    • 4. 发明授权
    • Nitrile resin composition
    • 丁腈树脂组成
    • US6084028A
    • 2000-07-04
    • US152518
    • 1998-09-14
    • Makoto SomedaMasahiro KanekoMitsuo KawataKyoji KurodaHiroaki NarisawaShinichi Asai
    • Makoto SomedaMasahiro KanekoMitsuo KawataKyoji KurodaHiroaki NarisawaShinichi Asai
    • C08F279/02C08L51/04C08G63/40C08G63/685C08G69/44
    • C08F279/02C08L51/04
    • A nitrile resin composition having excellent transparency, antistatic properties and practical physical properties. The composition comprises (A) 80 to 97 wt. % of a nitrile resin which is obtained by graft copolymerization, in the presence of 3 to 30 parts by weight of a rubbery polymer containing at least 50 wt. % of a conjugated diene unit, of 100 parts by weight of a monomer mixture containing an unsaturated nitrile and an alkyl methacrylate, and has, as a matrix component, 65 to 80 wt. % of an unsaturated nitrile unit and 20 to 35 wt. % in total of an alkyl (meth)acrylate unit and a unit of a further monomer copolymerizable with the unsaturated nitrile and alkyl (meth)acrylate; and (B) 3 to 20 wt. % of a polyether ester amide, wherein the ratio of the melt viscosity of the component (A) to that of the component (B) at 210.degree. C. is 0.5 to 5 at a shear rate of 10.sup.2 sec.sup.-1 and 0.5 to 3 at a shear rate of 10.sup.3 sec.sup.-1 and the difference of the refractive index between the matrix component (A) to the component (B) is 0.2 or less.
    • 具有优异透明性,抗静电性和实用物理性能的腈树脂组合物。 组合物包含(A)80-97重量% 通过接枝共聚获得的腈树脂的%,在3〜30重量份含有至少50重量%的橡胶状聚合物的情况下, %的共轭二烯单元,100重量份的含有不饱和腈和甲基丙烯酸烷基酯的单体混合物,并且具有65至80重量%的作为基质组分。 %的不饱和腈单元和20〜35wt。 (甲基)丙烯酸烷基酯单元的总数和可与不饱和腈和(甲基)丙烯酸烷基酯共聚的其它单体的单位% 和(B)3〜20重量% %的聚醚酯酰胺,其中组分(A)与组分(B)的熔体粘度在210℃下的比例为0.5至5,剪切速率为102秒-1和0.5至3 剪切速率为103秒-1,基质成分(A)与成分(B)的折射率差为0.2以下。
    • 5. 发明申请
    • Film for thermal sterilization packaging
    • 热灭菌包装膜
    • US20100310842A1
    • 2010-12-09
    • US12735686
    • 2009-02-06
    • Mitsuo Kawata
    • Mitsuo Kawata
    • B32B7/02B32B27/32
    • C08F297/083B32B15/08B32B15/20B32B25/08B32B25/14B32B27/08B32B27/10B32B27/18B32B27/327B32B27/34B32B27/36B32B2264/10B32B2307/30B32B2307/306B32B2307/31B32B2307/412B32B2307/50B32B2307/546B32B2307/558B32B2439/70B32B2439/80Y10T428/2495Y10T428/31938
    • Provided is a film for thermal sterilization packaging which is excellent in a total balance of characteristics such a transparency, an impact resistance, a heat sealing property, a blocking resistance, a heat resistance and the like.The film for thermal sterilization packaging according to the present invention is characterized by comprising: an outer layer containing a propylene/ethylene block copolymer (A) which has a melt flow rate (MFR; ASTM D1238, 230° C., load: 2.16 kg) in the range of 1 to 10 g/10 minutes and a melting point in the range of 150 to 170° C. measured by means of a differential scanning colorimeter. (DSC) and which is constituted from 90 to 80% by weight of a part (Dinsol) insoluble in n-decane at room temperature satisfying the specific requisites and 10 to 20% by weight of a part (Dsol) soluble in n-decane at room temperature satisfying the specific requisites and an intermediate layer or an outer layer containing a propylene/ethylene block copolymer (B) which is not the same as the above propylene/ethylene block copolymer (A).
    • 本发明提供一种热敏杀菌包装用膜,其透明性,耐冲击性,热封性,耐粘连性,耐热性等特性的总体平衡优异。 根据本发明的用于加热灭菌包装的薄膜的特征在于包括:含有丙烯/乙烯嵌段共聚物(A)的外层,其具有熔体流动速率(MFR; ASTM D1238,230℃,载荷2.16kg )在1至10g / 10分钟的范围内,并且通过差示扫描色度计测量在150至170℃范围内的熔点。 (DSC),其由在室温下不溶于正癸烷的部分(Dinsol)90〜80重量%构成,满足特定要求,10〜20重量%的可溶于正癸烷的部分(Dsol) 满足特定要求的室温和含有与上述丙烯/乙烯嵌段共聚物(A)不同的丙烯/乙烯嵌段共聚物(B)的中间层或外层。
    • 6. 发明授权
    • Heat-resistant high-nitrile polymer compositions and process for
preparing same
    • 耐热高腈聚合物组合物及其制备方法
    • US5728775A
    • 1998-03-17
    • US759961
    • 1996-12-03
    • Hiroaki NarisawaMasahiro KanekoMitsuo KawataSyuichi YamaguchiShinichi AsaiMakoto Someda
    • Hiroaki NarisawaMasahiro KanekoMitsuo KawataSyuichi YamaguchiShinichi AsaiMakoto Someda
    • C08F279/02C08L51/04C08L33/20
    • C08F279/02
    • A heat-resistant high-nitrile polymer composition obtained by the graft copolymerization of 100 parts by weight of a monomer mixture comprising 50 to 80% by weight of an unsaturated nitrile monomer, a maleimide monomer, an aromatic vinyl monomer, and a monomer copolymerizable with the foregoing monomers, in the presence of 1 to 40 parts by weight of a conjugated diene-based synthetic rubber containing not less than 50% by weight of a conjugated diene monomer unit, wherein the concentration of residual maleimide monomer in the polymer composition is not greater than 200 ppm by weight. This polymer composition is suitable for use as a molding material for extrusion molding, blow molding, injection molding and the like, and is useful in applications which require gas barrier properties, chemical resistance, non-adsorptive properties and the like, and which require use in automobiles, heat resistance sufficient for heat filling, and safety and hygienic properties.
    • 一种耐热高腈聚合物组合物,其通过将100重量份的单体混合物接枝共聚获得,所述单体混合物包含50至80重量%的不饱和腈单体,马来酰亚胺单体,芳族乙烯基单体和可与 上述单体在1〜40重量份含有不少于50重量%的共轭二烯单体单元的共轭二烯系合成橡胶的存在下,其中聚合物组合物中的残余马来酰亚胺单体的浓度不是 大于200ppm重量。 该聚合物组合物适合用作挤出成型,吹塑成型,注射成型等的成型材料,可用于需要阻气性,耐化学性,不吸附性等的应用中,需要使用 在汽车中,耐热性足以用于热填充,以及安全和卫生性能。