backing material is homogenized and brought to the intended temperature, b) in a co-extrusion adapter, a barrier layer conveyed by means of a further appropriate melting and conveying unit is placed onto the backing material on both sides, c) the resulting intermediate laminate is supplied to a three-channel slot die and is uniformly extruded in web form, d) in the said three-channel slot die a pressure-sensitive hotmelt adhesive, supplied in each case with the aid of an appropriate melting and conveying unit, is applied, top and bottom, over the whole area of the intermediate laminate, e) the adhesive tape thus produced is placed onto an antiadhesive substrate, preferably siliconized paper, f) if desired, the adhesive tape is cooled and crosslinked.
    • 制造压敏双面胶带的方法,其中a)将现成的橡胶基背衬材料引入螺杆挤出机中,其中1。 背衬材料通过存在于螺杆挤出机上的加热元件2来加热。 在脱气区,通过减压的应用,背衬材料可以免去挥发性成分3。 将背衬材料均质化并达到预期温度,b)在共挤出接头中,通过另一适当的熔化和输送单元输送的阻隔层被放置在两侧的背衬材料上,c)所得到的中间体 层压板被供应到三通道槽模,并且均匀地以网状形式挤出,d)在所述三通道槽模中,借助于适当的熔化和输送单元在每种情况下供应的压敏热熔粘合剂, 在中间层压体的整个区域上施加顶部和底部,e)将如此生产的粘合带放置在防粘衬底上,优选硅化纸上,f)如果需要,粘合带被冷却和交联。