会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明专利
    • Method and apparatus for molding resin molding
    • 用于模制树脂模塑的方法和装置
    • JP2008062427A
    • 2008-03-21
    • JP2006240312
    • 2006-09-05
    • Mazda Motor Corpマツダ株式会社
    • OGAWA JUNICHIKANEKO MITSUHARUICHIHARA YOHEISHINOMORI MASATOSHI
    • B29C69/02B29C45/14B29C49/04B29C49/42B29C49/48B29K105/04B29L9/00
    • PROBLEM TO BE SOLVED: To provide a method for molding a resin molding which can prevent wall thinning while accelerating foaming based on an expandable resin.
      SOLUTION: The molten expandable resin 70 is supplied into a blow-molded body 41 in a mold 4. After that, the mold 4 is opened in the mold opening direction in a prescribed quantity to enlarge a cavity 27. The resin 70 is foamed to expand the blow-molded body 41. To a part 44 wherein the blow-molded body 41 is stretched on the basis of the expansion 2 of the body 41, during the time after the sagging of a parison and before the end of the mold opening action in the prescribed quantity of the mold 4, a molten non-expandable resin 45 is supplied to prevent the wall of the part 44 to be stretched of the blow-molded body 41 from being thinner than the walls of the other parts.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种用于模制树脂模制品的方法,其可以基于可发性树脂加速发泡而防止壁变薄。 解决方案:将熔融的可膨胀树脂70供应到模具4中的吹塑模制体41中。之后,模具4在开模方向上以规定的量打开以扩大空腔27.树脂70 发泡以膨胀吹塑体41.向吹塑模制体41基于主体41的膨胀2拉伸的部分44,在型坯下垂之后和在型坯结束之前的时间内 在规定量的模具4中的开模动作,熔融的不可膨胀树脂45被供给以防止部件44的壁被吹塑体41的拉伸比其他部分的壁更薄 。 版权所有(C)2008,JPO&INPIT
    • 2. 发明专利
    • Deodorization treatment apparatus
    • 除臭处理设备
    • JP2014173774A
    • 2014-09-22
    • JP2013045798
    • 2013-03-07
    • Mazda Motor Corpマツダ株式会社
    • NIIHARA YOSHIMISHINOMORI MASATOSHI
    • F23G7/07F23G7/06
    • PROBLEM TO BE SOLVED: To provide a deodorization treatment apparatus 1 which suppresses the degradation of recovery amount of deodorization rate due to heating treatment succeeding in the time lapse as much as possible and prevents the deodorization rate from lowering too much, in the deodorization treatment apparatus 1 having deodorization treatment means which has gas passage members 23, 24 causing gas to be treated containing organic material to pass therethrough and performs deodorization treatment of the gas to be treated, and deodorization rate recovery means which recovers deodorization rate of the deodorization treatment by subjecting the gas passage members 23, 24 to heating treatment for performing heating into a temperature higher than the temperature upon the deodorization treatment.SOLUTION: Gas to be treated which is heated into a temperature higher than the temperature upon the deodorization treatment is caused to pass through the gas passage member when the deodorization rate is deteriorated to a predetermined value and, thereby, the gas passage member is subjected to the heating treatment and, in the heating treatment succeeding in the time lapse, the heating treatment temperature for the gas passage member is set higher than that in the preceding heating treatment.
    • 要解决的问题:提供一种除臭处理装置1,该除臭处理装置1抑制在时间流逝中尽可能多的加热处理引起的除臭速度的回收量的劣化,并且在除臭处理装置中防止除臭速率降低太多 1,具有除臭处理装置,其具有使含有机材料的被处理气体通过并进行待处理气体的除臭处理的气体通道部件23,24;以及除臭速度回收装置,其通过对除臭处理的除臭速度进行 气体通道构件23,24进行加热处理以进行加热到高于除臭处理温度的温度。解决方案:将被加热到高于除臭处理温度的温度的被处理气体通过 气道通道成员除臭时 n速率劣化到预定值,从而对气体通道部件进行加热处理,并且在随后的加热处理中,将通气部件的加热处理温度设定为高于 进行加热处理。
    • 3. 发明专利
    • Molding process and molding apparatus of resin molding
    • 树脂模塑成型工艺及成型设备
    • JP2009214498A
    • 2009-09-24
    • JP2008062967
    • 2008-03-12
    • Mazda Motor Corpマツダ株式会社
    • OGAWA JUNICHIKANEKO MITSUHARUSHINOMORI MASATOSHI
    • B29C45/56B29C45/28B29K105/04
    • PROBLEM TO BE SOLVED: To suppress an opening or a notched part in a resin molding from becoming larger than desired size in a molding process and a molding apparatus of a resin molding, where a physical foaming agent such as nitrogen and carbon dioxide or a chemical foaming agent such as sodium bicarbonate is contained in a resin and the foaming agent is vaporized at the time of molding.
      SOLUTION: In a core back of a molding die 4, a molten foaming resin 70b is additionally supplied from a second resin supply port 35a into a molten foaming resin body 70a consisting of a molten foaming resin 70 supplied into a cavity 27 in a molding die 4.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 待解决的问题:为了在树脂模制品中抑制树脂模制品中的开口或切口部分在成型过程中变得大于期望的尺寸,以及树脂模制件的模制装置,其中物理发泡剂如氮气和二氧化碳 或者在树脂中含有碳酸氢钠等化学发泡剂,在成型时发泡剂蒸发。 解决方案:在成形模4的芯背中,另外从第二树脂供给口35a将熔融发泡树脂70b供给到供给到空腔27中的熔融发泡树脂70的熔融发泡树脂体70a中 一个成型模具4.版权所有(C)2009,JPO&INPIT
    • 4. 发明专利
    • Joining method of workpiece
    • 工作接合方法
    • JP2009028662A
    • 2009-02-12
    • JP2007196048
    • 2007-07-27
    • Mazda Motor Corpマツダ株式会社
    • TANAKA TSUTOMUHIMURO TAKEYASHINOMORI MASATOSHI
    • B05D7/24B05D3/00B62D65/00C09J5/04C09J201/00
    • PROBLEM TO BE SOLVED: To secure a bonding strength of an adhesion main section more surely while preventing a man-hour increase to give energy.
      SOLUTION: The method comprises the coating process of applying a plurality of rows of adhesives 4 to the adhesion main section of any of one set of the workpieces W, bonded by the chain-reaction type adhesive 4 which cures in a chain-reaction by self-producing inner energy by the energy given from the outside, the mixture-uniting process of overlapping the workpiece W coated with a plurality of rows of the adhesive 4 and a workpiece W which is a counterpart of the workpiece W to mix to bring together the adjacent adhesives among a plurality of rows of the adhesives 4, and the curing process of curing the adhesive 4 giving the energy to cure to the adhesives 4 mixed to bring together.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:为了更加确实地确保粘附主体部分的粘结强度,同时防止工时增加以产生能量。 解决方案:该方法包括将多行粘合剂4施加到通过链式反应型粘合剂4粘合的一组工件W中的任一种的粘合主体部分的涂布过程, 通过从外部产生的能量自身产生内部能量的反应,将涂覆有多行粘合剂4的工件W与作为工件W的对应物的工件W重叠的混合物结合过程混合到 将粘合剂4的多排中的相邻粘合剂组合在一起,以及使粘合剂4固化的固化过程,使粘合剂4固化,从而固化成混合在一起的粘合剂4。 版权所有(C)2009,JPO&INPIT
    • 5. 发明专利
    • Method for joining work piece
    • 加工工作方法
    • JP2009007400A
    • 2009-01-15
    • JP2007167448
    • 2007-06-26
    • Mazda Motor Corpマツダ株式会社
    • TANAKA TSUTOMUHIMURO TAKEYASHINOMORI MASATOSHI
    • C09J5/00C09J163/00C09J201/00
    • PROBLEM TO BE SOLVED: To improve the accuracy of thickness dimension of an adhesive, and also obtain a prescribed curing reaction surely by avoiding a thermal effect caused by a clamp.
      SOLUTION: This method for joining work pieces is provided by forming a hollow projecting part 2b projecting into a work piece W becoming a partner of a work piece W for maintaining the adhesion distance (d) with each other at any one of adhering principal part of a set of work pieces joined by an adhesive 4. By fitting a position-setting member 12 to a recess formed at the reverse surface of the projecting part 2b, the position of the work piece W having the projected part 2b is set. In a state of mediating the adhesive 4 between the position-set work piece W and the work piece W becoming the partner of the work piece W, these work pieces Ws are clamped by a clamping member 21 cooperating with the position-setting member 12. A trigger is given to the adhesive 4 from the position-setting member 12 in the state that the work pieces Ws are clamped.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:为了提高粘合剂的厚度尺寸的精度,并且通过避免由夹具引起的热效应,可靠地获得规定的固化反应。 解决方案:这种连接工件的方法是通过形成一个中空的突出部分2b来形成的,该中空的突出部分2b突出到成为工件W的搭档的工件W中,用于将粘合距离(d)保持在彼此的任何一个粘附 通过粘合剂4接合的一组工件的主要部分。通过将位置设定构件12安装到形成在突出部2b的反面的凹部,设置具有突出部2b的工件W的位置 。 在介于位置固定工件W和成为加工件W的搭接部的工件W之间的粘合剂4的状态下,这些工件Ws被与定位构件12配合的夹紧构件21夹紧。 在夹持工件Ws的状态下,从位置设定部件12向粘合剂4施加触发。 版权所有(C)2009,JPO&INPIT
    • 6. 发明专利
    • Adhesion joint member and manufacturing method of the member
    • 会员联合会员和制造方法
    • JP2008296556A
    • 2008-12-11
    • JP2007148453
    • 2007-06-04
    • Mazda Motor Corpマツダ株式会社
    • TANAKA TSUTOMUHIMURO TAKEYASHINOMORI MASATOSHI
    • B29C65/52B62D25/02B62D25/04B62D25/06B62D25/20C09J5/06C09J9/00C09J201/00
    • PROBLEM TO BE SOLVED: To positively harden the whole of chain hardening adhesives so that a chain hardening reaction of the chain hardening adhesives is not stopped in midway when joining first and second adhered members with each other by the chain hardening adhesives.
      SOLUTION: A recess part 5 continuously extending along an adhesion joint part extending direction is formed near an adhesion joint part of at least one adhered member out of both the adhered members 2, 3. A first chain hardening adhesive 8 is continuously provided along the adhesion joint part extending direction between the adhesion joint parts 6, 7 of the both adhered members 2, 3, and in the recess part 5, the second chain hardening adhesive 9 is brought in contact over the whole adhesion joint part extending direction of the first chain hardening adhesive 8. The second chain hardening adhesive 9 is continuously provided along the adhesion joint part extending direction so that the volume per unit length of the second chain hardening adhesive 9 in the adhesion joint part extending direction is more than the volume per unit length of the first chain hardening adhesive 8 in the adhesion joint member extending direction.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:为了积极地硬化整个链状硬化粘合剂,使得通过链固化粘合剂将第一和第二粘合构件相互连接时,链硬化粘合剂的链硬化反应不会在中途停止。 解决方案:沿粘合接合部延伸方向连续延伸的凹部5形成在粘附构件2,3的至少一个附着构件的粘合接合部附近。连续设置第一链状硬化粘接剂8 沿着两个粘合部件2,3的粘合接合部6,7之间的粘合接合部延伸方向和凹部5中的第二链条硬化粘合剂9在整个粘合接合部延伸方向 第一链条硬化粘合剂8。沿着粘合接合部延伸方向连续设置第二链条硬化粘合剂9,使得第二链条硬化粘合剂9在粘合接合部延伸方向上的每单位长度的体积大于每个 第一链条硬化粘合剂8在粘合接合构件延伸方向上的单位长度。 版权所有(C)2009,JPO&INPIT
    • 7. 发明专利
    • Method and apparatus for molding resin molded product
    • 用于模制树脂模制产品的方法和装置
    • JP2008194840A
    • 2008-08-28
    • JP2007029519
    • 2007-02-08
    • Mazda Motor Corpマツダ株式会社
    • ICHIHARA YOHEIKANEKO MITSUHARUOGAWA JUNICHISHINOMORI MASATOSHI
    • B29C69/02B29C33/76B29C45/14B29C49/04B29C49/42B29K105/04B29L9/00
    • PROBLEM TO BE SOLVED: To suppress a partial decrease in the strength of the surface part of a resin molded product 50 even if a blow molded object 55 which constitutes a skin 52 is made thin-walled by the core back of a mold while accelerating the foaming of a molten foamable resin by the core back of the mold in the case of the molding of the resin molded product 50 composed of a foamed molded object 51 molded using the molten foamable resin and the skin 52 for covering the periphery of the foamed molded object 51. SOLUTION: The molten foamable resin is supplied into the blow molded object 55 so that a foamed cell small diameter part 51a, which is positioned in contact with the part to be stretched (the thin-walled part 52a of the skin 52) due to the expansion at the time of the core back in the blow molded object 55 and keeps the average foam cell diameter small as compared with another part (foamed cell large diameter part 51b), is formed to the foamed molded object 51. COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:即使构成皮肤52的吹塑成型体55由模具的芯背部薄壁化,也可以抑制树脂成型体50的表面部分的强度的部分降低 在模制由使用熔融可发泡树脂模制的发泡成型体51和用于覆盖周边的表皮52构成的树脂模制产品50的情况下,通过模具的芯背加速熔融的可发泡树脂的发泡 发泡成型体51.解决方案:将熔融的可发泡树脂供应到吹塑成型物体55中,使得与待拉伸部分(薄壁部分)接触的发泡单元小直径部分51a 与发泡单元大直径部51b相比,由于吹塑成形体55中的芯部的膨胀而使平均泡沫体直径保持较小,所以形成发泡体 模制对象51. COP YRIGHT:(C)2008,JPO&INPIT
    • 8. 发明专利
    • Method and apparatus for molding resin molding
    • 用于模制树脂模塑的方法和装置
    • JP2008062425A
    • 2008-03-21
    • JP2006240310
    • 2006-09-05
    • Mazda Motor Corpマツダ株式会社
    • OGAWA JUNICHIKANEKO MITSUHARUICHIHARA YOHEISHINOMORI MASATOSHI
    • B29C69/02B29C45/14B29C49/04B29C49/48B29C49/64B29K105/04B29L9/00
    • PROBLEM TO BE SOLVED: To provide a method for molding a resin molding which can prevent a degradation in physical properties of the molding based on the wall thinning while accelerating foaming based on an expandable resin.
      SOLUTION: The molten expandable resin 70 is supplied into a blow-molded body 41 in a mold 4. After that, the mold 4 is opened in the mold opening direction in a prescribed quantity to enlarge a cavity 27. The resin 70 is foamed to expand the blow-molded body 41. With regard to a part 44 wherein the blow-molded body 41 is stretched on the basis of the expansion of the body 41, the resin 70 in the neighborhood of a part to be stretched of the body 41 is cooled positively through a second movable mold 23 to form a skin layer 85. A surface layer part 86 is formed by the skin layer 85 and the part 44.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 解决问题的方案:提供一种树脂成形体的成型方法,该树脂成形体可以在基于可发性树脂加速发泡的同时,基于壁变薄防止模制品的物理性能降低。 解决方案:将熔融的可膨胀树脂70供应到模具4中的吹塑模制体41中。之后,模具4在开模方向上以规定的量打开以扩大空腔27.树脂70 发泡以膨胀吹塑体41.关于吹塑成型体41基于主体41的膨胀而被拉伸的部分44,树脂70在待拉伸部分附近 主体41通过第二可移动模具23被正确地冷却以形成表层85.表层86由表皮层85和部分44形成。版权所有(C)2008,JPO&INPIT
    • 9. 发明专利
    • Method and apparatus for molding foamed resin molding
    • 用于模制泡沫树脂模塑的方法和装置
    • JP2009226872A
    • 2009-10-08
    • JP2008078052
    • 2008-03-25
    • Mazda Motor Corpマツダ株式会社
    • KANEKO MITSUHARUOGAWA JUNICHINAKAJIMA YUKINORIMIYAMOTO TSUGUHISASHINOMORI MASATOSHI
    • B29C45/56B29C45/26B29K105/04
    • B29C44/586
    • PROBLEM TO BE SOLVED: To prevent a resin part adjoining a vertical wall part from being pulled to the side of an opposite vertical wall part when the vertical wall part of a mold in the e core ward movement direction of a movable core is made to exist in a molding cavity, and an expandable resin adjoining the vertical wall part is also expanded with the backward movement of the core of a movable mold in foamed resin molding using a core back method. SOLUTION: In a method for molding a foamed resin molding, the vertical wall part 34w is made to exist in the molding cavity 30 approximately in the core backward movement direction of a movable mold 31, and the expandable resin adjoining the vertical wall part is also expanded with the backward movement of the core of the movable mold. The movable mold is divided into a first movable mold part 32 having the vertical wall part and a second movable mold part 36 adjoining it, and the rate of the amount of the backward movement of the core of the first movable mold part is made to be smaller than that of the amount of the backward movement of the core of the second movable mold part. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:为了防止在可动铁心的e芯区域移动方向上的模具的垂直壁部分是在垂直壁部分相邻的树脂部分被拉到相对的垂直壁部分的侧面时 并且与发泡树脂成型中的可动模具的芯部的反向运动相比,也使扩展树脂与垂直壁部相邻地扩展。 解决方案:在用于模制发泡树脂模制品的方法中,垂直壁部分34w大致沿着可动模具31的芯向后移动方向存在于模制腔30中,并且可膨胀树脂与垂直壁 部分也随着活动模具的芯的向后运动而扩大。 可移动模具被分成具有垂直壁部的第一可移动模具部分32和与其相邻的第二可移动模具部分36,并且使第一可动模具部件的芯部向后移动的速率为 小于第二可移动模具部件的芯部的向后运动的量。 版权所有(C)2010,JPO&INPIT
    • 10. 发明专利
    • Molding method and molding device of foamed resin molded article
    • 泡沫树脂模制品的成型方法和成型装置
    • JP2009196284A
    • 2009-09-03
    • JP2008042336
    • 2008-02-25
    • Mazda Motor Corpマツダ株式会社
    • KANEKO MITSUHARUOGAWA JUNICHINAKAJIMA YUKINORIMIYAMOTO TSUGUHISASHINOMORI MASATOSHI
    • B29C45/00B29C45/26B29C45/56B29C45/70B29K105/04
    • PROBLEM TO BE SOLVED: To prevent an unqualified shape of a foamed resin molded article and a decrease of a dimensional accuracy of a plane shape thereof, both problems being caused by a shrinkage of a margin of a sparkling resin filled in a cavity to the inside of the molded article during backward moving a shaping mold (core back) in case of molding the foamed resin article by backward moving the shaping mold.
      SOLUTION: When a molten sparkling resin 40 is filled in the cavity 33 between a fixed mold 31 and a movable mold 32 and then the foamed resin molded article 50 is molded by backward moving the movable mold 32 in such a direction that the cavity volume increases, after the movable mold 32 is backward moved and before the movable mold is opened, the movable mold 32 is compressively moved in such an anti-core back direction that the cavity volume decreases to compress the sparkling resin 40 in the cavity 33 to the degree that the foaming state is maintained and to push out the margin of the sparkling resin 40 to the space 93 of the cavity margin generated in the cavity 33 during backward moving the mold.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题为了防止发泡树脂成型体的不合格形状和其平面形状的尺寸精度的降低,这两个问题是由填充在空腔中的起泡树脂的边缘的收缩引起的 在通过向后移动成形模具成型发泡树脂制品的情况下,在成型模具(芯背)中向后移动期间,向模制品的内部。 解决方案:当熔融的起泡树脂40填充在固定模具31和可移动模具32之间的空腔33中时,通过使可移动模具32沿着这样的方向向后移动来模制发泡树脂模制品50: 空腔体积增加,在可动模具32向后移动之后并且在可动模具打开之前,可移动模具32以空腔体积减小的反芯方向压缩移动,以压缩空腔33中的起泡树脂40 达到保持发泡状态的程度,并且在反模移动模具期间将起泡树脂40的边缘推出到在空腔33中产生的空腔边缘的空间93。 版权所有(C)2009,JPO&INPIT