    • 3. 发明授权
    • Process for producing aromatic polyester carbonate resin
    • 制备芳香族聚酯碳酸酯树脂的方法
    • US4395534A
    • 1983-07-26
    • US322244
    • 1981-11-17
    • Senzo ShimizuIsao NomuraMasahiro HaradaMotohachi UsuiSusumu TaniyamaShigeo Yanada
    • Senzo ShimizuIsao NomuraMasahiro HaradaMotohachi UsuiSusumu TaniyamaShigeo Yanada
    • C08G63/64
    • C08G63/64
    • A process for producing an aromatic polyester carbonate resin in which the molar ratio of the dihydric phenolic compound residue to aromatic dicarboxylic acid residue to carbonate bond is in the range of 2:0.5:1.5-2:1.4:0.6 and these constituent components form an alternating configuration of high regularity, said process comprising a first step wherein in producing a hydroxyl-terminated aromatic oligocarbonate by reacting a dihydric phenolic compound with a halogenated carbonyl compound in a reaction medium consisting of water and a water-immiscible solvent in the presence of a basic inorganic compound, the reaction is carried out by using the basic inorganic compound in an amount of 0.6-1.6 moles per mole of the dihydric phenolic compound and the halogenated carbonyl compound in an amount of 0.3-0.8 mole per mole of the dihydric phenolic compound to form a reaction product mixture consisting predominantly of a phenolic hydroxyl-terminated oligocarbonate of a degree of polymerization of 1-3, and a second step in which an esterification reaction is carried out by reacting the reaction product mixture obtained in the first step with an aromatic dicarboxylic acid dichloride in the presence of a basic inorganic compound in an amount at least sufficient to neutralize the free phenolic hydroxyl groups that remain in the reaction product mixture.
    • 一种芳族聚酯碳酸酯树脂的制造方法,其中二羟基酚类化合物残基与芳族二羧酸残基与碳酸酯键的摩尔比在2:0.5:1.5-2:1.4:0.6的范围内,并且这些组成成分形成 所述方法包括第一步骤,其中通过在由水和水不混溶溶剂组成的反应介质中在二元酚化合物与卤代羰基化合物的反应介质中反应来制备羟基封​​端的芳族低聚碳酸酯 碱性无机化合物,通过使用每摩尔二元酚类化合物和卤代羰基化合物的0.6-1.6摩尔量的碱性无机化合物,其量为每摩尔二羟基酚化合物0.3-0.8摩尔 以形成主要由聚合度为酚羟基封端的低聚碳酸酯组成的反应产物混合物 为1-3,第二步是在碱性无机化合物存在下使至少足以中和的第一步获得的反应产物混合物与芳族二羧酸二氯化物反应进行酯化反应 保留在反应产物混合物中的游离酚羟基。